Erosive Wear Study of Nitrogen-Containing 23-8-N Austenitic Stainless Steel and Bead on Plate Weld Using ER2209 Stainless Steel Filler Wire

Authors : Naveen Kumar, Navneet Arora, S. K. Goel

Published in: Recent Advances in Mechanical Engineering

Publisher: Springer Singapore

Activate our intelligent search to find suitable subject content or patents.

search-config
loading …

Abstract

Jet-type slurry erosion testing of the nitrogen-containing austenitic stainless steel 23-8-N in as-received, heat-treated (950 °C and 1150 °C temperatures) and bead on plate weld have been carried out with less than 500 µm size of erodent silica sand. The bead on plate weld is performed with ER2209 filler wire with gas metal arc welding. Erosion resistance of base metal increases at higher heat treatment temperature but there is no effect on weld bead erosion resistance. Weld has higher cumulative weight loss as compared to base metal.

Dont have a licence yet? Then find out more about our products and how to get one now:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Springer Professional "Wirtschaft"

Online-Abonnement

Mit Springer Professional "Wirtschaft" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 340 Zeitschriften

aus folgenden Fachgebieten:

  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Versicherung + Risiko




Jetzt Wissensvorsprung sichern!

Literature
1.
go back to reference Goel DB (2008) Metallurgy of erosion of underwater parts in hydroelectric projects. In: Proceedings of the 3rd international conference on silting problems in hydropower projects, pp 1–10 Goel DB (2008) Metallurgy of erosion of underwater parts in hydroelectric projects. In: Proceedings of the 3rd international conference on silting problems in hydropower projects, pp 1–10
2.
go back to reference Mendez PF et al (2014) Welding processes for wear resistant overlays. J Manuf Process 4–25 Mendez PF et al (2014) Welding processes for wear resistant overlays. J Manuf Process 4–25
3.
go back to reference Gou WJ (2016) Study on welding repair process of turbine blade. In: Chen (ed) Material science and environmental engineering, London, pp 497–500 Gou WJ (2016) Study on welding repair process of turbine blade. In: Chen (ed) Material science and environmental engineering, London, pp 497–500
4.
go back to reference Naidu BSK (2004) Silting problem in hydro power plant & their possible solutions. NPTI, India Naidu BSK (2004) Silting problem in hydro power plant & their possible solutions. NPTI, India
5.
go back to reference Chaudhary CS (1999) Impact of high sediment on hydraulic equipment of Marsyangdi hydropower plant. In: Proceedings of the international seminar on sediment handling technique, NHA, Kathmandu Chaudhary CS (1999) Impact of high sediment on hydraulic equipment of Marsyangdi hydropower plant. In: Proceedings of the international seminar on sediment handling technique, NHA, Kathmandu
6.
go back to reference Singh RP (2009) Silt damage control measures for underwater parts—Nathpa Jhakri Hydro power station—case study of a success story Satluj Jal Vidyut Nigam Ltd., India, p 66 Singh RP (2009) Silt damage control measures for underwater parts—Nathpa Jhakri Hydro power station—case study of a success story Satluj Jal Vidyut Nigam Ltd., India, p 66
7.
go back to reference Gavriljuk V, Berns H (1999) High nitrogen steels: structure, properties, manufacture, applications, 1st edn. Springer, New YorkCrossRef Gavriljuk V, Berns H (1999) High nitrogen steels: structure, properties, manufacture, applications, 1st edn. Springer, New YorkCrossRef
8.
go back to reference Gavriljuk V, Razumov O, Petrov Y, Surzhenko I, Berns H (2017) High strength stainless austenitic CrMnCN steels—Part II: structural changes by repeated impacts. Steel Res Int 78:720–723CrossRef Gavriljuk V, Razumov O, Petrov Y, Surzhenko I, Berns H (2017) High strength stainless austenitic CrMnCN steels—Part II: structural changes by repeated impacts. Steel Res Int 78:720–723CrossRef
9.
go back to reference Chauhan AK, Goel DB, Prakash S (2008) Erosion behaviour of hydro turbine steels. Bull Mater Sci 31:115–120 Chauhan AK, Goel DB, Prakash S (2008) Erosion behaviour of hydro turbine steels. Bull Mater Sci 31:115–120
10.
go back to reference Kumar A, Sharma A, Goel SK (2015) Effect of heat treatment on microstructure, mechanical properties and erosion resistance of cast 23-8-N nitronic steel. Mater Sci Eng A 637:56–62CrossRef Kumar A, Sharma A, Goel SK (2015) Effect of heat treatment on microstructure, mechanical properties and erosion resistance of cast 23-8-N nitronic steel. Mater Sci Eng A 637:56–62CrossRef
11.
go back to reference Aniruddha AG (2011) Characterization study of steels for erosion resistant applications. Ph.D. thesis, MNIT, Jaipur, India Aniruddha AG (2011) Characterization study of steels for erosion resistant applications. Ph.D. thesis, MNIT, Jaipur, India
12.
go back to reference Kumar A, Sharma A, Goel SK (2016) Erosion behaviour of WC–10Co–4Cr coating on 23-8-N nitronic steel by HVOF thermal spraying. Appl Surf Sci 370:418–426CrossRef Kumar A, Sharma A, Goel SK (2016) Erosion behaviour of WC–10Co–4Cr coating on 23-8-N nitronic steel by HVOF thermal spraying. Appl Surf Sci 370:418–426CrossRef
13.
go back to reference Thakur L (2014) An investigation on thermal spray wear resistant coating. Ph.D. thesis, IIT Roorkee, India Thakur L (2014) An investigation on thermal spray wear resistant coating. Ph.D. thesis, IIT Roorkee, India
14.
go back to reference Padilha AF, Rios PR (2002) Decomposition of austenite in austenitic stainless steels. ISIJ Int 42:325–327 Padilha AF, Rios PR (2002) Decomposition of austenite in austenitic stainless steels. ISIJ Int 42:325–327
15.
go back to reference Kotecki DJ, Siewert TA (1992) WRC-1992 constitution diagram for stainless steel weld metals: a modification of the WRC-1988 diagram. Weld Res Suppl 171–178 Kotecki DJ, Siewert TA (1992) WRC-1992 constitution diagram for stainless steel weld metals: a modification of the WRC-1988 diagram. Weld Res Suppl 171–178
16.
go back to reference Desale GR, Gandhi BK, Jain SC (2005) Improvement in the design of a pot tester to simulate erosion wear due to solid-liquid mixture. Wear 259:196–202 Desale GR, Gandhi BK, Jain SC (2005) Improvement in the design of a pot tester to simulate erosion wear due to solid-liquid mixture. Wear 259:196–202
Metadata
Title
Erosive Wear Study of Nitrogen-Containing 23-8-N Austenitic Stainless Steel and Bead on Plate Weld Using ER2209 Stainless Steel Filler Wire
Authors
Naveen Kumar
Navneet Arora
S. K. Goel
Copyright Year
2020
Publisher
Springer Singapore
DOI
https://doi.org/10.1007/978-981-15-1071-7_47

Premium Partners