Abstract
The corrosion resistance of a 12CrMoV alloy incontact with a molten mixture of (52-48)mol.%PbCl2-KCl, similar to that found inwaste incineration plants, has been studied. Thecorrosion kinetics have been analyzed using continuous-currentelectrochemical techniques and electrochemical impedancespectroscopy (EIS). Studies were performed to determinethe influence that temperature and the presence of carbon in the salt have on the corrosion rate.Scanning electron microscopy (SEM) and electron-probemicroanalysis (EPMA) were used as additional analyticaltechniques to analyze the corrosion products in order to elucidate the corrosionmechanism.
Similar content being viewed by others
REFERENCES
G. Y. Lai, High Temperature Corrosion of Engineering Alloys (ASM Intern, 1990).
Manuales de Energías Renovables/2 Incineración de residuos sólidos urbanos. (Instituto para la Diversificación y Ahorro de Energía, 1992).
G. Y. Lai, Proc. Conf. Chemical Waste Incineration, 12-13 March, Manchester, 1990).
P. Elliot, Mater. Selection Design, Feb., 1993.
Corrosion des materiaux à haute temperature. (Les editions de physique, 1985).
G. Y. Lai, Materials Performance in Waste Incineration System (NACE, 1991).
H. J. Grabke, E. Reese, and M. Spiegel, Corros. Sci. 37, 1023 (1995).
ASTMG59-78. Standard practice for conducting potentiodynamic polarization resistance measurements.
ASTMG102-89. Standard practice for calculation of corrosion rates and related information from electrochemical measurements.
F. Mansfeld, Corrosion 36(5), 301 (1981).
K. Hldaky, L. M. Callow, and J. L. Dawson, Brit. Corros. J. 15(1), 20 (1980).
L. M. Callow, J. A. Richardson, and J. L. Dawson, Brit. Corros. J. 11, 123, 132 (1976).
I. Epelboin and M. Keddam, J. Electrochem. Soc. 117, 1052 (1970).
R. D. Armstrong and M. Henderson, J. Electroanal. Chem. 39, 81 (1972).
I. Epelboin, J. Keddam, and H. Takenouti, J. Appl. Electrochem. 2, 71 (1972).
Rights and permissions
About this article
Cite this article
Otero, E., Pardo, A., Perez, F.J. et al. Corrosion Behavior of 12CrMoV Steel in Waste Incineration Environments: Hot Corrosion by Molten Chlorides. Oxidation of Metals 49, 467–484 (1998). https://doi.org/10.1023/A:1018851029023
Issue Date:
DOI: https://doi.org/10.1023/A:1018851029023