Skip to main content
Erschienen in: Wood Science and Technology 1/2017

06.10.2016 | Original

Fracture in Norway spruce wood treated with Physisporinus vitreus

verfasst von: Marjan Sedighi Gilani, Markus Heeb, Anja Huch, Siegfried Fink, Francis Willis Mathew Robert Schwarze

Erschienen in: Wood Science and Technology | Ausgabe 1/2017

Einloggen

Aktivieren Sie unsere intelligente Suche, um passende Fachinhalte oder Patente zu finden.

search-config
loading …

Abstract

Changes in the fracture behaviour of Norway spruce tonewood after fungal treatment were studied. Specimens were incubated for 6, 9 and 12 months with Physisporinus (P.) vitreus. Fracture tests were performed in a compact-tension fracture experiment set-up, and the results were compared with the morphological analysis of the degraded wood structure and transverse sections of the crack tip viewed under light and fluorescence microscopy. It was evident that both the failure load and critical stress intensity factors were reduced in wood after prolonged incubation periods. Weight losses were significantly higher in sapwood than in heartwood. With prolonged incubation periods, the frequency of unstable fracture and brittle behaviour of the wood increased. In untreated wood, cracks were initiated in the earlywood. The process involved both delamination of the cells within the middle lamellae and rupture of the cell walls, inducing a zigzag crack tip pattern. In fungally treated wood, cracks often commenced from the intersection between late- and earlywood, resulting in a straight tangential crack line. Micrographic images showed that P. vitreus was more active in the secondary walls of latewood tracheids. In this region of the wood, the cell walls were strongly degraded after 9–12 months of incubation, resulting in a reduction in tensile strength, even though the wood did not show strong features of decay at the macroscopic level.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Literatur
Zurück zum Zitat Boatright SWJ, Garrett GG (1983) The effect of microstructure and stress state on the fracture behaviour of wood. J Mater Sci 18:2181–2199CrossRef Boatright SWJ, Garrett GG (1983) The effect of microstructure and stress state on the fracture behaviour of wood. J Mater Sci 18:2181–2199CrossRef
Zurück zum Zitat Bower AF (2009) Applied mechanics of solids. CRC Press, Boca Raton Bower AF (2009) Applied mechanics of solids. CRC Press, Boca Raton
Zurück zum Zitat Dill-Langer G, Lutye S, Aicher S (2002) Microfracture in wood monitored by confocal laser scanning microscopy. Wood Sci Technol 36:487–499CrossRef Dill-Langer G, Lutye S, Aicher S (2002) Microfracture in wood monitored by confocal laser scanning microscopy. Wood Sci Technol 36:487–499CrossRef
Zurück zum Zitat European Standard EN 113 (1997) Wood preservatives: test method for determining the protective effectiveness against wood destroying basidiomycetes. Determination of toxic values. European Committee for Standardization, Brussels European Standard EN 113 (1997) Wood preservatives: test method for determining the protective effectiveness against wood destroying basidiomycetes. Determination of toxic values. European Committee for Standardization, Brussels
Zurück zum Zitat Gamstedt EK, Bader TK, de Borst K (2013) Mixed numerical—experimental methods in wood micromechanics. Wood Sci Technol 47:183–202CrossRef Gamstedt EK, Bader TK, de Borst K (2013) Mixed numerical—experimental methods in wood micromechanics. Wood Sci Technol 47:183–202CrossRef
Zurück zum Zitat Keunecke D, Niemz P, Tollert M, Hänsel A (2012) Mechanical properties and failure of yew and spruce determined with a compact tension test and digital image correlation. Wood Res 54:669–676 Keunecke D, Niemz P, Tollert M, Hänsel A (2012) Mechanical properties and failure of yew and spruce determined with a compact tension test and digital image correlation. Wood Res 54:669–676
Zurück zum Zitat Landis EN, Vasic S, Davids WG, Parrod P (2002) Coupled experiments and simulations of microstructural damage in wood. Exp Mech 42:389–394CrossRef Landis EN, Vasic S, Davids WG, Parrod P (2002) Coupled experiments and simulations of microstructural damage in wood. Exp Mech 42:389–394CrossRef
Zurück zum Zitat Lehringer C, Hillebrand K, Richter K, Arnold M, Schwarze FWMR, Militz H (2010) Anatomy of bioincised Norway spruce wood. Int Biodeterior Biodegrad 64:346–355CrossRef Lehringer C, Hillebrand K, Richter K, Arnold M, Schwarze FWMR, Militz H (2010) Anatomy of bioincised Norway spruce wood. Int Biodeterior Biodegrad 64:346–355CrossRef
Zurück zum Zitat Lehringer C, Saake B, Živkovic V, Richter K, Militz H (2011) Effect of Physisporinus vitreus on wood properties of Norway spruce. Part 2: aspects of microtensile strength and chemical changes. Holzforschung 65:721–727 Lehringer C, Saake B, Živkovic V, Richter K, Militz H (2011) Effect of Physisporinus vitreus on wood properties of Norway spruce. Part 2: aspects of microtensile strength and chemical changes. Holzforschung 65:721–727
Zurück zum Zitat Maeda K, Ohta M, Momohara I (2015) Relationship between the mass profile and the strength property profile of decayed wood. Wood Sci Technol 49:331–344CrossRef Maeda K, Ohta M, Momohara I (2015) Relationship between the mass profile and the strength property profile of decayed wood. Wood Sci Technol 49:331–344CrossRef
Zurück zum Zitat Pandey KK, Pitman AJ (2003) FTIR studies of the changes in wood chemistry following decay by brown-rot and white-rot fungi. Int Biodeterior Biodegrad 52:151–160CrossRef Pandey KK, Pitman AJ (2003) FTIR studies of the changes in wood chemistry following decay by brown-rot and white-rot fungi. Int Biodeterior Biodegrad 52:151–160CrossRef
Zurück zum Zitat Ray M, Kleist G, Murphy R (2005) Decay assessment in a hardwood handrail at the South Bank, London. J Inst Wood Sci 17(1):51–58CrossRef Ray M, Kleist G, Murphy R (2005) Decay assessment in a hardwood handrail at the South Bank, London. J Inst Wood Sci 17(1):51–58CrossRef
Zurück zum Zitat Schwarze FWMR (2007) Wood decay under the microscope. Fungal Biol Rev 21:133–170CrossRef Schwarze FWMR (2007) Wood decay under the microscope. Fungal Biol Rev 21:133–170CrossRef
Zurück zum Zitat Schwarze FWMR, Landmesser L, Zgraggen B, Heeb M (2006) Permeability changes in heartwood of Picea abies and Abies alba induced by incubation with Physisporinus vitreus. Holzforschung 60:450–454CrossRef Schwarze FWMR, Landmesser L, Zgraggen B, Heeb M (2006) Permeability changes in heartwood of Picea abies and Abies alba induced by incubation with Physisporinus vitreus. Holzforschung 60:450–454CrossRef
Zurück zum Zitat Schwarze FWMR, Spycher M, Fink S (2008) Superior wood for violins wood decay fungi as a substitute for cold climate. New Phytol 179:1095–1104CrossRefPubMed Schwarze FWMR, Spycher M, Fink S (2008) Superior wood for violins wood decay fungi as a substitute for cold climate. New Phytol 179:1095–1104CrossRefPubMed
Zurück zum Zitat Sedighi Gilani M, Navi P (2007) Micromechanical approach to wood fracture by three-dimensional mixed lattice-continuum model at fiber level. Wood Sci Technol 41(7):619–634CrossRef Sedighi Gilani M, Navi P (2007) Micromechanical approach to wood fracture by three-dimensional mixed lattice-continuum model at fiber level. Wood Sci Technol 41(7):619–634CrossRef
Zurück zum Zitat Sedighi Gilani M, Tingout P, Heeb M, Schwarze FWMR (2014a) Influence of moisture on the vibro-mechanical properties of bio-engineered wood. J Mater Sci 49(22):7679–7687CrossRef Sedighi Gilani M, Tingout P, Heeb M, Schwarze FWMR (2014a) Influence of moisture on the vibro-mechanical properties of bio-engineered wood. J Mater Sci 49(22):7679–7687CrossRef
Zurück zum Zitat Sedighi Gilani M, Boone MN, Mader M, Schwarze FWMR (2014b) Synchrotron X-ray micro-tomography imaging and analysis of wood degraded by Physisporinus vitreus and Xylaria longipes. Struct Biol 187:149–157CrossRef Sedighi Gilani M, Boone MN, Mader M, Schwarze FWMR (2014b) Synchrotron X-ray micro-tomography imaging and analysis of wood degraded by Physisporinus vitreus and Xylaria longipes. Struct Biol 187:149–157CrossRef
Zurück zum Zitat Sedighi Gilani M, Neuenschwander J, Heeb M, Furrer R, Sanabria SJ, Stoel BC, Schwarze FWMR (2016) Influence of incubation time on the vibration and mechanic properties of mycowood. Holzforschung 70(6):557–565 Sedighi Gilani M, Neuenschwander J, Heeb M, Furrer R, Sanabria SJ, Stoel BC, Schwarze FWMR (2016) Influence of incubation time on the vibration and mechanic properties of mycowood. Holzforschung 70(6):557–565
Zurück zum Zitat Smith I, Landis E, Gong M (2003) Fracture and fatigue in wood. Wiley, Chichester. ISBN 978-0-471-48708-1 Smith I, Landis E, Gong M (2003) Fracture and fatigue in wood. Wiley, Chichester. ISBN 978-0-471-48708-1
Zurück zum Zitat Vasic S, Stanzl-Tschegg S (2006) Experimental and numerical investigation of wood fracture mechanisms at different humidity levels. Holzforschung 61:367–374 Vasic S, Stanzl-Tschegg S (2006) Experimental and numerical investigation of wood fracture mechanisms at different humidity levels. Holzforschung 61:367–374
Metadaten
Titel
Fracture in Norway spruce wood treated with Physisporinus vitreus
verfasst von
Marjan Sedighi Gilani
Markus Heeb
Anja Huch
Siegfried Fink
Francis Willis Mathew Robert Schwarze
Publikationsdatum
06.10.2016
Verlag
Springer Berlin Heidelberg
Erschienen in
Wood Science and Technology / Ausgabe 1/2017
Print ISSN: 0043-7719
Elektronische ISSN: 1432-5225
DOI
https://doi.org/10.1007/s00226-016-0873-6

Weitere Artikel der Ausgabe 1/2017

Wood Science and Technology 1/2017 Zur Ausgabe

IAWS NEWS

IAWS News