Elevated Temperature Tensile Behavior of Rheo-Cast 7075-T6 Al Alloy Produced by GISS Technique

Article Preview

Abstract:

Tensile properties of rheo-cast 7075-T6 Al alloy produced by Gas Induced Semi-Solid (GISS) technique was investigated as a function of temperatures from 25°C to 250 °C in order to assess the potent of high temperature applications. It was found that the ultimate tensile strength and yield strength of the alloy decreased steadily with increasing temperature. There was loss in strength of about 33% at 200°C and 46% at 250 °C comparing to the strength at room temperature. At T = 250 °C, the ultimate tensile strength and yield strength of the rheo-cast 7075-T6 Al alloy were higher than those of the wrought 7075-T651 Al alloy. Keyword: 7075 Al alloy; Gas Induced Semi Solid (GISS) technique; Elevated temperature tensile.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 881-883)

Pages:

1597-1600

Citation:

Online since:

January 2014

Export:

Price:

* - Corresponding Author

[1] S. Thanabumrungkul, S. Janudom, R. Burapa, P. Dulyapraphant, J. Wannasin, Trans. Nonferrous Met. Soc. China 20 (2010) s1016–s1021.

DOI: 10.1016/s1003-6326(10)60623-1

Google Scholar

[2] J. Wannasin, S. Janudom, T. Rattanochaikul, R. Canyook, R. Burapa, T. Chucheep, S. Thanabumrungkul, Trans. Nonferrous Met. Soc. China 20 (2010) s1010–s1015.

DOI: 10.1016/s1003-6326(10)60622-x

Google Scholar

[3] N. Mahathaninwong, T. Plookphol, J. Wannasin, S. Wisutmethangoon., Mater. Sci. Eng. A 532 (2012) 91–99.

DOI: 10.1016/j.msea.2011.10.068

Google Scholar

[4] ASM Metals handbook, Properties and Selection: Nonferrous Alloy and Special-Purpose Materials, Vol. 2, ASM International, USA, (1991).

DOI: 10.31399/asm.hb.v02.9781627081627

Google Scholar

[5] N. Mahathaninwong, T. Plookphol, J. Wannasin, S. Wisutmethangoon., Mater. Sci. Eng. A 556 (2012) 107–113.

Google Scholar

[6] A. Deschamps, F. Livet, Y. Breachet, Acta Mater. 47 (1999) 281–292.

Google Scholar