Abstract
When bulk ferromagnetic Fe80P13C7 amorphous rods of approximately 2-mm diameter are compacted together in a hot press, a variety of different microstructures, depending on the experimental conditions, are produced. The most intriguing microstructure is that two different bulk amorphous rods can be fused together perfectly at a temperature of 683 K and under a pressure of 2.5 to 4 GPa for a period of 5 min.
References
W. Klement Jr., R.H. Willens, and P. Duwez, Nature 187, 869 (1960).
A. Inoue, Acta Mater. 48, 279 (2000).
W.L. Johnson, in Bulk Metallic Glasses, edited by W.L. Johnson, A. Inoue, and C.T. Liu (Mater. Res. Soc. Symp. Proc. 554, Warrendale, PA, 1999), p. 311.
R. Birringer, H. Gleiter, H.P. Klein, and P. Marquardt, Phys. Lett. A102, 365 (1984).
P.G. Sanders, J.A. Eastman, and J.R. Weertman, Acta Mater. 45, 4019 (1997).
A. Kojima, A Makino, and A. Inoue, IEEE Trans. Magn. 33, 3817 (1997).
D.V. Louzguine, Y. Kawamura, and A. Inoue, Mater. Sci. Technol. 15, 583 (1999).
F.W. Chan, Q. Li, and H.W. Kui (unpublished).
P. Duwez and S.C.H. Lin, J. Appl. Phys. 38, 4096 (1967).
H.W. Kui, A.L. Greer, and D. Turnbull, Appl. Phys. Lett. 45, 615 (1984).
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Chan, F.W., Ma, N.G. & Kui, H.W. Compaction of bulk ferromagnetic Fe80P13C7amorphous alloys. Journal of Materials Research 16, 2767–2769 (2001). https://doi.org/10.1557/JMR.2001.0377
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1557/JMR.2001.0377