Abstract:

Fusion casting has been commercially available for over 3 years. Although there are many interesting points to casting, there are several downstream considerations such as scalping, preheat and rolling. Quality rolled clad sheet needs to have a consistent clad thickness. Appropriately varying the geometry of the clad layer during the transient portions of casting results in consistent clad thickness from head to butt. Controlling the edge wipe during rolling off does the same from edge to edge. The severity of edge wipe off can be predicted from relative flow stresses at rolling temperatures and guides the choice of alloy combinations.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

175-178

Citation:

Online since:

October 2009

Export:

Price:

[1] Graham, M.B., Pruitt, W. and Pruitt, B. H. (1990) R&D for Industry A Century of Technical Innovation at Alcoa, p.144, 145.

Google Scholar

[2] Miller, M.A. (1952) Aluminous Brazing Product and Method of Brazing, US Patent 2, 602, 413 July 8, (1952).

Google Scholar

[3] Sturgell, B.W. (2006) Breaking the Barriers: Unlocking New Possibilities for Aluminum, presentation at CRU 11 th World Aluminum Conference, Montreal, June (2006).

Google Scholar

[4] Anderson, M.D. et al. (2005) Method for Casting Composite Ingot, US Patent Filing 20050011630, January 20, (2005).

Google Scholar

[5] Hudson, L.G. et al. (2007) Direct Chill Casting of Heat Exchanger Material Via the Novelis Fusion ™ Process, Light Metals, p.739.

Google Scholar

[6] Wagstaff, R.B. and Fenton, W.J. (2007) Homogenization and Heat-Treatment of Cast Metals, US Patent Filing 20070102136, May 10, (2007).

Google Scholar

[7] Prasad, Y.V.R.K. and Sasidhara, S. (1997) Hot Working Guide, A Compendium of Processing Maps, ASM International, 92-103.

Google Scholar