Abstract:

High performance rigid cross-linked PVC foam has been prepared by molding process and boiling foam process with the main materials including polyvinyl chloride paste resin (PVC), liquefied methylene bis-phenyl diisocyanate (MDI-L) and methylhexahydrophthalic anhydride (MHHPA). The chemical structure, cellular structure and thermal properties were respectively characterized by fourier transform infrared spectrometer (FTIR), scanning electron microscopy (SEM), thermomechanical analyzer (TMA) and thermogravimetric analyzer (TGA). Results showed that the foam had a uniform cellular structure, and cell size was about 760μm. The glass transition temperature (Tg) was 81°C and 5% weight loss temperature (T5d) was 252°C.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 311-313)

Pages:

1056-1060

Citation:

Online since:

August 2011

Export:

Price:

[1] L.Leone, E.P. Patent 0,458,404. (1990).

Google Scholar

[2] Information on http://www.diabgroup.com

Google Scholar

[3] M.F. Cao, P.Hu: Jiangsu Ship (in Chinese), Vol.21 (2004), p.3.

Google Scholar

[4] L.Leone, S.A. Sam, J.C.S. Jan and B.Raffaela, U.S. Patent 0, 068, 487. (2010).

Google Scholar

[5] M.Elser, U.S. Patent 0,200,266. (2007).

Google Scholar

[6] Y.H. Yan, Z.G. Huang, Q.Zhou: Journal of Qingdao Institute of Chemical Technology (in Chinese), Vol.20 (1999), p.208.

Google Scholar

[7] M.Danielsson, J.L. Grenested: Composites Part A: Applied Science and Manufacturing. Vol.29 (1998), p.983.

Google Scholar

[8] Y.Y.Wu, J.Y.Xu: Foam Plastics Molding (Chemical Industry Press, China1999).

Google Scholar