Effect of hybrid-SiO2 particles on characterization of EPDM and silicone rubber composites for outdoor high-voltage insulations

  • Hidayatullah Khan EMAIL logo , Muhammad Amin , Muhammad Yasin , Muhammad Ali and Ayaz Ahmad

Abstract

Ethylene propylene diene monomer (EPDM) and silicone rubber (SiR) are well-known polymers for high-voltage (HV) outdoor applications. In this research work, the effect of hybrid SiO2 (a mixture of 15% microsized and 5% nanosized silica) has been investigated on the mechanical, thermal, and electrical properties of EPDM and SiR composites. Using the ASTM standard procedure, the EPDM and SiR composites filled with hybrid silica were compounded by two roll mill and simple blending techniques, respectively. It was observed that with the addition of hybrid SiO2, the composites exhibited improved tensile strength of ~2500 kPa, reduced elongation at break, and enhanced hardness. The samples filled with SiR hybrid silica showed higher thermal stability and volume/surface resistivities relative to EPDM hybrid composites. However, EPDM hybrid composites showed higher dielectric strength of ~23.4 kV/mm as compared with SiR composites. From these characterization results, it can be suggested that SiR hybrid composites are more suitable for outdoor HV insulation applications.

Acknowledgments

The authors of this work would like to express their gratitude to Prof. Raji Sundararajan of Purdue University, Lafayette, IN, for encouragement and valuable suggestions.

References

[1] Meichsner C, Clark T, Groeppel P, Winter B, Butz B, Spiecker E. IEEE Trans. Dielectr. Electr. Insul. 2012, 19, 786–792.10.1109/TDEI.2012.6215081Search in Google Scholar

[2] Cherney EA. IEEE Trans. Dielectr. Electr. Insul. 2005, 12, 1108–1115.10.1109/TDEI.2005.1561790Search in Google Scholar

[3] Moghadam MK, Morshedian J, Ehsani M, Bahrami M, Saddadi H. IEEE Trans. Dielectr. Electr. Insul. 2013, 20, 711–716.10.1109/TDEI.2013.6518939Search in Google Scholar

[4] Mackevich J, Shah M. IEEE Elect. Insul. Mag. 1997, 13, 5–12.10.1109/57.591510Search in Google Scholar

[5] Ehsani M, Borsi H, Gockenbach E, Bakhshandeh G, Morshedian J. Adv. Polym. Tech. 2005, 24, 51–61.10.1002/adv.20027Search in Google Scholar

[6] Ehsani M, Borsi H, Gockenbach E, Morshedian J, Bakhshandeh G. Eur. Polym. J. 2004, 40, 2495–2503.10.1016/j.eurpolymj.2004.03.014Search in Google Scholar

[7] Gjerde A. IEEE Elect. Insul. Mag. 1997, 13, 6–13.10.1109/57.567392Search in Google Scholar

[8] Prabu RR, Usa S, Udayakumar K, Abdullah Khan M, Majeed SSM. IEEE Trans. Dielectr. Electr. Insul. 2007, 14, 1207–1214.10.1109/TDEI.2007.4339481Search in Google Scholar

[9] Cherney EA. IEEE Elect. Insul. Mag. 2013, 29, 59–65.10.1109/MEI.2013.6648754Search in Google Scholar

[10] Wang Z, Jia ZD, Fang MH, Guan ZC. IEEE Trans. Dielectr. Electr. Insul. 2015, 22, 3357–3365.10.1109/TDEI.2015.005192Search in Google Scholar

[11] Ali M, Hackam R. IEEE Trans. Dielectr. Electr. Insul. 2009, 16, 842–852.10.1109/TDEI.2009.5128525Search in Google Scholar

[12] Yanfeng G, Jiafu W, Xidong L, Zhipeng Y, Yingyan L, Yuanji C. IEEE Trans. Dielectr. Electr. Insul. 2014, 21, 2428–2437.10.1109/TDEI.2014.004476Search in Google Scholar

[13] Momen G, Farzaneh M. Rev. Adv. Mater. Sci. 2011, 27, 13.Search in Google Scholar

[14] Rong MZ, Zhe YX, Friedrich K. Polymer 2001, 42, 4.10.1016/S0032-3861(00)00325-6Search in Google Scholar

[15] Douar MA, Beroual A, Souche X. IEEE Trans. Dielectr. Electr. Insul. 2015, 22, 1644–1653.10.1109/TDEI.2015.7116361Search in Google Scholar

[16] Pan G, Mark JE, Schaefer DW. J. Polym. Sci. A. Polym. Phys. 2003, 41, 3314–3323.10.1002/polb.10695Search in Google Scholar

[17] Baumann TF, Jones TV, Wilson T, Saab AP, Maxwell RS. J. Polym. Sci. A. Polym. Chem. 2009, 47, 2589–2596.10.1002/pola.23344Search in Google Scholar

[18] Moghadam MK, Morshedian J, Ehsani M, Laine RM, Lim Yan K, Umehara N. IEEE Trans. Dielectr. Electr. Insul. 2014, 21, 244–252.10.1109/TDEI.2013.004047Search in Google Scholar

[19] Jun-Wei Z, Zhi-Min D, Wei-Kang L, Yan-Hui Z, Chen G. IEEE Trans. Dielectr. Electr. Insul. 2014, 21, 1989–1996.10.1109/TDEI.2014.004330Search in Google Scholar

[20] Sim LC, Ramanan S, Ismail H, Seetharamu K, Goh T. Thermochim. Acta 2005, 430, 155–165.10.1016/j.tca.2004.12.024Search in Google Scholar

[21] Kemaloglu S, Ozkoc G, Aytac, A. Thermochim. Acta 2010, 499, 40–47.10.1016/j.tca.2009.10.020Search in Google Scholar

[22] Ramirez I, Cherney EA, Jarayam, S. IEEE Trans. Dielectr. Electr. Insul. 2012, 19, 218–224.10.1109/TDEI.2012.6148521Search in Google Scholar

[23] Ansorge S, Schmuck F, Aitken S, Papailiou K. Improved Performance of Silicone Rubbers for the Use in Composite Insulators. CIGRE, Paris, France, 2010.Search in Google Scholar

[24] Burditt N. In Proceedings of Mineral Fillers in Polymers. J. Griffiths, Ed., Metal Bulletin pic: London, UK, 1991.Search in Google Scholar

[25] Chen D, Liu Y, Huang C. Poly. Degrad. Stab. 2012, 97, 308–315.10.1016/j.polymdegradstab.2011.12.016Search in Google Scholar

[26] Yousafa I, Alib S, Mirzac S. “Ethylene-propylene-diene terpolymer vulcanizates’ reinforcement with precipitated silica.” 2013 10th International Bhurban Conference on Applied Sciences and Technology (IBCAST), 2013, pp. 43–46.10.1109/IBCAST.2013.6512128Search in Google Scholar

[27] Tan H, Isayev AI. J. Appl. Polym. Sci. 2008, 109, 767–774.10.1002/app.28130Search in Google Scholar

[28] Khattak A, Amin M. J. Polym. Eng. 2016, 36, 199–209.10.1515/polyeng-2015-0004Search in Google Scholar

[29] Hosier I, Rahman MA, Vaughan A, Krivda A, Kornmann X, Schmidt L. IEEE Trans. Dielectr. Electr. Insul. 2013, 20, 1808–1819.10.1109/TDEI.2013.6633712Search in Google Scholar

[30] Ansorge S, Schmuck F, Papailiou KO. IEEE Trans. Dielectr. Electr. Insul. 2015, 22, 979–988.10.1109/TDEI.2015.7076799Search in Google Scholar

[31] MoghadamMK, Morshedian J, Ehsani M, Laine RM, Kuang LY, Umehara N. IEEE Trans. Dielectr. Electr. Insul. 2014, 21, 244–252.10.1109/TDEI.2013.004047Search in Google Scholar

[32] ASTM D 3182-07: Standard Practice for Rubber-Materials, Equipment, and Procedures for Mixing Standard Compounds and Preparing Standard Vulcanized Sheets. ASTM Internaltional, 2007, p. 7.Search in Google Scholar

[33] ASTM D 1418-10a: Standard Practice for Rubber and Rubber Lattices Nomenclature. ASTM International, 2010, p. 3.Search in Google Scholar

[34] ASTM D 412-15a: Standard Test Methods for Vulcanized Rubber and Thermoplastic Elastomers – Tension. ASTM international, 2015, p. 14.Search in Google Scholar

[35] ASTM D 2240-10: Standard Test Method for Rubber Property-Durometer Hardness. ASTM International, 2010, p. 13.Search in Google Scholar

[36] ASTM D 149-13: Standard Test Method for Dielectric Breakdown Voltage and Dielectric Strength of Solid Electrical Insulation Materials at Commercial Power Frequencies. ASTM International 2013, p. 13.Search in Google Scholar

[37] ASTM D 257-05: Standard Test Methods for DC Resistance or Conductance of Insulating Materials. ASTM International, 2005, p. 18.Search in Google Scholar

[38] Ahmed K, Nizami SS, Raza NZ, Shirin K. Adv. Mater. Phys. Chem. 2012, 2, 90–97.10.4236/ampc.2012.22016Search in Google Scholar

[39] Kochetov R, Andritsch T, Morshuis PH, Smit JJ. IEEE Trans. Dielectr. Electr. Insul. 2012, 19, 107–117.10.1109/TDEI.2012.6148508Search in Google Scholar

[40] Patil S, Sharma RA, Chaudhari L, Bhattacharya S, Swain S, D’Melo D. IEEE Trans. Dielectr. Electr. Insul. 2013, 20, 988–994.10.1109/TDEI.2013.6518969Search in Google Scholar

[41] Ramirez I, Jayaram S, Cherney EA, Gauthier M, Simon L. IEEE Trans. Dielectr. Electr. Insul. 2009, 16, 52–59.10.1109/TDEI.2009.4784551Search in Google Scholar

[42] Masood A, Zuberi MU, Husain E. IEEE Trans. Dielectr. Electr. Insul. 2008, 15, 1051–1055.10.1109/TDEI.2008.4591227Search in Google Scholar

[43] Fairus M, Mansor NS, Hafiz M, Kamarol M, Mariatti M. “Investigation on dielectric strength of alumina nanofiller with SiR/EPDM composites for HV insulator.” 2015 IEEE 11th International Conference on the Properties and Applications of Dielectric Materials (ICPADM), 2015, pp. 923–926.10.1109/ICPADM.2015.7295424Search in Google Scholar

[44] Loganathan N, Muniraj C, Chandrasekar S. IEEE Trans. Dielectr. Electr. Insul. 2014, 21, 2172–2180.10.1109/TDEI.2014.003892Search in Google Scholar

[45] Hashiguchi T, Arise N, Otsubo M, Honda C, Takenouchi O. “Water absorption, hydrophobicity characteristics and surface change of polymer.” 2000 Annual Report Conference on Electrical Insulation and Dielectric Phenomena, 2000, Vol. 1, pp. 195–198.Search in Google Scholar

Received: 2016-4-4
Accepted: 2016-11-1
Published Online: 2016-12-15
Published in Print: 2017-8-28

©2017 Walter de Gruyter GmbH, Berlin/Boston

Downloaded on 16.5.2024 from https://www.degruyter.com/document/doi/10.1515/polyeng-2016-0102/html
Scroll to top button