Abstract

Unsatisfactory dimensional control, distortion, and defects are frequently observed in powder-injection-molded parts, particularly after the solvent and thermal-debinding processing steps. One of the reasons is that the amount of soluble binder removed during the first step, solvent debinding, is not great enough to form interconnected pores throughout the compact, particularly in the core region. Thus, blistering, cracking, and bubbles can form easily during the subsequent thermal debinding. To determine the minimum debinding fraction required for solvent debinding, at which point interconnected pore channels are formed at the center, modeling of the distribution of the remaining soluble binder in the compact was established. The actual distribution, which was obtained by measuring the binder content layer by layer with the soxhelt extraction method, is in good agreement with the model. The modeling, bubble test, and fluorescence dye-penetration analysis show that, regardless of the compact thickness, the minimum bulk debinding fraction needed is consistently approximately 59 pct, yielding a local debinding fraction of 37 pct and a porosity of 8.5 pct at the center. This porosity is close to the value at which pores in a sintered compact transform from open to closed at the beginning of the final stage of sintering.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
1.
Zurück zum Zitat R.M. German, and A. Bose: Injection Molding of Metals and Ceramics, Metal Powder Industries Federation, Princeton, NJ, 1997, pp. 11–13 R.M. German, and A. Bose: Injection Molding of Metals and Ceramics, Metal Powder Industries Federation, Princeton, NJ, 1997, pp. 11–13
2.
Zurück zum Zitat R.M. German: Int. J. Powder Metall., 1987, vol. 23, pp. 237–45 R.M. German: Int. J. Powder Metall., 1987, vol. 23, pp. 237–45
3.
Zurück zum Zitat C.E. Finn: Int. J. Powder Metall., 1991, vol. 27, pp. 127–32 C.E. Finn: Int. J. Powder Metall., 1991, vol. 27, pp. 127–32
4.
Zurück zum Zitat M. Bloemacher, and D. Weinand: J. Mater. Process. Technol., 1997, vol. 63, pp. 918–22CrossRef M. Bloemacher, and D. Weinand: J. Mater. Process. Technol., 1997, vol. 63, pp. 918–22CrossRef
5.
Zurück zum Zitat K S. Hwang, and Y.M. Hsieh: Metall. Mater. Trans. A, 1996, vol. 27A, pp. 245–53CrossRefADS K S. Hwang, and Y.M. Hsieh: Metall. Mater. Trans. A, 1996, vol. 27A, pp. 245–53CrossRefADS
6.
Zurück zum Zitat M.J. Cima, J.A. Lewis, and D. Devoe: J. Am. Ceram. Soc., 1989, vol. 72, pp. 1192–99CrossRef M.J. Cima, J.A. Lewis, and D. Devoe: J. Am. Ceram. Soc., 1989, vol. 72, pp. 1192–99CrossRef
7.
Zurück zum Zitat H.-H. Angermann, and O. Van Der Biest: Int. J. Powder. Metall., 1993, vol. 29, pp. 239–50 H.-H. Angermann, and O. Van Der Biest: Int. J. Powder. Metall., 1993, vol. 29, pp. 239–50
8.
Zurück zum Zitat K.S. Hwang, and T.H. Tsou: Metall. Trans. A, 1992, vol. 23A, pp. 2775–82ADS K.S. Hwang, and T.H. Tsou: Metall. Trans. A, 1992, vol. 23A, pp. 2775–82ADS
9.
Zurück zum Zitat E.J. Westcot, C. Binet, and R.M. German: Powder Metall., 2003, vol. 46, pp. 61–67CrossRef E.J. Westcot, C. Binet, and R.M. German: Powder Metall., 2003, vol. 46, pp. 61–67CrossRef
10.
Zurück zum Zitat S.T. Lin, and R.M. German: Powder Metall. Int., 1989, vol. 21, pp. 19–24 S.T. Lin, and R.M. German: Powder Metall. Int., 1989, vol. 21, pp. 19–24
11.
12.
Zurück zum Zitat B. Zhu, X. Qu, and Y. Tao: Mater. Process. Technol., 2003, vol. 142, pp. 487–92CrossRef B. Zhu, X. Qu, and Y. Tao: Mater. Process. Technol., 2003, vol. 142, pp. 487–92CrossRef
13.
Zurück zum Zitat T.S. Shivashankar, and R.M. German: J. Am. Ceram. Soc., 1999, vol. 85, pp. 1146–52 T.S. Shivashankar, and R.M. German: J. Am. Ceram. Soc., 1999, vol. 85, pp. 1146–52
14.
Zurück zum Zitat M.R. Barone, and J.C. Ulicny: J. Am. Ceram. Soc., 1990, vol. 73, pp. 3323–33CrossRef M.R. Barone, and J.C. Ulicny: J. Am. Ceram. Soc., 1990, vol. 73, pp. 3323–33CrossRef
15.
Zurück zum Zitat Y. Li, F. Jiang, L. Zhao, and B. Huang: Mater. Sci. Eng., A, 2003, vol. 362, pp. 292–99CrossRef Y. Li, F. Jiang, L. Zhao, and B. Huang: Mater. Sci. Eng., A, 2003, vol. 362, pp. 292–99CrossRef
16.
Zurück zum Zitat ASTM Standards B328-96, Standard Test Method for Density, Oil Content, and Interconnected Porosity of Sintered Metal Structural Parts and Oil-Impregnated Bearings, ASTM International, West Conshohocken, PA, 2003 ASTM Standards B328-96, Standard Test Method for Density, Oil Content, and Interconnected Porosity of Sintered Metal Structural Parts and Oil-Impregnated Bearings, ASTM International, West Conshohocken, PA, 2003
17.
Zurück zum Zitat ASTM Standards E128-99, Standard Test Method for Maximum Pore Diameter and Permeability of Rigid Porous Filters for Laboratory Use, ASTM International, West Conshohocken, PA, 2005 ASTM Standards E128-99, Standard Test Method for Maximum Pore Diameter and Permeability of Rigid Porous Filters for Laboratory Use, ASTM International, West Conshohocken, PA, 2005
18.
Zurück zum Zitat J. Crank: The Mathematics of Diffusion, 2nd ed., Clarendon Press, Oxford, UK, 1975, pp. 47–48 J. Crank: The Mathematics of Diffusion, 2nd ed., Clarendon Press, Oxford, UK, 1975, pp. 47–48
19.
Zurück zum Zitat R.M. German: Sintering Theory and Practice, John Wiley & Sons, Inc., New York, NY, 1996, pp. 155–56 R.M. German: Sintering Theory and Practice, John Wiley & Sons, Inc., New York, NY, 1996, pp. 155–56
Metadaten
Titel
Minimum Amount of Binder Removal Required during Solvent Debinding of Powder-Injection-Molded Compacts
verfasst von
Yang-Liang Fan
Kuen-Shyang Hwang
Shiau-Han Wu
Yau-Ching Liau
Publikationsdatum
01.04.2009
Verlag
Springer US
Erschienen in
Metallurgical and Materials Transactions A / Ausgabe 4/2009
Print ISSN: 1073-5623
Elektronische ISSN: 1543-1940
DOI
https://doi.org/10.1007/s11661-008-9760-6

Weitere Artikel der Ausgabe 4/2009

Metallurgical and Materials Transactions A 4/2009 Zur Ausgabe

    Marktübersichten

    Die im Laufe eines Jahres in der „adhäsion“ veröffentlichten Marktübersichten helfen Anwendern verschiedenster Branchen, sich einen gezielten Überblick über Lieferantenangebote zu verschaffen.