01-12-2012
Irradiation-Assisted Stress-Corrosion Cracking of Nitinol During eBeam Sterilization
Published in: Journal of Materials Engineering and Performance | Issue 12/2012
Log inActivate our intelligent search to find suitable subject content or patents.
Select sections of text to find matching patents with Artificial Intelligence. powered by
Select sections of text to find additional relevant content using AI-assisted search. powered by