Abstract

In this paper, thermal and thermo-oxidative stability of three water-based polyurethanes (PUs) derived from hydroxypropyl terminated poly(dimethylsiloxane) (HPT-PDMS) were studied. The structural properties of the synthesized samples were investigated by 1H NMR measurements, while characterization of their surface, performed by atomic force microscopy, revealed the existence of microphase-separated structures. According to the results obtained by thermogravimetric analysis (TGA), thermo-oxidative and thermal stability of the investigated water-based PUs decreases with decreasing HPT-PDMS content. Furthermore, obtained results also suggest that both, thermo-oxidative and thermal degradation reaction of water-based PUs occurred as a three-step process. In both atmospheres the first step of degradation is attributed to the degradation of weak urethane and urea bonds and the second step to the decomposition of polysiloxane chains. In order to undertake a detail investigation of thermal degradation process of water-based PUs, TG measurements in nitrogen atmosphere at four different heating rates (5, 10, 15 and 20 °C/min) were performed. Different iso-conversional model-free methods, such as Ozawa-Flynn-Wall, Kissinger-Akahira-Sunose and Friedman, were applied to determine apparent activation energy of thermal degradation reaction (Ea) of water-based PUs, at different conversions (α). Deviation in parallelism of the obtained fitted lines confirmed that thermal degradation reaction of water-based PUs occurred in three successive steps, followed by different degradation mechanism. Since linear fitting of the experimental data by Friedman method had the lowest correlation coefficient, Ozawa-Flynn-Wall and Kissinger-Akahira-Sunose methods were considered to be the most reliable for Ea calculation. A comprehensive analysis of the obtained results revealed that, despite their similar structure, each water-based PU shows unique profile of Ea = f(α) plot.

Dont have a licence yet? Then find out more about our products and how to get one now:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literature
15.
32.
go back to reference Harvey JA (2005). In: Kutz M (ed) Handbook of environmental degradation of materials. William Andrew Publishing, New York, USA Harvey JA (2005). In: Kutz M (ed) Handbook of environmental degradation of materials. William Andrew Publishing, New York, USA
36.
go back to reference Thuilliez AL, Gavard-Lonchay O, Doisneau D, Loubat C, Crouzet Q (2017) Rubber composition with a high level of fluidity based on an aromatic aldehyde and an aromatic polyphenol. Patent number: WO 2017/103404. 22. 06. 2017 Thuilliez AL, Gavard-Lonchay O, Doisneau D, Loubat C, Crouzet Q (2017) Rubber composition with a high level of fluidity based on an aromatic aldehyde and an aromatic polyphenol. Patent number: WO 2017/103404. 22. 06. 2017
44.
go back to reference Akahira T, Sunose T (1971) Method of determining activation deterioration constant of electrical insulating materials, joint convention of four electrical institutes. Res Rep Chiba Inst Technol (Sci Technol) 16:22–31 Akahira T, Sunose T (1971) Method of determining activation deterioration constant of electrical insulating materials, joint convention of four electrical institutes. Res Rep Chiba Inst Technol (Sci Technol) 16:22–31
49.
go back to reference Dvornić PR, Lenz RW (1990) High temperature siloxane elastomers. Hüthing & Wepf, New York Dvornić PR, Lenz RW (1990) High temperature siloxane elastomers. Hüthing & Wepf, New York
Metadata
Title
Study on thermal stability of water-based polyurethanes derived from hydroxypropyl terminated poly(dimethylsiloxane)
Authors
Jasna V. Džunuzović
Ivan S. Stefanović
Enis S. Džunuzović
Andrea Basagni
Carla Marega
Publication date
01-05-2024
Publisher
Springer Netherlands
Published in
Journal of Polymer Research / Issue 5/2024
Print ISSN: 1022-9760
Electronic ISSN: 1572-8935
DOI
https://doi.org/10.1007/s10965-024-03982-w

Other articles of this Issue 5/2024

Journal of Polymer Research 5/2024 Go to the issue

Premium Partners