Abstract
In this study, the kiln drying yield of 30 mm Rubberwood (Hevea brasiliensis) used for the furniture manufacturing industry in South East Asia was evaluated. The results showed that the average yield loss was 10%, and end-checks, splits and warping were the most common drying defects. It was found that sawn timber from older trees (> 21 years) were less prone to drying defects, and the use of stress relieving treatments significantly reduced the incidence of drying defects.
Similar content being viewed by others
References
Hong LT, Sim HC (1999) Rubberwood – processing and utlization. Malayan Forest Record No. 39, Forest Research Institute of Malaysia
Ratnasingam J (2004) Economic of the Rubberwood processing industry – a South East Asian perspective. Asian Timber 23(2):16–18
Ratnasingam J, Florin I, Macpherson TH (2007) Influence of wood species on the perceived value of wooden furniture: the case of Rubberwood. Holz Roh- Werkst 65:487–489
Ratnasingam J, Scholz F (2008) Yield studies of Rubberwood lumber during rough milling operation. Holz Roh- Werkst 66:467–468
Zobel BJ, van Buijtenen JP (1989) Wood variation – its causes and control. Spinger, Berlin
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Ratnasingam, J., Grohmann, R. & Scholz, F. Drying quality of rubberwood: an industrial perspective . Eur. J. Wood Prod. 68, 115–116 (2010). https://doi.org/10.1007/s00107-009-0353-x
Received:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s00107-009-0353-x