Abstract

The effects of polyvinyl alcohol (PVA) molecules on the porosity of disk-like hematite particles produced from the forced hydrolysis reaction using two kinds of PVA molecules with a well-defined molecular weight and a high degree of saponification (PVA-105 and PVA-124) were investigated. It is evident from TEM and field-emission scanning electron microscope (FE-SEM) measurements that a fraction of particles lost their spherical habit and acquired a disk-like shape by the addition of small amounts of both PVA molecules, though no difference in the particle size between the two PVA systems was observed. FE-SEM images of the particles revealed that the disk-like hematite particles are made up of small cluster particles with a diameter of approx. 5–10 nm. The disk-like particles produced a rather lower concentration for PVA-124 with a higher molecular weight than that for PVA-105 with a lower molecular weight. This fact was due to the large number of hydroxy groups in PVA-124 molecules than in PVA-105; hydroxy groups act as adsorption sites onto polynuclear (PN) primary particles and cause pronounced effects on the formation and structure of particles during the aggregation of PN particles. It was clarified from N2 adsorption measurements at 77 K that the porosity of the hematite particles can be controlled from microporous to mesoporous by changing the concentrations of PVA-105 and PVA-124, as was classified into three groups, i.e., groups 1, 2, and 3. The control particles produced without PVA molecules, classified into group 1, showed type IV adsorption isotherms, and only the voids produced between spherical particles were detected as mesopores. On the other hand, the particles produced with small amounts of PVA produced micropores as classified in group 2. In this group, the particles produced uniform micropores after being outgassed at 100–200 °C. The hematite particles produced with high concentrations of PVAs were classified into group 3. In this group, the particles after being outgassed at lower temperature produced micropores with diameters between 0.6 and 2.0 nm, though the micropores in the particles changed to mesopores after outgassing at 300 °C. This mesopore formation was attributed to the elimination of the PVA-adsorbed layer by evacuation at 300 °C, i.e., the large voids residing in the disk-like hematite particles make the particles mesoporous. This mesopore formation was further confirmed by adsorption experiments of C6H6(benzene) and CCl4 molecules at 298 K.

Dont have a licence yet? Then find out more about our products and how to get one now:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literature
1.
3.
5.
go back to reference Kandori K, Hayashi K, Matsumoto M, Fukusumi M, Moriosada Y (2010) Colloid Polym Sci 288:1071CrossRef Kandori K, Hayashi K, Matsumoto M, Fukusumi M, Moriosada Y (2010) Colloid Polym Sci 288:1071CrossRef
7.
8.
go back to reference Privman V, Goia DV, Park J, Matijević E (1999) J Colloid Interface Sci 213:36CrossRef Privman V, Goia DV, Park J, Matijević E (1999) J Colloid Interface Sci 213:36CrossRef
9.
go back to reference Schwertmann U, Cornell RM (1996) The iron oxide: structure, properties, reactions, occurrence and uses. Wiley-VCH, Weinheim Schwertmann U, Cornell RM (1996) The iron oxide: structure, properties, reactions, occurrence and uses. Wiley-VCH, Weinheim
10.
go back to reference Kandori K, Yamamoto N, Yasukawa A, Ishikawa T (2002) Phys Chem Chem Phys 4:6116CrossRef Kandori K, Yamamoto N, Yasukawa A, Ishikawa T (2002) Phys Chem Chem Phys 4:6116CrossRef
11.
12.
14.
go back to reference Gregg SJ, Sing KSW (1982) Adsorption, surface area and porosity, 2nd edn. Academic, London Gregg SJ, Sing KSW (1982) Adsorption, surface area and porosity, 2nd edn. Academic, London
Metadata
Title
Control on the porosity of disk-like hematite particles prepared from a forced hydrolysis reaction using polyvinyl alcohol
Authors
Kazuhiko Kandori
Gohki Yonekawa
Publication date
01-08-2013
Publisher
Springer Berlin Heidelberg
Published in
Colloid and Polymer Science / Issue 8/2013
Print ISSN: 0303-402X
Electronic ISSN: 1435-1536
DOI
https://doi.org/10.1007/s00396-013-2920-2

Other articles of this Issue 8/2013

Colloid and Polymer Science 8/2013 Go to the issue

Premium Partners