Abstract
For the example of a disk–shoe frictional pair, it is shown that the use of cold-rolled carbon steel 45 with plasma quenching instead of heat-treated 40X structural steel not only reduces wear and expenditures on materials but also shortens the production process.
Similar content being viewed by others
References
Orlov, P.I., Osnovy konstruirovaniya: spravochno-metodicheskoe posobie (Principles of Engineering: Handbook), Uchaev, P.N., Ed., Moscow: Mashinostroenie, 1988, book 1.
Garkunov, D.N., Tribotekhnika (Frictional Engineering), Moscow: Mashinostroenie, 1989.
Safronov, E.N. and Zhuravlev, V.I., Surface reinforcing of iron-carbon alloys by arc quenching, Svarochnoe Proizvod., 1997, no. 10, pp. 30–32.
Korotkov, V.A., Plasma quenching of gears and slotted couplings, Russ. Eng. Res., 2009, vol. 29,no. 8, pp. 813–816.
Yong, X., Yu, D., Li, Q., et al., Effects of thermal plasma jet heat flux characteristics on surface hardening, J. Mater. Process. Technol., 2015, vol. 226, pp. 238–246.
Korotkov, V.A., Anan’ev, S.P., and Shekurov, A.V., The effect of cooling rate on the structure and mechanical properties at a plasma quenching, Svarochnoe Proizvod., 2013, no. 2, pp. 26–29.
Korotkov, V.A., Equipment for surface quenching, Khim. Neftegaz. Mashinostr., 2012, no. 11, pp. 43–45.
Spravochnik stalei i splavov (Handbook of Steels and Alloys), Zubchenko, A.S., Ed., Moscow: Mashinostroenie, 2003.
Kiselev, B.R., Illarionov, A.A., and Belov, V.V., Modernization of differential screw gear, Remont, Vosstanovlenie, Modernizatsiya, 2014, no. 11, pp. 25–28.
Author information
Authors and Affiliations
Corresponding author
Additional information
Original Russian Text © V.A. Korotkov, 2016, published in Vestnik Mashinostroeniya, 2016, No. 8, pp. 48–51.
About this article
Cite this article
Korotkov, V.A. Influence of plasma quenching on the wear resistance of 45 and 40X steel. Russ. Engin. Res. 36, 916–919 (2016). https://doi.org/10.3103/S1068798X16110125
Published:
Issue Date:
DOI: https://doi.org/10.3103/S1068798X16110125