Abstract
The deposition of uniform coatings of fluorinated polymers from solutions in supercritical carbon dioxide on a number of rough substrates allowed superhydrophobic (ultrahydrophobic) properties to be imparted to their surfaces, and, namely, to increase the value of the contact angle for water droplet to 150° and greater. The dynamics of changing of geometry of a drying droplet on a substrate is studied. A procedure is developed that permits the penetration of water into the substrate to be detected.
Similar content being viewed by others
References
Barthlott, W. and Neinhuis, C., Planta, 1997, vol. 202, p. 1.
Wenzel, R.N., Ind. Eng. Chem., 1936, vol. 28, p. 988.
Cassie, A.B.D. and Baxter, S., Trans. Faraday Soc., 1944, vol. 40, p. 546.
Quéré, D., Lafuma, A., and Bico, J., Nanotecnology, 2003, vol. 14, p. 1109.
McHale, G., Shirtcliffe, N.J., and Newton, M.I., Langmuir, 2004, vol. 20, p. 10146.
Johnson, R.E. and Dettre, R.U., Adv. Chem. Ser., 1964, no. 43.
Nakajima, A., Hashimoto, K., and Watanabe, T., Monatsh. Chem., 2001, vol. 132, p. 31.
Feng, L., Li, S., Li, Y., et al., Adv. Mater. (Weinheim, Fed. Repub. Ger.), 2002, vol. 14, p. 1857.
Quéré, D., Nature Mater., 2002, vol. 1, p. 14.
Blossey, R., Nature Mater., 2003, vol. 2, p. 301.
Gould, P., Mater. Today, 2003, vol. 6, no. 11, p. 44.
Otten, A. and Herminghaus, S., Langmuir, 2004, vol. 20, p. 2405.
Sun, T., Feng, L., Gao, X., and Jiang, L., Acc. Chem. Res., 2005, vol. 38, p. 644.
Quéré, D., Rep. Prog. Phys., 2005, vol. 68, p. 2495.
Lafuma, A. and Quéré, D., Nature Mater., 2003, vol. 2, p. 457.
Cheng, Y.-T. and Rodak, D.E., Appl. Phys. Lett., 2005, vol. 86, p. 144101.
Wier, K.A. and McCarthy, T.J., Langmuir, 2006, vol. 22, p. 2433.
Sugimoto, H. and Ohashi, M. Jpn. Patent 11116278, 1999.
McHugh, M.A., Mertdogan, C.A., DiNoia, T.P., et al., Macromolecules, 1998, vol. 31, p. 2252.
Henon, F.E., Camaiti, M., Burke, A., et al., J. Supercrit. Fluids, 1999, vol. 15, p. 173.
Rindfleisch, F., DiNoia, T.P., and McHugh, M.A., J. Phys. Chem., 1996, vol. 100, p. 15581.
Kirby, C.F. and McHugh, M.A., Chem. Rev., 1999, vol. 99, p. 565.
Petersen, R.C., Matson, D.W., and Smith, R.D., J. Am. Chem. Soc., 1986, vol. 108, p. 2100.
Matson, D.W., Fulton, J.L., Petersen, R.C., and Smith, R.D., Ind. Eng. Chem. Res., 1987, vol. 26, p. 2298.
Kim, J.-H., Paxton, T.E., and Tomasko, D.L., Biotechnol. Prog., 1996, vol. 12, p. 650.
Shim, J.-J., Yates, M.Z., and Johnston, K.P., Ind. Eng. Chem. Res., 1999, vol. 38, p. 3655.
Tepper, G. and Levit, N., Ind. Eng. Chem. Res., 2000, vol. 39, p. 4445.
Chernyak, Y., Henon, F., Harris, R.B., et al., Ind. Eng. Chem. Res., 2001, vol. 40, p. 6118.
Matsuyama, K., Mishima, K., Umemoto, H., and Yamaguchi, S., Environ. Sci. Technol., 2001, vol. 35, p. 4149.
Wang, T.-J., Tsutsumi, A., Hasegawa, H., and Mineo, T., Powder Technol., 2001, vol. 118, p. 229.
Wang, Y., Wei, D., Dave, R., et al., Powder Technol., 2002, vol. 127, p. 32.
Levit, N., Pestov, D., and Tepper, G., Sens. Actuators, B, 2002, vol. 82, p. 241.
Fulton, J.L., Deverman, G.S., Yonker, C.R., et al., Polymer, 2003, vol. 44, p. 3627.
Inoue, H., Jpn. Patent 2001314810, 2001.
Mawson, S., Johnston, K.P., Betts, D.E., et al., Macromolecules, 1997, vol. 30, p. 71.
Reverchon, E., J. Supercrit. Fluids, 1999, vol. 15, p. 1.
Elvassore, N., Bertucco, A., and Caliceti, P., Ind. Eng. Chem. Res., 2001, vol. 40, p. 795.
Chattopadhyay, P. and Gupta, R.B., Ind. Eng. Chem. Res., 2000, vol. 39, p. 2281.
Chattopadhyay, P. and Gupta, R.B., Ind. Eng. Chem. Res., 2001, vol. 40, p. 3530.
Chattopadhyay, P. and Gupta, R.B., Ind. Eng. Chem. Res., 2002, vol. 41, p. 6049.
Chattopadhyay, P. and Gupta, R.B., Ind. Eng. Chem. Res., 2003, vol. 42, p. 465.
Wang, Y., Dave, R.N., and Pfetter, R., J. Supercrit. Fluids, 2004, vol. 28, p. 85.
Glebov, E.M., Yuan, L., Krishtopa, L.G., et al., Ind. Eng. Chem. Res., 2001, vol. 40, p. 4058.
Hoggan, E.N., Flowers, D., Carbonell, R.G., and DeSimone, J.M., Ind. Eng. Chem. Res., 2004, vol. 43, p. 2113.
Cho, D., Kim, Y.J., Erkey, C., and Koberstein, J.T., Macromolecules, 2005, vol. 38, p. 1829.
Kim, J., Novick, B.J., DeSimone, J.M., and Carbonell, R.G., Langmuir, 2006, vol. 22, p. 642.
Kim, J. and Carbonell, R.G., Langmuir, 2006, vol. 22, p. 2117.
Fukushima, Y. and Wakayama, H., J. Phys. Chem., B, 1999, vol. 103, p. 3062.
Watkins, J.J., Blackburn, J.M., and McCarthy, T.J., Chem. Mater., 1999, vol. 11, p. 213.
Ye, X.R., Wai, C.M., Zhang, D., et al., Chem. Mater., 2003, vol. 15, p. 83.
Cabanas, A., Shan, X., and Watkins, J.J., Chem. Mater., 2003, vol. 15, p. 2910.
Weinstein, R.D., Yan, D., and Jennings, G.K., Ind. Eng. Chem. Res., 2001, vol. 40, p. 2046.
Zemanian, T.S., Fryxell, G.E., Liu, J., et al., Langmuir, 2001, vol. 17, p. 8172.
Efimenko, K., Novick, B., Carbonell, R.G., et al., Langmuir, 2002, vol. 18, p. 6170.
Yan, D., Jennings, G.K., and Weinstein, R.D., Ind. Eng. Chem. Res., 2002, vol. 41, p. 4528.
Luscombe, C.K., Li, H.-W., Huck, W.T.S., and Holmes, A.B., Langmuir, 2003, vol. 19, p. 5273.
Gallyamov, M.O., Vinokur, R.A., Nikitin, L.N., et al., Phys. Low-Dimens. Struct., 2002, vols. 5–6, p. 153.
Gallyamov, M.O., Vinokur, R.A., Nikitin, L.N., et al., Langmuir, 2002, vol. 18, p. 6928.
Gallyamov, M.O., Yaminskii, I.V., Khokhlov, A.R., et al., Mikrosist. Tekh., 2003, no. 1, p. 31.
Gallyamov, M.O., Yaminskii, I.V., Khokhlov, A.R., et al., Mikrosist. Tekh., 2003, no. 2, p. 11.
Gallyamov, M.O., Bouznik, V.M., Tsvetnikov, A.K., et al., Khim. Fiz., 2004, vol. 23, no. 6, p. 76.
Shumilkina, N.A., Myakushev, V.D., Tatarinova, E.A., et al., Vysokomol. Soedin., Ser. A, 2006, vol. 48, p. 2102.
Gallyamov, M.O., Bouznik, V.M., Tsvetnikov, A.K., et al., Dokl. Akad. Nauk, 2003, vol. 392, p. 77.
Gallyamov, M.O., Bouznik, V.M., Tsvetnikov, A.K., et al., Polym. Prepr. (Am. Chem. Soc., Div. Polym. Chem.), 2004, vol. 45, p. 504.
McHale, G., Aqil, S., Shirtcliffe, N.J., et al., Langmuir, 2005, vol. 21, p. 11053.
Obraztsov, A.N., Zolotukhin, A.A., Ustinov, A.O., et al., Carbon, 2003, vol. 41, p. 836.
Zolotukhin, A.A., Obraztsov, A.N., Ustinov, A.O., and Volkov, A.P., Zh. Eksp. Teor. Fiz., 2003, vol. 124, p. 1291.
McHugh, M.A., Seckner, A.J., and Yogan, Th.J., Ind. Eng. Chem. Fundam., 1984, vol. 23, p. 493.
Yau, J.-S. and Tsai, F.-N., J. Chem. Eng. Data, 1993, vol. 38, p. 171.
Reverchon, E., Russo, P., and Stassi, A., J. Chem. Eng. Data, 1993, vol. 38, p. 458.
Chandler, K., Pouillot, F.L.L., and Eckert, C.A., J. Chem. Eng. Data, 1996, vol. 41, p. 6.
Muidinov, M.R., Ross. Khim. Zh., 2002, vol. 46, no. 3, p. 64.
Author information
Authors and Affiliations
Additional information
Original Russian Text & M.O. Gallyamov, L.N. Nikitin, A.Yu. Nikolaev, A.N. Obraztsov, V.M. Bouznik, A.R. Khokhlov, 2007, published in Kolloidnyi Zhurnal, 2007, Vol. 69, No. 4, pp. 448–462.
Rights and permissions
About this article
Cite this article
Gallyamov, M.O., Nikitin, L.N., Nikolaev, A.Y. et al. Formation of superhydrophobic surfaces by the deposition of coatings from supercritical carbon dioxide. Colloid J 69, 411–424 (2007). https://doi.org/10.1134/S1061933X07040035
Received:
Issue Date:
DOI: https://doi.org/10.1134/S1061933X07040035