Skip to main content
Top

2021 | OriginalPaper | Chapter

Wear Behaviour of PCBN, PCD, Binderless PCBN and Cemented Carbide Cutting Inserts When Machining Ti-6Al-4V in an Oxygen-Free Atmosphere

Authors : F. Schaper, B. Denkena, M.-A. Dittrich, A. Krödel, J. Matthies, S. Worpenberg

Published in: Production at the leading edge of technology

Publisher: Springer Berlin Heidelberg

Activate our intelligent search to find suitable subject content or patents.

search-config
loading …

Abstract

One approach to overcome the difficulties in machining titanium can be the selection of a suitable cutting material. However, influences of the chemical tool wear under machining atmosphere has not been considered jet. In this work the tribochemical wear resistance of uncoated carbide tools, polycrystalline cubic boron nitride (PCBN) tools polycrystalline binderless CBN tools, and polycrystalline diamond (PCD) tools is investigated under different atmospheric conditions cutting Ti-6Al-4V. Air, pure argon and silane-doped argon are used to determine the influence of oxygen contents on tool wear. It was found that oxidation and adhesion behaviour were influenced by oxygen content. Up to 33% increase in tool live were obtained with uncoated carbide- and the PCBN tools with high CBN content. The reduced oxidation also affects PCBN tool behaviour. During machining under oxygen-free conditions increased adhesion of Ti-6Al-4V occurs. The increased wear behaviour for binderless PCBN tools lead to significantly reduced tool life.

Dont have a licence yet? Then find out more about our products and how to get one now:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Springer Professional "Wirtschaft"

Online-Abonnement

Mit Springer Professional "Wirtschaft" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 340 Zeitschriften

aus folgenden Fachgebieten:

  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Versicherung + Risiko




Jetzt Wissensvorsprung sichern!

Literature
1.
go back to reference Denkena, B., Dege, J.H., Groppe, M., Grove, T.: Zerspanbarkeit von β-Titanlegierungen. VDI-Z Special Werkzeuge, pp. 24–27 (2010) Denkena, B., Dege, J.H., Groppe, M., Grove, T.: Zerspanbarkeit von β-Titanlegierungen. VDI-Z Special Werkzeuge, pp. 24–27 (2010)
2.
go back to reference Shaw, M.C.: Metal Cutting Principles. Oxford University Press, Oxford (2005) Shaw, M.C.: Metal Cutting Principles. Oxford University Press, Oxford (2005)
3.
go back to reference Sun, S., Brandt, M., Dargusch, M.S.: Machining Ti-6Al-4V alloy with cryogenic compressed air cooling. Int. J. Mach. Tools Manuf. 50, 933–942 (2010)CrossRef Sun, S., Brandt, M., Dargusch, M.S.: Machining Ti-6Al-4V alloy with cryogenic compressed air cooling. Int. J. Mach. Tools Manuf. 50, 933–942 (2010)CrossRef
4.
go back to reference Chim, Y.C., Ding, X.Z., Zeng, X.T.: Oxidation resistance of TiN, CrN, TiAlN and CrAlN coatings deposited by lateral rotating cathode arc. Thin Solid Films 517, 4845–4849 (2009)CrossRef Chim, Y.C., Ding, X.Z., Zeng, X.T.: Oxidation resistance of TiN, CrN, TiAlN and CrAlN coatings deposited by lateral rotating cathode arc. Thin Solid Films 517, 4845–4849 (2009)CrossRef
5.
go back to reference Aspinwall, D.K., Dewes, R.C., Manfle, A.L.: The machining of γ-TiAl intermetallic alloys. CIRP Ann. 54(1), 99–104 (2005)CrossRef Aspinwall, D.K., Dewes, R.C., Manfle, A.L.: The machining of γ-TiAl intermetallic alloys. CIRP Ann. 54(1), 99–104 (2005)CrossRef
6.
go back to reference Denkena, B., Köhler, J., Behrens, L.: Methoden zur Bewertung der Verschleißmechanismen beim Schleifen von PCBN-Wendeschneidplatten, Jahrbuch Schleifen, Honen, Läppen, Polieren: Verfahren und Maschinen, 66th edn. Denkena, B., Hoffmeister, H.-W., Vulkan (2014) Denkena, B., Köhler, J., Behrens, L.: Methoden zur Bewertung der Verschleißmechanismen beim Schleifen von PCBN-Wendeschneidplatten, Jahrbuch Schleifen, Honen, Läppen, Polieren: Verfahren und Maschinen, 66th edn. Denkena, B., Hoffmeister, H.-W., Vulkan (2014)
7.
go back to reference Denkena, B., Grove, T., Behrens, L., Müller-Cramm, D.: Wear mechanism model for grinding of PcBN cutting inserts. J. Mater. Process. Tech. 277, 116474 (2010)CrossRef Denkena, B., Grove, T., Behrens, L., Müller-Cramm, D.: Wear mechanism model for grinding of PcBN cutting inserts. J. Mater. Process. Tech. 277, 116474 (2010)CrossRef
8.
go back to reference Uhlmann, E., Herter, S.: Studies on conventional cutting of intermetallic nickel and titanium aluminides. Proc. Inst. Mech. Eng. [B]: J. Eng. Manuf. 220, 1391–1398 (2006)CrossRef Uhlmann, E., Herter, S.: Studies on conventional cutting of intermetallic nickel and titanium aluminides. Proc. Inst. Mech. Eng. [B]: J. Eng. Manuf. 220, 1391–1398 (2006)CrossRef
9.
10.
go back to reference Wang, Z.G., Ragman, M., Wong, Y.S.: Tool wear characteristics of binderless CBN tools used in high-speed milling of titanium alloys. Wear 258, 752–758 (2005)CrossRef Wang, Z.G., Ragman, M., Wong, Y.S.: Tool wear characteristics of binderless CBN tools used in high-speed milling of titanium alloys. Wear 258, 752–758 (2005)CrossRef
11.
go back to reference Mercer, A.P., Hutchings, I.M.: The influence of atmospheric composition on the abrasive wear of titanium and Ti-6Al-4V. Wear 124, 165–176 (1988)CrossRef Mercer, A.P., Hutchings, I.M.: The influence of atmospheric composition on the abrasive wear of titanium and Ti-6Al-4V. Wear 124, 165–176 (1988)CrossRef
12.
go back to reference Katuku, K., Koursaris, A., Sigals, I.: High-temperature stability of polycrystalline cubic boron nitride cutting tool materials in air. Corros. Sci. 64, 55–63 (2023)CrossRef Katuku, K., Koursaris, A., Sigals, I.: High-temperature stability of polycrystalline cubic boron nitride cutting tool materials in air. Corros. Sci. 64, 55–63 (2023)CrossRef
13.
go back to reference Bagnall, C., Capo, J., Moorhead, W.J.: Oxidation behavior of tungsten carbide-6% cobalt cemented carbide. Metallogr. Microstruct. Anal. 7, 661–679 (2018)CrossRef Bagnall, C., Capo, J., Moorhead, W.J.: Oxidation behavior of tungsten carbide-6% cobalt cemented carbide. Metallogr. Microstruct. Anal. 7, 661–679 (2018)CrossRef
14.
go back to reference Jaworska, L., Szutkowska, M., Klimczyk, P., Sitarz, M., Bucko, M., Rutkowski, P., Figiel, P., Lojewska, J.: Oxidation, graphitization and thermal resistance of PCD materials with the various bonding phases up to 800 °C. Int. J. Refract. Met. Hard Mater. 45, 109–116 (2014) CrossRef Jaworska, L., Szutkowska, M., Klimczyk, P., Sitarz, M., Bucko, M., Rutkowski, P., Figiel, P., Lojewska, J.: Oxidation, graphitization and thermal resistance of PCD materials with the various bonding phases up to 800 °C. Int. J. Refract. Met. Hard Mater. 45, 109–116 (2014) CrossRef
15.
go back to reference Aizawa, T., Mitsuo, A., Yamamoto, S., Sumitomo, T., Muraishi, S.: Self-lubrication mechanism via the in situ formed lubricious oxide tribofilm. Wear 256, 708–718 (2005)CrossRef Aizawa, T., Mitsuo, A., Yamamoto, S., Sumitomo, T., Muraishi, S.: Self-lubrication mechanism via the in situ formed lubricious oxide tribofilm. Wear 256, 708–718 (2005)CrossRef
Metadata
Title
Wear Behaviour of PCBN, PCD, Binderless PCBN and Cemented Carbide Cutting Inserts When Machining Ti-6Al-4V in an Oxygen-Free Atmosphere
Authors
F. Schaper
B. Denkena
M.-A. Dittrich
A. Krödel
J. Matthies
S. Worpenberg
Copyright Year
2021
Publisher
Springer Berlin Heidelberg
DOI
https://doi.org/10.1007/978-3-662-62138-7_28

Premium Partners