Abstract
Double-base propellants undergo chemical, physical and mechanical changes upon ageing, leading to changes in ballistic performance and presenting explosive hazards. This report studies the variation of chemical and mechanical properties of aged N,N′-dimethyl-N,N′-diphenylcarbamide (methyl centralite) stabilized propellants in order to simulate and evaluate the natural ageing throughout the artificial one. Therefore, a comparative study of stabilizer depletion, plasticizers content, heat of combustion and mechanical properties such as storage modulus, loss modulus and damping of naturally and artificially aged propellants has been carried out by the following techniques: high-performance liquid chromatography (HPLC), thermogravimetric analyzer (TG), calorimeter of combustion and dynamic mechanical analyzer (DMA), respectively. The results obtained show that all properties are closely connected. In addition, the determination of stabilizer depletion, plasticizers evaporation, decrease of heat of combustion and mechanical properties are very useful for a better understanding of the decomposition and ageing behaviour of propellants. The HPLC investigation of stabilizer has shown good stability of the propellants. The results obtained for DMA have shown that some considerable changes of the mechanical and viscoelastic properties of the propellants occurred during ageing. These results confirm the results obtained by TG for the reduction of the nitroglycerine amount and the decrease of the heat of combustion.
Similar content being viewed by others
References
Bohn MA, Volk F. Aging behavior of propellants investigated by heat generation, stabilizer consumption, and molar mass degradation. Propellant Explos Pyrotech. 1992;17:171–8.
Vogelsanger B. Chemical stability, compatibility and shelf life of explosives. Chimia. 2004;58:401–8.
Lussier LS, Gagnon H. Development of modern methods for determination of stabilizers in propellants. Defense research establishment. Valcartier, Quebec: DREV R-9511; 1996.
Volk F, Bohn MA, Wunsch G. Determination of chemical properties of double base propellants during aging. Propellant Explos Pyrotech. 1987;12:81–7.
Trache D, Mazroua A, Khimeche K. Determination of chemical and mechanical properties of propellants during ageing. In: Proceedings of 42nd international annual conference of ICT, Karlsruhe; 2011. pp. 83/1–10.
Lindblom T. Reaction in stabilizer and between stabilizer and nitrocellulose in propellants. Propellant Explos Pyrotech. 2002;27:197–208.
Venkatesan D, Srinivasan M, Reddy KA, Pendse VV. The migration of plasticizer in solid propellant grains. Polym internatl. 1993;32:395–9.
Sorensen DN, Knott DL, Bell RF. Two-gram DTA as a thermal compatibility tool. J Therm Anal Calorim. 2008;91:305–9.
Boers MN, de Klerk WPO. Lifetime prediction of EC, DPA, akardite II and MNA stabilized triple base propellants, comparison of heat generation rate and stabilizer consumption. Propellant Explos Pyrotech. 2005;30:356–62.
Lussier LS, Berger E, Gapnon H. Study of daughter products of Akardite-II. Propellant Explos Pyrotech. 2006;31:253–62.
Bohn MA. Kinetic modelling of the ageing of gun and rocket propellants for the improved and time extended prediction of their service lifetime. In: Proceedings of 4th life cycles of energetic materials conference, Fullerton; 1998. pp. 1-38.
Bohn MA. Kinetic modelling of the concentrations of the stabilizer DPA and some of its consecutive products as function of time and temperature. J Therm Anal Calorim. 2001;65:103–20.
Bohn MA. Prediction of equivalent time-temperature loads for accelerated ageing to simulate preset in-storage ageing and time- temperature profile loads. In: Proceedings of 40th international annual conference of ICT, Karlsruhe; 2009. pp. 78/1–28.
Sućeska M, Mušanić SM, Houra IF. Kinetics and enthalpy of nitroglycerin evaporation from double base propellants by isothermal thermogravimetry. Thermochim Acta. 2010;510:9–16.
Husband DM. Use of dynamic mechanical measurements to determine the aging behaviour of solid propellant. Propellant Explos Pyrotech. 1992;17:196–201.
Herder G, Weterings FP, de Klerk WPC. Mechanical analysis on rocket propellants. J Therm Anal Calorim. 2003;72:921–9.
Herder G, de Klerk WPC. Measurement of the relaxation transitions of nitrocellulose based gunpowder. J Therm Anal Calorim. 2006;85:169–72.
Musanic SM, Suceska M. Artificial ageing of double base rocket propellant-Effect on dynamic mechanical properties. J Therm Anal Calorim. 2009;96:523–9.
Suceska M, Musanic SM, Fiamengo I. Study of mechanical properties of naturally aged double base rocket propellants. Cent Eur J Energ Mater. 2010;7(1):47–60.
Townend DJ, Warren RC. Relaxations in double base propellants. Polym. 1985;26:79–83.
Standardization agreement STANAG 4117, explosives, stability test procedures and requirements for propellants stabilized with diphenylamine, ethyl centralite or mixtures of both. 3rd ed. NATO; 1998.
Stancovic M, Filipovic M, Kapor V. Thermal analysis in propellant stability examinations. J Therm Anal. 1998;52:439–45.
Parr® (1978) Introduction to bomb calorimetry No. 202M, Moline, IL.
Bohn MA, Eisenreich N. Kinetic modelling of the stabilizer consumption and of the consecutive products of the stabilizer in a gun propellant. Propellant Explos Pyrotech. 1997;22:125–36.
Tompsa AS. Thermal analysis of liquid and solid propellants. J Hazard Mater. 1980;4:95–112.
Verneker VRP, Kishore K. Studies on thermal decomposition of double base propellants. J Spacecraft. 1983;20(2):141–3.
Gabbott P. Principles and applications of thermal analysis. Oxford: Blackwell publishing; 2008.
Menard KP. Dynamic mechanical analysis, a practical introduction. Boca Raton : CRC Press; 1999.
ASTM E1640. Test method for assignment of the glass transition temperature by dynamic mechanical analysis.
Bohn MA. Characterization of the ageing of HTPB binder based insensitive high explosive charge by heat flow microcalorimetry, chemiluminescence, GAP test and dynamic mechanical analysis. In: Proceedings of 40th international annual conference of ICT, Karlshure; 2009. pp. 7/1–16.
Kai D, Jianhong Y, Weiwei H, Fei C, Chaofeng L, Chengwu L, Hui Z, Yanjun W. A new method to obtain shear modulus of solid propellant. Acta Astronaut. 2011;69:440–4.
Li Y, Chenxia K, Huang C, Cheng Y. Effect of MnC2O4 nanoparticules on the thermal decomposition of TEGDN/NC propellant. J Therm Anal Calorim. 2011. doi:10.1007/s10973-011-1694-3.
Sućeska M, Liu Z-Y, Matečić Mušanić S, Fiamengo I. Numerical modelling of sample–furnace thermal lag in dynamic mechanical analyser. J Therm Anal Calorim. 2010;100:337–45.
Calvo S, Escribano J, Prolongo MG, Masegosa RM, Salom C. Thermomechanical properties of cured isophtalic polyester resin modified with poly(ε-caprolactone). J Therm Anal Calorim. 2011;103:195–203.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Trache, D., Khimeche, K. Study on the influence of ageing on chemical and mechanical properties of N,N′-dimethyl-N,N′-diphenylcarbamide stabilized propellants. J Therm Anal Calorim 111, 305–312 (2013). https://doi.org/10.1007/s10973-012-2320-8
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s10973-012-2320-8