Special Features of the Structure of Laser-Welded Joints of Dissimilar Alloys Based on Titanium and Aluminum

verfasst von: A. A. Nikulina, A. I. Smirnov, G. A. Turichin, O. G. Klimova-Korsmik, K. D. Babkin

Erschienen in: Metal Science and Heat Treatment | Ausgabe 7-8/2017

Einloggen

Aktivieren Sie unsere intelligente Suche, um passende Fachinhalte oder Patente zu finden.

search-config
loading …

Abstract

The structure of laser-welded joints of parts having different thicknesses fabricated from alloys based on aluminum and titanium has been studied. Results of transmission and scanning electron microscopy measurements and x-ray diffraction analysis show that the diffusion interaction of microvolumes of two alloys in the weld leads to the formation of two interlayers: (i) a continuous intermetallic TiAl layer with thickness below 1 μm adjacent to the titanium alloy and (ii) a layer consisting of TiAl3 intermetallic dendrites with thickness of 2 – 6 μm adjacent to the TiAl layer. The average microhardness of the intermetallic layer is about 490 HV.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
1.
Zurück zum Zitat V. R. Ryabov and D. M. Rabkin, Welding of Dissimilar Materials [in Russian], Mashinostroenie, Moscow (1984), 239 p. V. R. Ryabov and D. M. Rabkin, Welding of Dissimilar Materials [in Russian], Mashinostroenie, Moscow (1984), 239 p.
2.
Zurück zum Zitat S. M. Gurevich, Handbook on Welding of Non-Ferrous Metals [in Russian], Naukova Dumka, Kiev (1990), 512 p. S. M. Gurevich, Handbook on Welding of Non-Ferrous Metals [in Russian], Naukova Dumka, Kiev (1990), 512 p.
3.
Zurück zum Zitat G. A. Turichin, O. G. Klimova, and K. D. Babkin, “Peculiarities of structure formation in laser-welded joints between dissimilar materials of Al – Cu and Al –Ti systems,” Tsvetn. Met., No. 4, 45 – 50 (2014). G. A. Turichin, O. G. Klimova, and K. D. Babkin, “Peculiarities of structure formation in laser-welded joints between dissimilar materials of Al – Cu and Al –Ti systems,” Tsvetn. Met., No. 4, 45 – 50 (2014).
4.
Zurück zum Zitat V. A. Bataev, A. A. Nikulina, and A. A. Bataev, “The investigation of fracture processes in heterogeneous steels joined by the method of contact welding,” in: Proc. of the 3rd Int. IEEE Forum on Strategic Technologies (IFOST-2008), Novosibirsk – Tomsk (2008), pp. 75 – 76. V. A. Bataev, A. A. Nikulina, and A. A. Bataev, “The investigation of fracture processes in heterogeneous steels joined by the method of contact welding,” in: Proc. of the 3rd Int. IEEE Forum on Strategic Technologies (IFOST-2008), Novosibirsk – Tomsk (2008), pp. 75 – 76.
5.
Zurück zum Zitat A. Nikulina, A. Smirnov, and A. Chevakinskaya, “Formation of a transition zone structure in welded joints between dissimilar steels,” Appl. Mech. Mater., 698, 283 – 287 (2015).CrossRef A. Nikulina, A. Smirnov, and A. Chevakinskaya, “Formation of a transition zone structure in welded joints between dissimilar steels,” Appl. Mech. Mater., 698, 283 – 287 (2015).CrossRef
6.
Zurück zum Zitat W. Chuaiphan, S. Chandra-Ambhorn, S. Niltawach, and B. Sornil, “Dissimilar Welding between AISI 304 Stainless steel and AISI 1020 carbon steel plates,” Appl. Mech. Mater., 268 – 270, 283 – 290 (2013). W. Chuaiphan, S. Chandra-Ambhorn, S. Niltawach, and B. Sornil, “Dissimilar Welding between AISI 304 Stainless steel and AISI 1020 carbon steel plates,” Appl. Mech. Mater., 268 – 270, 283 – 290 (2013).
7.
Zurück zum Zitat B. Majumdar, R. Galun, A. Weisheit, and B. L. Mordike, ”Formation of a crack-free joint between Ti alloy and Al alloy by using a high-power CO2 laser,” J. Mater. Sci., 32, 6191 – 6200 (1997).CrossRef B. Majumdar, R. Galun, A. Weisheit, and B. L. Mordike, ”Formation of a crack-free joint between Ti alloy and Al alloy by using a high-power CO2 laser,” J. Mater. Sci., 32, 6191 – 6200 (1997).CrossRef
8.
Zurück zum Zitat Y. Mishin and Chr. Herzig, “Diffusion in Al – Ti system,” Acta Mater., 48, 589 – 623 (2000).CrossRef Y. Mishin and Chr. Herzig, “Diffusion in Al – Ti system,” Acta Mater., 48, 589 – 623 (2000).CrossRef
9.
Zurück zum Zitat S. Chen, L. Li, Y. Chen, et al., “Improving interfacial reaction nonhomogeneity during laser welding-brazing aluminum to titanium,” Mater. Design, 32, 4408 – 4416 (2011).CrossRef S. Chen, L. Li, Y. Chen, et al., “Improving interfacial reaction nonhomogeneity during laser welding-brazing aluminum to titanium,” Mater. Design, 32, 4408 – 4416 (2011).CrossRef
10.
Zurück zum Zitat Y. Chen, S. Chen, and L. Li, “Effects of heat input on microstructure and mechanical properties of Al – Ti joints by rectangular spot laser welding-brazing method,” Int. J. Adv. Manuf. Technol., 44, 265 – 272 (2009).CrossRef Y. Chen, S. Chen, and L. Li, “Effects of heat input on microstructure and mechanical properties of Al – Ti joints by rectangular spot laser welding-brazing method,” Int. J. Adv. Manuf. Technol., 44, 265 – 272 (2009).CrossRef
11.
Zurück zum Zitat Z. Song, K. Nakata, A.Wu, and J. Liao, “Interfacial microstructure and mechanical properties of Ti6Al4V/A6061 dissimilar joint by direct laser brazing without filler metal and groove,” Mater. Sci. Eng. A, 560, 111 – 120 (2013).CrossRef Z. Song, K. Nakata, A.Wu, and J. Liao, “Interfacial microstructure and mechanical properties of Ti6Al4V/A6061 dissimilar joint by direct laser brazing without filler metal and groove,” Mater. Sci. Eng. A, 560, 111 – 120 (2013).CrossRef
12.
Zurück zum Zitat S. Chen, L. Li, Y. Chen, and J. Huang, “Joining mechanism of Ti/Al dissimilar alloys during laser welding-brazing process,” J. Alloys Compds., 509, 891 – 898 (2011).CrossRef S. Chen, L. Li, Y. Chen, and J. Huang, “Joining mechanism of Ti/Al dissimilar alloys during laser welding-brazing process,” J. Alloys Compds., 509, 891 – 898 (2011).CrossRef
13.
Zurück zum Zitat M. Gao, C. Chen, Y. Gu, and X. Zeng, “Microstructure and tensile behavior of laser arc hybrid welded dissimilar Al and Ti alloys,” Materials, 7, 1590 – 1602 (2014).CrossRef M. Gao, C. Chen, Y. Gu, and X. Zeng, “Microstructure and tensile behavior of laser arc hybrid welded dissimilar Al and Ti alloys,” Materials, 7, 1590 – 1602 (2014).CrossRef
14.
Zurück zum Zitat S. H. Chen, L. Q. Li, and Y. B. Chen, “Interfacial reaction mode and its influence on tensile strength in laser joining Al alloy to Ti alloy,” Mater. Sci. Technol., 2, 230 – 235 (2010).CrossRef S. H. Chen, L. Q. Li, and Y. B. Chen, “Interfacial reaction mode and its influence on tensile strength in laser joining Al alloy to Ti alloy,” Mater. Sci. Technol., 2, 230 – 235 (2010).CrossRef
15.
Zurück zum Zitat Y. Chen, S. Chen, and L. Li, “Influence of interfacial reaction layer morphologies on crack initiation and propagation in Ti/Al joint by laser welding-brazing,” Mater. Design, 31, 227 – 233 (2010).CrossRef Y. Chen, S. Chen, and L. Li, “Influence of interfacial reaction layer morphologies on crack initiation and propagation in Ti/Al joint by laser welding-brazing,” Mater. Design, 31, 227 – 233 (2010).CrossRef
16.
Zurück zum Zitat Y. Wei, W. Aiping, Z. Guisheng, and R. Jialie, “Formation process of the bonding joint in Ti/Al diffusion bonding,” Mater. Sci. Eng. A, 480, 456 – 463 (2008).CrossRef Y. Wei, W. Aiping, Z. Guisheng, and R. Jialie, “Formation process of the bonding joint in Ti/Al diffusion bonding,” Mater. Sci. Eng. A, 480, 456 – 463 (2008).CrossRef
17.
Zurück zum Zitat W. Shouzheng, L. Yajiang, W. Juan, and L. Kun, “Improving of interfacial microstructure of Ti/Al joint during GTA welding by adopting pulsed current,” Int. J. Adv. Manuf. Technol., 73, 1307 – 1312 (2014).CrossRef W. Shouzheng, L. Yajiang, W. Juan, and L. Kun, “Improving of interfacial microstructure of Ti/Al joint during GTA welding by adopting pulsed current,” Int. J. Adv. Manuf. Technol., 73, 1307 – 1312 (2014).CrossRef
18.
Zurück zum Zitat W. Shouzheng, L. Yajiang, W. Juan, et al., “Microstructure and joining mechanism of Ti/Al dissimilar joint by pulsed gas metal arc welding,” Int. J. Adv. Manuf. Technol., 70, 1137 – 1142 (2014).CrossRef W. Shouzheng, L. Yajiang, W. Juan, et al., “Microstructure and joining mechanism of Ti/Al dissimilar joint by pulsed gas metal arc welding,” Int. J. Adv. Manuf. Technol., 70, 1137 – 1142 (2014).CrossRef
19.
Zurück zum Zitat Y. C. Chen and K. Nakata, “Microstructural characterization and mechanical properties in friction stir welding of aluminum and titanium dissimilar alloys,” Mater. Design, 30, 469 – 474 (2009).CrossRef Y. C. Chen and K. Nakata, “Microstructural characterization and mechanical properties in friction stir welding of aluminum and titanium dissimilar alloys,” Mater. Design, 30, 469 – 474 (2009).CrossRef
20.
Zurück zum Zitat W. H. Sohn, H. H. Bong, and S. H. Hong, “Microstructure and bonding mechanism of Al – Ti bonded joint using Al – 10Si – 1Mg filler metal,” Mater Sci. Eng. A, 355, 231 – 240 (2003).CrossRef W. H. Sohn, H. H. Bong, and S. H. Hong, “Microstructure and bonding mechanism of Al – Ti bonded joint using Al – 10Si – 1Mg filler metal,” Mater Sci. Eng. A, 355, 231 – 240 (2003).CrossRef
21.
Zurück zum Zitat S. H. Chen, L. Q. Li, Y. B. Chen, and D. J. Liu, “Silicon diffusion behavior during laser welding-brazing of Al alloy and Ti alloy with Al – 12Si filler wire,” Trans. Nonferrous Met. Soc. China, 20, 64 – 70 (2010).CrossRef S. H. Chen, L. Q. Li, Y. B. Chen, and D. J. Liu, “Silicon diffusion behavior during laser welding-brazing of Al alloy and Ti alloy with Al – 12Si filler wire,” Trans. Nonferrous Met. Soc. China, 20, 64 – 70 (2010).CrossRef
22.
Zurück zum Zitat L. Xu, Y. Y. Cui, Y. L. Hao, and R. Yang, “Growth of intermetallic layer in multilaminated Ti/Al diffusion couples,” Mater. Sci. Eng. A, 435 – 436, 638 – 647 (2006).CrossRef L. Xu, Y. Y. Cui, Y. L. Hao, and R. Yang, “Growth of intermetallic layer in multilaminated Ti/Al diffusion couples,” Mater. Sci. Eng. A, 435 – 436, 638 – 647 (2006).CrossRef
23.
Zurück zum Zitat M. A. Gureeva, O. E. Grushko, and V. V. Ovchinnikov, “Weldable aluminum alloys in structures of transport vehicles,” Zagot. Proizvod. Mashinostr., No. 3, 11 – 22 (2009). M. A. Gureeva, O. E. Grushko, and V. V. Ovchinnikov, “Weldable aluminum alloys in structures of transport vehicles,” Zagot. Proizvod. Mashinostr., No. 3, 11 – 22 (2009).
24.
Zurück zum Zitat V. S. Kovalenko, Metallographic Reagents [in Russian], Metallurgiya, Moscow (1981), 120 p. V. S. Kovalenko, Metallographic Reagents [in Russian], Metallurgiya, Moscow (1981), 120 p.
25.
Zurück zum Zitat V. I. Makhnenko and A. S. Milenin, “Mathematical modeling of reactive diffusion processes in welding-brazing of titanium – aluminum lap joints,” Avtomat. Svarka, No. 10, 5 – 9 (2007). V. I. Makhnenko and A. S. Milenin, “Mathematical modeling of reactive diffusion processes in welding-brazing of titanium – aluminum lap joints,” Avtomat. Svarka, No. 10, 5 – 9 (2007).
26.
Zurück zum Zitat J. C. Schuster and M. Palm, “Reassessment of the binary aluminum-titanium phase diagram,” J. Phase Equilib. Diffus., 27, 255 – 277 (2006).CrossRef J. C. Schuster and M. Palm, “Reassessment of the binary aluminum-titanium phase diagram,” J. Phase Equilib. Diffus., 27, 255 – 277 (2006).CrossRef
27.
Zurück zum Zitat F. Zhang, S. L. Chen, Y. A. Chang, and U. R. Kattner, “A thermodynamic description of the Ti – Al system,” Intermetallics, 5, 471 – 482 (1997).CrossRef F. Zhang, S. L. Chen, Y. A. Chang, and U. R. Kattner, “A thermodynamic description of the Ti – Al system,” Intermetallics, 5, 471 – 482 (1997).CrossRef
28.
Zurück zum Zitat M. Sujata, S. Bhargava, and S. Sangal, “On the formation of TiAl3 during reaction between solid Ti and liquid Al,” J. Mater. Sci. Lett., 16, 1175 – 1178 (1997). M. Sujata, S. Bhargava, and S. Sangal, “On the formation of TiAl3 during reaction between solid Ti and liquid Al,” J. Mater. Sci. Lett., 16, 1175 – 1178 (1997).
Metadaten
Titel
Special Features of the Structure of Laser-Welded Joints of Dissimilar Alloys Based on Titanium and Aluminum
verfasst von
A. A. Nikulina
A. I. Smirnov
G. A. Turichin
O. G. Klimova-Korsmik
K. D. Babkin
Publikationsdatum
11.11.2017
Verlag
Springer US
Erschienen in
Metal Science and Heat Treatment / Ausgabe 7-8/2017
Print ISSN: 0026-0673
Elektronische ISSN: 1573-8973
DOI
https://doi.org/10.1007/s11041-017-0185-y

Weitere Artikel der Ausgabe 7-8/2017

Metal Science and Heat Treatment 7-8/2017 Zur Ausgabe

    Marktübersichten

    Die im Laufe eines Jahres in der „adhäsion“ veröffentlichten Marktübersichten helfen Anwendern verschiedenster Branchen, sich einen gezielten Überblick über Lieferantenangebote zu verschaffen.