2019 | OriginalPaper | Chapter
Casting Defect Analysis on Fracture Surface of 356 Aluminium Alloy
Authors : Özen Gürsoy, Eray Erzi, Derya Dispinar
Published in: Shape Casting
Publisher: Springer International Publishing