Skip to main content
Top
Published in: Metallurgical and Materials Transactions B 1/2016

14-09-2015

A Novel Technology to Develop a Nickel-Enriched Layer on Slab Surface by Utilizing NiO-Containing Synthetic Powder

Authors: Tae-In Chung, Jung-Wook Cho, Youn-Bae Kang

Published in: Metallurgical and Materials Transactions B | Issue 1/2016

Log in

Activate our intelligent search to find suitable subject content or patents.

search-config
loading …

Abstract

Cu, as one of the typical tramp elements, is known to cause hot shortness during reheating of slabs followed by hot rolling of sheet products. In order to prevent such harmful aspects, a new idea is proposed by using synthetic powders containing NiO in the mold flux during continuous casting of the slab. During the casting, NiO is reduced and absorbed on initial solidified steel shell, and a Ni-rich layer is developed near the surface region of the slab. According to the proposed idea, it is expected that both the Cu solubility and the melting temperature of Cu-segregated region would increase considerably by virtue of Ni-rich layer, which is believed to play an important role to prevent the Cu hot shortness. A series of laboratory-scale experiments were carried out in order to confirm the reduction and the absorption of Ni into the steel matrix. It was observed by SEM–EDS and FE-EPMA that a Ni-enriched layer, as thick as a few hundred μm, formed near the surface of the slab. Also, a number of laboratory-scale heat treatment tests under oxidizing atmosphere showed that the samples with the Ni-enriched layer had a decreased Cu enrichment at the interface between scale and steel, compared to a case without Ni-rich layer. A pilot-plant-scale steel slab (medium carbon steel containing 0.3 wt pct Cu) was obtained in a continuous casting process with the NiO-containing mold flux, and a Ni-enriched layer was also observed. It was concluded that the use of NiO in the mold flux is a promising new approach for suppressing the hot shortness of Cu-containing steel, without an expensive addition of Ni to the whole steel matrix.

Dont have a licence yet? Then find out more about our products and how to get one now:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literature
1.
2.
go back to reference D. Young: High Temperature Oxidation and Corrosion of Metals, Elsevier, 2008, pp. 185–193. D. Young: High Temperature Oxidation and Corrosion of Metals, Elsevier, 2008, pp. 185–193.
3.
go back to reference 3. T. Kajitani, M. Wakoh, S. Ogibayashi and S. Mizoguchi: Tetsu-to-Hagané, 1995, vol. 81, pp. 185-190. 3. T. Kajitani, M. Wakoh, S. Ogibayashi and S. Mizoguchi: Tetsu-to-Hagané, 1995, vol. 81, pp. 185-190.
4.
go back to reference 4. H. G. Katayama, T. Momono, M. Doe and H. Saitoh: ISIJ Int., 1994, vol. 34, pp. 171-176.CrossRef 4. H. G. Katayama, T. Momono, M. Doe and H. Saitoh: ISIJ Int., 1994, vol. 34, pp. 171-176.CrossRef
5.
go back to reference 5. A. Hartman, C. Williamson and D. Davis: Iron Steelmaker, 1996, vol. 23, pp. 43-45. 5. A. Hartman, C. Williamson and D. Davis: Iron Steelmaker, 1996, vol. 23, pp. 43-45.
6.
go back to reference 6. K. Matsumaru, M. Susa and K. Nagata: Tetsu-to-Hagané, 1996, vol. 82, pp. 799-804. 6. K. Matsumaru, M. Susa and K. Nagata: Tetsu-to-Hagané, 1996, vol. 82, pp. 799-804.
7.
go back to reference 7. M. Sasabe, E. Harada and S Yamashita: Tetsu-to-Hagané, 1996, vol. 82, pp. 129-134. 7. M. Sasabe, E. Harada and S Yamashita: Tetsu-to-Hagané, 1996, vol. 82, pp. 129-134.
8.
go back to reference R.E. Brown, H.V. Divilio, R.J. Divilio (1975) Removal of Copper, Tin and other Impurities from Iron Scrap. BuMines, RI, pp. 1-31 R.E. Brown, H.V. Divilio, R.J. Divilio (1975) Removal of Copper, Tin and other Impurities from Iron Scrap. BuMines, RI, pp. 1-31
9.
go back to reference 9. C. Wang, T. Nagasaka and M. Hino: ISIJ Int.,1991, vol. 31, pp. 1300-1308.CrossRef 9. C. Wang, T. Nagasaka and M. Hino: ISIJ Int.,1991, vol. 31, pp. 1300-1308.CrossRef
10.
go back to reference 10. C. Wang, T. Nagasaka and M. Hino: ISIJ Int., 1991, vol. 31, pp. 1309-1315.CrossRef 10. C. Wang, T. Nagasaka and M. Hino: ISIJ Int., 1991, vol. 31, pp. 1309-1315.CrossRef
11.
go back to reference 11. X. Chen, N. Ito and K. Nakashima: Tetsu-to-Hagané, 1995, vol.81, pp. 959-964. 11. X. Chen, N. Ito and K. Nakashima: Tetsu-to-Hagané, 1995, vol.81, pp. 959-964.
12.
go back to reference 12. R. Morales D. and N. Sano: Ironmaking and Steelmaking, 1982, vol. 9, pp. 65-76. 12. R. Morales D. and N. Sano: Ironmaking and Steelmaking, 1982, vol. 9, pp. 65-76.
13.
go back to reference 13. T. Hidani, K. Takemura and R. O. Suzuki: Tetsu-to-Hagané, 1996, vol. 82, pp. 135-140. 13. T. Hidani, K. Takemura and R. O. Suzuki: Tetsu-to-Hagané, 1996, vol. 82, pp. 135-140.
14.
go back to reference 14. T. Maruyama, H. G. Katayama and T. Momono: Tetsu-to-Hagané, 1998, vol. 84 pp. 243-248. 14. T. Maruyama, H. G. Katayama and T. Momono: Tetsu-to-Hagané, 1998, vol. 84 pp. 243-248.
15.
go back to reference 15. H. Ono-Nakazato, K. Taguchi, Y. Seike and T. Usui: ISIJ Int., 2003, vol. 43, pp. 1691-1697.CrossRef 15. H. Ono-Nakazato, K. Taguchi, Y. Seike and T. Usui: ISIJ Int., 2003, vol. 43, pp. 1691-1697.CrossRef
16.
go back to reference 16. N. Imai, N. Komatsubara and K. Kunishige: ISIJ Int., 1997, vol. 37, pp. 224-231.CrossRef 16. N. Imai, N. Komatsubara and K. Kunishige: ISIJ Int., 1997, vol. 37, pp. 224-231.CrossRef
17.
go back to reference 17. M. Hatano and K. Kunishige: Tetsu-to-Hagané, 2003, vol. 89, pp. 42-49. 17. M. Hatano and K. Kunishige: Tetsu-to-Hagané, 2003, vol. 89, pp. 42-49.
18.
go back to reference 18. B. Webler, L. Yin, S. Sridhar: Metall. Mater. Trans. B, 2008, vol. 39B, pp. 725-737.CrossRef 18. B. Webler, L. Yin, S. Sridhar: Metall. Mater. Trans. B, 2008, vol. 39B, pp. 725-737.CrossRef
19.
go back to reference 19. L. Yin, S. Balaji and S. Sridhar: Metall. Mater. Trans. B, 2010 vol. 41, pp. 598-611.CrossRef 19. L. Yin, S. Balaji and S. Sridhar: Metall. Mater. Trans. B, 2010 vol. 41, pp. 598-611.CrossRef
20.
go back to reference 20. A. Takemura, K. Kunishige, S. Okaguchi and K. Fujiwara: Tetsu-to-Hagané, 2009, vol.95, pp. 369-377.CrossRef 20. A. Takemura, K. Kunishige, S. Okaguchi and K. Fujiwara: Tetsu-to-Hagané, 2009, vol.95, pp. 369-377.CrossRef
21.
go back to reference 21. S.-W Kim and H.-G. Lee: Steel Research Int., 2009, vol. 80, pp. 121-129. 21. S.-W Kim and H.-G. Lee: Steel Research Int., 2009, vol. 80, pp. 121-129.
22.
go back to reference 22. C.W. Bale, E. Belisle, P. Chartrand, S.A. Decterov, G. Eriksson, K. Hack, I.-H. Jung, Y.-B. Kang, J. Melancon, A.D. Pelton, C. Robelin, and S. Petersen: Calphad, 2009, vol. 33, pp. 295-311.CrossRef 22. C.W. Bale, E. Belisle, P. Chartrand, S.A. Decterov, G. Eriksson, K. Hack, I.-H. Jung, Y.-B. Kang, J. Melancon, A.D. Pelton, C. Robelin, and S. Petersen: Calphad, 2009, vol. 33, pp. 295-311.CrossRef
23.
go back to reference E. A. Brandes, G. B. Brook: Smithells Metals Reference Book. The Bath Press, London 1992, pp. 13. E. A. Brandes, G. B. Brook: Smithells Metals Reference Book. The Bath Press, London 1992, pp. 13.
24.
go back to reference 24. C. W. Tuck, M. Odgers, and K. Sachs: Corros. Sci., 1969, vol. 9, pp. 271-285.CrossRef 24. C. W. Tuck, M. Odgers, and K. Sachs: Corros. Sci., 1969, vol. 9, pp. 271-285.CrossRef
26.
go back to reference 26. N. Birks: Electrochemical Society, Proc. Symp., 1976, vol. 1, pp. 215-260. 26. N. Birks: Electrochemical Society, Proc. Symp., 1976, vol. 1, pp. 215-260.
27.
go back to reference P. Kofstad: High Temperature Corrosion, Elsevier, London, 1988, pp. 120-125. P. Kofstad: High Temperature Corrosion, Elsevier, London, 1988, pp. 120-125.
29.
go back to reference 29. R. Y. Chen and W. Y. D. Yuen: Oxidation of Metals, 2003, vol. 59, pp. 433-468.CrossRef 29. R. Y. Chen and W. Y. D. Yuen: Oxidation of Metals, 2003, vol. 59, pp. 433-468.CrossRef
30.
go back to reference 30. H. Ohtani, H. Suda and K. Ishida: ISIJ Int., 1997, vol. 37, pp. 207-216.CrossRef 30. H. Ohtani, H. Suda and K. Ishida: ISIJ Int., 1997, vol. 37, pp. 207-216.CrossRef
31.
go back to reference 31. H. T. Abuluwefa, and R. I. L Guthrie and F. Ajersch: Metall. Mater. Trans. A, 1997, vol. 28, pp. 1633-1642.CrossRef 31. H. T. Abuluwefa, and R. I. L Guthrie and F. Ajersch: Metall. Mater. Trans. A, 1997, vol. 28, pp. 1633-1642.CrossRef
32.
go back to reference H. T. Abuluwefa, and R. I. L Guthrie and F. Ajersch: Metall. Mater. Trans. A, 1997, vol. 28, pp. 1643-1651CrossRef H. T. Abuluwefa, and R. I. L Guthrie and F. Ajersch: Metall. Mater. Trans. A, 1997, vol. 28, pp. 1643-1651CrossRef
Metadata
Title
A Novel Technology to Develop a Nickel-Enriched Layer on Slab Surface by Utilizing NiO-Containing Synthetic Powder
Authors
Tae-In Chung
Jung-Wook Cho
Youn-Bae Kang
Publication date
14-09-2015
Publisher
Springer US
Published in
Metallurgical and Materials Transactions B / Issue 1/2016
Print ISSN: 1073-5615
Electronic ISSN: 1543-1916
DOI
https://doi.org/10.1007/s11663-015-0459-y

Other articles of this Issue 1/2016

Metallurgical and Materials Transactions B 1/2016 Go to the issue

Premium Partners