Published in: Journal of Materials Science 21/2015

01-11-2015 | Original Paper

Stress corrosion and droplets formation in calcium phosphate and calcium alumino-phosphate glasses

Authors: Stephanie Etter, Annelise Faivre, Pierre Solignac, Sébastien Clément, Jean-Marc Fromental, Laurent Duffour, Florence Despetis

Published in: Journal of Materials Science | Issue 21/2015

Log in

Activate our intelligent search to find suitable subject content or patents.

search-config
loading …

Abstract

Subcritical crack growth and crack closure are analysed using the double cleavage drilled compression method, in two calcium phosphate-based glasses. The measurements of the crack velocity as a function of temperature, from ambient to 250 °C, are reported for two different relative humidity levels. Studied glasses present unusual trends characterized by a non-gradual shift of VK I curves versus temperature. Moreover, when the load is released and crack closes, expulsion of a “liquid-like” phase is observed forming droplets along the crack path. These droplets are only formed at certain temperatures, but both under high and low water humidity. They evolve towards residues when temperature is decreased.

Dont have a licence yet? Then find out more about our products and how to get one now:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literature
1.
go back to reference Wiederhorn M (1967) Influence of water vapour pressure on crack propagation in soda-lime glass. J Am Ceram Soc 50:407–414CrossRef Wiederhorn M (1967) Influence of water vapour pressure on crack propagation in soda-lime glass. J Am Ceram Soc 50:407–414CrossRef
2.
go back to reference Frieman SW (1980) Fracture mechanics of glass. In: Uhlmann DR, Kreidl NJ (eds) Glass science and technology, vol 5., Elasticity and strength in glasses. Academic Press, New York, pp 21–78 Frieman SW (1980) Fracture mechanics of glass. In: Uhlmann DR, Kreidl NJ (eds) Glass science and technology, vol 5., Elasticity and strength in glasses. Academic Press, New York, pp 21–78
3.
go back to reference Wiederhorn SM, Bolz LH (1970) Stress corrosion and static fatigue of glass. J Am Ceram Soc 53:543–548CrossRef Wiederhorn SM, Bolz LH (1970) Stress corrosion and static fatigue of glass. J Am Ceram Soc 53:543–548CrossRef
4.
go back to reference Freiman SW, Wiederhorn SM, Mecholsky JJ (2009) Environmentally enhanced fracture of glass: a historical perspective. J Am Ceram Soc 92:1371–1382CrossRef Freiman SW, Wiederhorn SM, Mecholsky JJ (2009) Environmentally enhanced fracture of glass: a historical perspective. J Am Ceram Soc 92:1371–1382CrossRef
5.
go back to reference Suratwala TI, Steele RA (2003) Anomalous temperature dependence of subcritical crack growth in silica glass. J Non-Cryst Solids 316:174–182CrossRef Suratwala TI, Steele RA (2003) Anomalous temperature dependence of subcritical crack growth in silica glass. J Non-Cryst Solids 316:174–182CrossRef
6.
go back to reference Hibino Y, Sakaguchi S, Tajima Y (1984) Crack growth in silica glass under dynamic loading. J Am Ceram Soc 67:64–68CrossRef Hibino Y, Sakaguchi S, Tajima Y (1984) Crack growth in silica glass under dynamic loading. J Am Ceram Soc 67:64–68CrossRef
7.
go back to reference Crichton SN, Tomozawa M, Hayden JS, Suratwala TI, Campbell JH (1999) Subcritical crack growth in a phosphate laser glass. J Am Ceram Soc 82:3097–3104CrossRef Crichton SN, Tomozawa M, Hayden JS, Suratwala TI, Campbell JH (1999) Subcritical crack growth in a phosphate laser glass. J Am Ceram Soc 82:3097–3104CrossRef
8.
go back to reference Suratwala TI, Steele RA, Wilke GD, Campbell JH, Takeuchi K (2000) Effects of OH content, water vapor pressure and temperature on sub-critical crack growth in phosphate glass. J Non-Cryst Solids 263&264:213–227CrossRef Suratwala TI, Steele RA, Wilke GD, Campbell JH, Takeuchi K (2000) Effects of OH content, water vapor pressure and temperature on sub-critical crack growth in phosphate glass. J Non-Cryst Solids 263&264:213–227CrossRef
9.
go back to reference Etter S, Despetis F, Etienne P (2008) Sub-critical crack growth in some phosphate glasses. J Non-Cryst Solids 354:580–586CrossRef Etter S, Despetis F, Etienne P (2008) Sub-critical crack growth in some phosphate glasses. J Non-Cryst Solids 354:580–586CrossRef
10.
go back to reference Brow RK (1993) Nature of alumina in phosphate glass: I, properties of sodium aluminophosphate glass. J Am Ceram Soc 76:913–918CrossRef Brow RK (1993) Nature of alumina in phosphate glass: I, properties of sodium aluminophosphate glass. J Am Ceram Soc 76:913–918CrossRef
11.
go back to reference He MY, Turner MR, Evans AG (1995) Analysis of the double cleavage drilled compression specimen for the interface fracture energy measurements over a range of mode mixities. Acta Metall Mater 43:3453–3458CrossRef He MY, Turner MR, Evans AG (1995) Analysis of the double cleavage drilled compression specimen for the interface fracture energy measurements over a range of mode mixities. Acta Metall Mater 43:3453–3458CrossRef
12.
go back to reference Lee YK, Tomozawa M (1999) Effect of water content in phosphate glasses on slow crack growth rate. J Non-Cryst Solids 248:203–210CrossRef Lee YK, Tomozawa M (1999) Effect of water content in phosphate glasses on slow crack growth rate. J Non-Cryst Solids 248:203–210CrossRef
13.
go back to reference Gehrke E, Ullner C, Hähnert M (1990) Effect of corrosive media on crack growth of model glasses and commercial silicate glasses. Glastech Ber 63:255–265 Gehrke E, Ullner C, Hähnert M (1990) Effect of corrosive media on crack growth of model glasses and commercial silicate glasses. Glastech Ber 63:255–265
15.
go back to reference Michalske TA, Bunker BC, Keefer KD (1990) Mechanical properties and adhesion of hydrated glass surface layers. J Am Ceram Soc 120:126–137 Michalske TA, Bunker BC, Keefer KD (1990) Mechanical properties and adhesion of hydrated glass surface layers. J Am Ceram Soc 120:126–137
16.
go back to reference Watanabe Y, Nakamura Y, Dickinson JT, Langford SC (1994) Changes in air exposed fracture surfaces of silicate glasses observed by atomic force microscopy. J Non-Cryst Solids 177:9–25CrossRef Watanabe Y, Nakamura Y, Dickinson JT, Langford SC (1994) Changes in air exposed fracture surfaces of silicate glasses observed by atomic force microscopy. J Non-Cryst Solids 177:9–25CrossRef
17.
go back to reference Celarie F, Ciccotti M, Marliere C (2007) Stress-enhanced ion diffusion at the vicinity of a crack tip as evidenced by atomic force microscopy in silicate glasses. J Non-Cryst Solids 353:51–68CrossRef Celarie F, Ciccotti M, Marliere C (2007) Stress-enhanced ion diffusion at the vicinity of a crack tip as evidenced by atomic force microscopy in silicate glasses. J Non-Cryst Solids 353:51–68CrossRef
18.
go back to reference Simmons CJ, Freiman SW (1981) Effect of corrosion processes on subcritical crack growth in glass. J Am Ceram Soc 64:683–686CrossRef Simmons CJ, Freiman SW (1981) Effect of corrosion processes on subcritical crack growth in glass. J Am Ceram Soc 64:683–686CrossRef
Metadata
Title
Stress corrosion and droplets formation in calcium phosphate and calcium alumino-phosphate glasses
Authors
Stephanie Etter
Annelise Faivre
Pierre Solignac
Sébastien Clément
Jean-Marc Fromental
Laurent Duffour
Florence Despetis
Publication date
01-11-2015
Publisher
Springer US
Published in
Journal of Materials Science / Issue 21/2015
Print ISSN: 0022-2461
Electronic ISSN: 1573-4803
DOI
https://doi.org/10.1007/s10853-015-9253-0

Other articles of this Issue 21/2015

Journal of Materials Science 21/2015 Go to the issue

Premium Partners