Abstract

Hot corrosion arises when metals are excited in the temperature range 700–900 °C in the existence of sulphate deposits, formed as a result of the reaction among sodium chloride and sulphur mixtures in the gas phase adjoining the metals. No alloy is resistant to hot corrosion occurrence indefinitely even though there are certain alloys that require a prolonged origination time at which the hot corrosion progression from the beginning stage to the circulation stage. Superalloys have been established for high-temperature applications. However, these alloys are not constantly able to meet both the high-temperature strength and high-temperature corrosion resistance simultaneously, so the need is to protect from hot corrosion. The high-temperature guarding system must meet numerous benchmarks, provide satisfactory environment resistance, be chemically and mechanically compatible with the substrate, be practically applicable, reliable and economically viable. This chapter briefly reviews the hot corrosion of some Ni- and Fe-base superalloys to recognise the occurrence. Extensive reviews on the hot corrosion of coatings have looked regularly since early 1970; the purpose of this chapter is not to repeat the published resources but relatively to emphasis on research developments and to point out some research forecasts.

Dont have a licence yet? Then find out more about our products and how to get one now:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literature
go back to reference Backman, R., Hupa, M., & Uppstu, E. (1987). Fouling and corrosion mechanisms in the recovery boiler superheater area. Tappi Journal, 70, 123–127. Backman, R., Hupa, M., & Uppstu, E. (1987). Fouling and corrosion mechanisms in the recovery boiler superheater area. Tappi Journal, 70, 123–127.
go back to reference Bansal, P., Padture, N. P., & Vasiliev, A. (2003). Improved interfacial properties of Al2O3–13 wt% TiO2 plasma sprayed coatings derived from nanocrytalline powders. Acta Materialia, 51, 2959–2970.CrossRef Bansal, P., Padture, N. P., & Vasiliev, A. (2003). Improved interfacial properties of Al2O3–13 wt% TiO2 plasma sprayed coatings derived from nanocrytalline powders. Acta Materialia, 51, 2959–2970.CrossRef
go back to reference Beltran, A. M., & Shores, D. A. (1972). Hot corrosion. In C. T. Sims & W. C. Hagel (Eds.), Shores. NY: Wiley Publ., John Wiley and Sons. (Chapter 11). Beltran, A. M., & Shores, D. A. (1972). Hot corrosion. In C. T. Sims & W. C. Hagel (Eds.), Shores. NY: Wiley Publ., John Wiley and Sons. (Chapter 11).
go back to reference Bhushan, B., & Gupta, B. K. (1991). Handbook of tribology: Materials, coatings and surface treatments. New York: McGraw-Hill. Bhushan, B., & Gupta, B. K. (1991). Handbook of tribology: Materials, coatings and surface treatments. New York: McGraw-Hill.
go back to reference Bornstein, N. S., & DeCrescente, M. A. (1969). Relationship between compounds of sodium and sulfur and sulfidation. Transactions of the Metallurgical Society of AIME, 245(9), 1947. Bornstein, N. S., & DeCrescente, M. A. (1969). Relationship between compounds of sodium and sulfur and sulfidation. Transactions of the Metallurgical Society of AIME, 245(9), 1947.
go back to reference Bornstein, N. S., DeCrescente, M. A., & Roth, H. A. (1973). The relationship between relative oxide ion content of Na2SO4, the presence of liquid metal oxides and sulfidation attack. Metallurgical Transactions, 4, 1799–1810.CrossRef Bornstein, N. S., DeCrescente, M. A., & Roth, H. A. (1973). The relationship between relative oxide ion content of Na2SO4, the presence of liquid metal oxides and sulfidation attack. Metallurgical Transactions, 4, 1799–1810.CrossRef
go back to reference Bornstein, N. S., Decrescente, M. A., & Roth, H. A. (1975). Effect of vanadium and sodium compounds on the accelerated oxidation of nickel base alloys. In: Proceedings of the Conference on Gas Turbine Materials in the Marine Environment, MMIC-75–27 (pp. 115–160). Columbus, Ohio, USA. Bornstein, N. S., Decrescente, M. A., & Roth, H. A. (1975). Effect of vanadium and sodium compounds on the accelerated oxidation of nickel base alloys. In: Proceedings of the Conference on Gas Turbine Materials in the Marine Environment, MMIC-75–27 (pp. 115–160). Columbus, Ohio, USA.
go back to reference Deb, D., Iyer, S. R., & Radhakrishnan, V. M. (1996). A comparative study of oxidation and hot corrosion of a cast nickel base superalloy in different corrosive environments. Materials Letters, 29, 19–23.CrossRef Deb, D., Iyer, S. R., & Radhakrishnan, V. M. (1996). A comparative study of oxidation and hot corrosion of a cast nickel base superalloy in different corrosive environments. Materials Letters, 29, 19–23.CrossRef
go back to reference Ding, C., Chen, H., Liu, X., & Zeng, Y. (2003). Plasma sprayed nanostructure zirconia coatings for wear resistance. In C. Moreau & B. Marple (Eds.), Thermal spray 2003: Advancing the science & applying the technology (pp. 455–458). Materials Park, Ohio, USA: ASM International. Ding, C., Chen, H., Liu, X., & Zeng, Y. (2003). Plasma sprayed nanostructure zirconia coatings for wear resistance. In C. Moreau & B. Marple (Eds.), Thermal spray 2003: Advancing the science & applying the technology (pp. 455–458). Materials Park, Ohio, USA: ASM International.
go back to reference Eliaz, N., Shemesh, G., & Latanision, R. M. (2002). Hot corrosion in gas turbine components. Engineering Failure Analysis, 9, 31–43.CrossRef Eliaz, N., Shemesh, G., & Latanision, R. M. (2002). Hot corrosion in gas turbine components. Engineering Failure Analysis, 9, 31–43.CrossRef
go back to reference Fairman, L. (1962). Technical note: Mechanism of accelerated oxidation by vanadium-containing fuel ash. Corrosion Science, 2, 293–296.CrossRef Fairman, L. (1962). Technical note: Mechanism of accelerated oxidation by vanadium-containing fuel ash. Corrosion Science, 2, 293–296.CrossRef
go back to reference Gitanjaly, Prakash, S., & Singh, S. (2002). Effects of MgO and CaO on hot corrosion of Fe base superalloy superfer 800H in Na2SO4–60 %V2O5 environment. British Corrosion Journal, 37(1), 56–62.CrossRef Gitanjaly, Prakash, S., & Singh, S. (2002). Effects of MgO and CaO on hot corrosion of Fe base superalloy superfer 800H in Na2SO4–60 %V2O5 environment. British Corrosion Journal, 37(1), 56–62.CrossRef
go back to reference Gledhill, H. C., Turner, I. G., & Doyle, C. (1999). Direct morphological comparison of vacuum plasma sprayed and detonation gun sprayed hydroxyapatite coatings for orthopedic applications. Biomaterials, 20, 315–322.CrossRef Gledhill, H. C., Turner, I. G., & Doyle, C. (1999). Direct morphological comparison of vacuum plasma sprayed and detonation gun sprayed hydroxyapatite coatings for orthopedic applications. Biomaterials, 20, 315–322.CrossRef
go back to reference Goebel, J. A., & Pettit, F. S. (1970a). Na2SO4-induced accelerated oxidation (hot corrosion) of nickel. Metallurgical Transactions, 1, 1943–1954.CrossRef Goebel, J. A., & Pettit, F. S. (1970a). Na2SO4-induced accelerated oxidation (hot corrosion) of nickel. Metallurgical Transactions, 1, 1943–1954.CrossRef
go back to reference Goebel, J. A., & Pettit, F. S. (1970b). The influence of sulphides on the oxidation behaviour of nickel-base alloys. Metallurgical Transactions, 1, 3421–3429.CrossRef Goebel, J. A., & Pettit, F. S. (1970b). The influence of sulphides on the oxidation behaviour of nickel-base alloys. Metallurgical Transactions, 1, 3421–3429.CrossRef
go back to reference Goebel, J. A., Pettit, F. S., & Goward, G. W. (1973). Mechanisms for the hot corrosion of nickel-base alloys. Metallurgical Transactions, 4, 261–275.CrossRef Goebel, J. A., Pettit, F. S., & Goward, G. W. (1973). Mechanisms for the hot corrosion of nickel-base alloys. Metallurgical Transactions, 4, 261–275.CrossRef
go back to reference Guo, M. H., Wang, Q. M., Gong, J., Sun, C., Huang, R. F., & Wen, L. S. (2006). Oxidation and hot corrosion behavior of gradient NiCoCrAlYSiB coatings deposited by a combination of arc ion plating and magnetron sputtering techniques. Corrosion Science, 48, 2750–2764.CrossRef Guo, M. H., Wang, Q. M., Gong, J., Sun, C., Huang, R. F., & Wen, L. S. (2006). Oxidation and hot corrosion behavior of gradient NiCoCrAlYSiB coatings deposited by a combination of arc ion plating and magnetron sputtering techniques. Corrosion Science, 48, 2750–2764.CrossRef
go back to reference Gurrappa, I. (1999). Hot corrosion behavior of CM 247 LC alloy in Na2SO4 and NaCl environments. Oxidation of Metals, 51(5), 353–382.CrossRef Gurrappa, I. (1999). Hot corrosion behavior of CM 247 LC alloy in Na2SO4 and NaCl environments. Oxidation of Metals, 51(5), 353–382.CrossRef
go back to reference Gurrappa, I. (2000). Hot corrosion of protective coatings. Materials and Manufacturing Processes, 15(5), 761–773.CrossRef Gurrappa, I. (2000). Hot corrosion of protective coatings. Materials and Manufacturing Processes, 15(5), 761–773.CrossRef
go back to reference Gurrappa, I. (2003). Influence of alloying elements on hot corrosion of superalloys and coatings: Necessity of smart coatings for gas turbine engines. Journal of Materials Science and Technology, 19(2), 178–183.CrossRef Gurrappa, I. (2003). Influence of alloying elements on hot corrosion of superalloys and coatings: Necessity of smart coatings for gas turbine engines. Journal of Materials Science and Technology, 19(2), 178–183.CrossRef
go back to reference Hancock, P. (1987). Vanadic and chloride attack of superalloys. Materials Science and Technology, 3, 536–544.CrossRef Hancock, P. (1987). Vanadic and chloride attack of superalloys. Materials Science and Technology, 3, 536–544.CrossRef
go back to reference Handbook, M. (1975). Failure analysis and prevention (Vol. 10). Metals Park OH, USA: ASM Publication. Handbook, M. (1975). Failure analysis and prevention (Vol. 10). Metals Park OH, USA: ASM Publication.
go back to reference Hao, D., Hua, W., Liu, J., Gong, J., Sun, C., & Wen, L. (2005). Influence of process variables on the qualities of detonation gun sprayed WC–Co coatings. Materials Science and Engineering: A, 408, 202–210.CrossRef Hao, D., Hua, W., Liu, J., Gong, J., Sun, C., & Wen, L. (2005). Influence of process variables on the qualities of detonation gun sprayed WC–Co coatings. Materials Science and Engineering: A, 408, 202–210.CrossRef
go back to reference Heath, G. R., Heimgartner, P., Irons, G., Miller, R., & Gustafsson, S. (1997). An assessment of thermal spray coating technologies for high temperature corrosion protection. Materials Science Forum, 251–54, 809–816.CrossRef Heath, G. R., Heimgartner, P., Irons, G., Miller, R., & Gustafsson, S. (1997). An assessment of thermal spray coating technologies for high temperature corrosion protection. Materials Science Forum, 251–54, 809–816.CrossRef
go back to reference Herman, H. (1988). Plasma sprayed coatings. Scientific American, 259(3), 78–83.CrossRef Herman, H. (1988). Plasma sprayed coatings. Scientific American, 259(3), 78–83.CrossRef
go back to reference Hocking, M. G. (1993). Coatings resistant to erosive/corrosive and severe environments. Surface and Coatings Technology, 62, 460–466.CrossRef Hocking, M. G. (1993). Coatings resistant to erosive/corrosive and severe environments. Surface and Coatings Technology, 62, 460–466.CrossRef
go back to reference Hwang, Y. S., & Rapp, R. A. (1989). Thermochemistry and solubilities of oxides in sodium sulfate-vanadate solutions. Corrosion, 45(11), 933–937.CrossRef Hwang, Y. S., & Rapp, R. A. (1989). Thermochemistry and solubilities of oxides in sodium sulfate-vanadate solutions. Corrosion, 45(11), 933–937.CrossRef
go back to reference Iyer, S. R., Iyer, K. J. L., & Radhakrishan, V. M. (1987). High temperature corrosion of a Ni-base superalloy by Vanadium. In Proceedings of the 10th ICMC (Vol. IV, pp. 3665–3670) Madras, India. Iyer, S. R., Iyer, K. J. L., & Radhakrishan, V. M. (1987). High temperature corrosion of a Ni-base superalloy by Vanadium. In Proceedings of the 10th ICMC (Vol. IV, pp. 3665–3670) Madras, India.
go back to reference Jordan, E. H., Gell, M., Sohn, Y. H., Goberman, D., Shaw, L., Jiang, S., et al. (2001). Fabrication and evaluation of plasma sprayed nanostructured alumina-titania coatings with superior properties. Materials Science and Engineering: A, 301, 80–89.CrossRef Jordan, E. H., Gell, M., Sohn, Y. H., Goberman, D., Shaw, L., Jiang, S., et al. (2001). Fabrication and evaluation of plasma sprayed nanostructured alumina-titania coatings with superior properties. Materials Science and Engineering: A, 301, 80–89.CrossRef
go back to reference Kamachi Mudali, U., Bhuvaneswaran, N., Shankar, P., & Raj, Baldev. (2004). Corrosion behaviour of intermetallic aluminide coatings on nitrogen-containing austenitic stainless steels. Corrosion Science, 46, 2867–2892.CrossRef Kamachi Mudali, U., Bhuvaneswaran, N., Shankar, P., & Raj, Baldev. (2004). Corrosion behaviour of intermetallic aluminide coatings on nitrogen-containing austenitic stainless steels. Corrosion Science, 46, 2867–2892.CrossRef
go back to reference Kamal, S., Jayaganthan, R., & Prakash, S. (2009). Evaluation of cyclic hot corrosion behaviour of detonation gun sprayed Cr3C2–NiCr coating on nickel and iron based superalloys. Surface and Coatings Technology, 203(8), 1004–1013.CrossRef Kamal, S., Jayaganthan, R., & Prakash, S. (2009). Evaluation of cyclic hot corrosion behaviour of detonation gun sprayed Cr3C2–NiCr coating on nickel and iron based superalloys. Surface and Coatings Technology, 203(8), 1004–1013.CrossRef
go back to reference Kamal, S., Jayaganthan, R., & Prakash, S. (2010). Hot corrosion studies of detonation-gun-sprayed NiCrAlY + 0.4 wt%CeO2 coatings on superalloys in molten salt environment. Journal of Materials Engineering and Performance, 20(6), 1068–1077.CrossRef Kamal, S., Jayaganthan, R., & Prakash, S. (2010). Hot corrosion studies of detonation-gun-sprayed NiCrAlY + 0.4 wt%CeO2 coatings on superalloys in molten salt environment. Journal of Materials Engineering and Performance, 20(6), 1068–1077.CrossRef
go back to reference Kamal, S., Jayaganthan, R., Prakash, S., & Kumar, Sanjay. (2008). Hot corrosion behavior of detonation gun sprayed Cr3C2–NiCr coatings on Ni and Fe-based superalloys in Na2SO4–60 % V2O5 environment at 900 °C. Journal of Alloys and Compounds, 463(1-2), 358–372.CrossRef Kamal, S., Jayaganthan, R., Prakash, S., & Kumar, Sanjay. (2008). Hot corrosion behavior of detonation gun sprayed Cr3C2–NiCr coatings on Ni and Fe-based superalloys in Na2SO4–60 % V2O5 environment at 900 °C. Journal of Alloys and Compounds, 463(1-2), 358–372.CrossRef
go back to reference Kawase, R., & Nakano, A. (1996). Production of heat and corrosion-resistant plastic coating. In Proceedings of the 9th National Thermal Spray Conference (pp. 257–262). Cincinnati, Ohio. Kawase, R., & Nakano, A. (1996). Production of heat and corrosion-resistant plastic coating. In Proceedings of the 9th National Thermal Spray Conference (pp. 257–262). Cincinnati, Ohio.
go back to reference Kerby, R. C., & Wilson, J. R. (1972). Electrical conduction properties of liquid vanadates. II. The sodium. Canadian Journal of Chemistry, 58, 2871–2876.CrossRef Kerby, R. C., & Wilson, J. R. (1972). Electrical conduction properties of liquid vanadates. II. The sodium. Canadian Journal of Chemistry, 58, 2871–2876.CrossRef
go back to reference Khajavi, M. R., & Shariat, M. H. (2004). Failure of first stage gas turbine blades. Engineering Failure Analysis, 11, 589–597.CrossRef Khajavi, M. R., & Shariat, M. H. (2004). Failure of first stage gas turbine blades. Engineering Failure Analysis, 11, 589–597.CrossRef
go back to reference Khana, A. S., & Jha, S. K. (1998). Degradation of materials under hot corrosion conditions. Transactions of the Indian Institute of Metals, 51(5), 279–290. Khana, A. S., & Jha, S. K. (1998). Degradation of materials under hot corrosion conditions. Transactions of the Indian Institute of Metals, 51(5), 279–290.
go back to reference Kim, J.-H., Yang, H.-S., Baik, K.-H., Seong, B. G., Lee, C.-H., & Hwang, S. Y. (2006). Development and properties of nanostructured thermal spray coatings. Current Applied Physics, 6(6), 1002–1006.CrossRef Kim, J.-H., Yang, H.-S., Baik, K.-H., Seong, B. G., Lee, C.-H., & Hwang, S. Y. (2006). Development and properties of nanostructured thermal spray coatings. Current Applied Physics, 6(6), 1002–1006.CrossRef
go back to reference Knotek, O. (2001). Thermal spraying and detonation spray gun processes. In R. F. Bunshah (Ed.) Handbook of hard coatings: Deposition technologies, properties and applications. Noyes Pub. Park Ridge, New Jersey, USA/William Andrew Publishing, LLC, Norwich, New York, USA (pp. 77–107) (Chapter 3). Knotek, O. (2001). Thermal spraying and detonation spray gun processes. In R. F. Bunshah (Ed.) Handbook of hard coatings: Deposition technologies, properties and applications. Noyes Pub. Park Ridge, New Jersey, USA/William Andrew Publishing, LLC, Norwich, New York, USA (pp. 77–107) (Chapter 3).
go back to reference Koch, G. H., Brongers, M. P. H., Thompson, N. G., Virmani, Y. P., & Payer, J. H. (2002). Historic congressional study: Corrosion costs and preventive strategies in the United States. Supplement to Materials Performance, 1–11. Koch, G. H., Brongers, M. P. H., Thompson, N. G., Virmani, Y. P., & Payer, J. H. (2002). Historic congressional study: Corrosion costs and preventive strategies in the United States. Supplement to Materials Performance, 1–11.
go back to reference Kofstad, P. (1988). High temperature corrosion (p. 465). London, New York: Elsevier Applied Science. (Chapter 14). Kofstad, P. (1988). High temperature corrosion (p. 465). London, New York: Elsevier Applied Science. (Chapter 14).
go back to reference Kolta, G. A., Hewaidy, L. F., & Felix, N. S. (1972). Reactions between sodium sulphate and vanadium pentoxide. Thermochimica Acta, 4, 151–164.CrossRef Kolta, G. A., Hewaidy, L. F., & Felix, N. S. (1972). Reactions between sodium sulphate and vanadium pentoxide. Thermochimica Acta, 4, 151–164.CrossRef
go back to reference Korpiola, K., & Vuoristo, P. (1996). Effect of HVOF gas velocity and fuel to oxygen ratio on the wear properties of tungsten carbide coating. In C. C. Bernt, (Ed.), Thermal spray: Practical solutions for engineering problems. Cincinnati, USA: ASM, October, 11–17. Korpiola, K., & Vuoristo, P. (1996). Effect of HVOF gas velocity and fuel to oxygen ratio on the wear properties of tungsten carbide coating. In C. C. Bernt, (Ed.), Thermal spray: Practical solutions for engineering problems. Cincinnati, USA: ASM, October, 11–17.
go back to reference Kuroda, S., Kawakita, J., Watanabe, Makoto., & Katanoda, Hiroshi. (2008). Topical review warm spraying—a novel coating process based on high-velocity impact of solid particles. Science and Technology of Advanced Materials, 9, 1–17. Kuroda, S., Kawakita, J., Watanabe, Makoto., & Katanoda, Hiroshi. (2008). Topical review warm spraying—a novel coating process based on high-velocity impact of solid particles. Science and Technology of Advanced Materials, 9, 1–17.
go back to reference Lambert, P., Champagne, B., & Arseneault, B. (1991). Oxidation and hot corrosion in Na2SO4—10 %V2O5 of Ni-17Cr-6Al-0.5Y and Ni-16Cr-5.7Al-0.47Y-5Si, MCrAlY Alloys at 7000 C. Canadian Metallurgical Quarterly, 30(2), 125–130. Lambert, P., Champagne, B., & Arseneault, B. (1991). Oxidation and hot corrosion in Na2SO4—10 %V2O5 of Ni-17Cr-6Al-0.5Y and Ni-16Cr-5.7Al-0.47Y-5Si, MCrAlY Alloys at 7000 C. Canadian Metallurgical Quarterly, 30(2), 125–130.
go back to reference Leblanc, L. (2003). Abrasion and sliding wear of nanostructured ceramic coatings. In C. Moreau & B. Marple (Eds.), Thermal spray 2003: Advancing the science & applying the technology (pp. 291–299). Materials Park, Ohio, USA: ASM International. Leblanc, L. (2003). Abrasion and sliding wear of nanostructured ceramic coatings. In C. Moreau & B. Marple (Eds.), Thermal spray 2003: Advancing the science & applying the technology (pp. 291–299). Materials Park, Ohio, USA: ASM International.
go back to reference Li, Y. S., Spiegel, M., & Shimada, S. (2005). Corrosion behaviour of various model alloys With NaCl–KCl coating. Materials Chemistry and Physics, 93, 217–223.CrossRef Li, Y. S., Spiegel, M., & Shimada, S. (2005). Corrosion behaviour of various model alloys With NaCl–KCl coating. Materials Chemistry and Physics, 93, 217–223.CrossRef
go back to reference Liang, Bo., & Ding, Chuanxian. (2005). Thermal shock resistances of nanostructured and conventional zirconia coatings deposited by atmospheric plasma spraying. Surface and Coatings Technology, 197, 185–192.CrossRef Liang, Bo., & Ding, Chuanxian. (2005). Thermal shock resistances of nanostructured and conventional zirconia coatings deposited by atmospheric plasma spraying. Surface and Coatings Technology, 197, 185–192.CrossRef
go back to reference Lin, Xinhua., Zeng, Yi., Ding, Chuanxian., & Zhang, Pingyu. (2004). Effects of temperature on tribological properties of nanostructured and conventional Al2O3–3 wt% TiO2 coatings. Wear, 256, 1018–1025.CrossRef Lin, Xinhua., Zeng, Yi., Ding, Chuanxian., & Zhang, Pingyu. (2004). Effects of temperature on tribological properties of nanostructured and conventional Al2O3–3 wt% TiO2 coatings. Wear, 256, 1018–1025.CrossRef
go back to reference Liu, P. S., Liang, K. M., Zhou, H. Y., Gu, S. R., Sun, X. F., Guan, H. R., et al. (2001). Cyclic oxidation behavior of aluminide coatings on the Co-base superalloy DZ40M. Surface and Coatings Technology, 145, 75–79.CrossRef Liu, P. S., Liang, K. M., Zhou, H. Y., Gu, S. R., Sun, X. F., Guan, H. R., et al. (2001). Cyclic oxidation behavior of aluminide coatings on the Co-base superalloy DZ40M. Surface and Coatings Technology, 145, 75–79.CrossRef
go back to reference Luthra, K. L., & Shores, D. A. (1980). Mechanism of Na2SO4 induced corrosion at 600–900 °C. Journal of the Electrochemical Society, 127(10), 2202–2210.CrossRef Luthra, K. L., & Shores, D. A. (1980). Mechanism of Na2SO4 induced corrosion at 600–900 °C. Journal of the Electrochemical Society, 127(10), 2202–2210.CrossRef
go back to reference Maledi, N. B., Potgieter, J. H., Sephton, M., Cornish, L. A., Chown, L., & Suss, R. (2006). Hot corrosion behaviour of Pt-alloys for application in the next generation of gas turbines. International Platinum Conference ‘Platinum Surges Ahead’, the Southern African Institute of Mining and Metallurgy (pp. 81–90). Maledi, N. B., Potgieter, J. H., Sephton, M., Cornish, L. A., Chown, L., & Suss, R. (2006). Hot corrosion behaviour of Pt-alloys for application in the next generation of gas turbines. International Platinum Conference ‘Platinum Surges Ahead’, the Southern African Institute of Mining and Metallurgy (pp. 81–90).
go back to reference Marceau, J. A., & Adjorlolo, A. A. (1995). Commercial aircraft. In ASM, Corrosion tests and standards; application and interpretation (pp. 574–578). American Society for Testing and Material Society. Marceau, J. A., & Adjorlolo, A. A. (1995). Commercial aircraft. In ASM, Corrosion tests and standards; application and interpretation (pp. 574–578). American Society for Testing and Material Society.
go back to reference Matthews S. J. (2004). Erosion-corrosion of Cr3C2–NiCr high velocity thermal spray coatings (Ph.D. thesis). The University of Auckland. Matthews S. J. (2004). Erosion-corrosion of Cr3C2–NiCr high velocity thermal spray coatings (Ph.D. thesis). The University of Auckland.
go back to reference Mevrel, R. (1989). State of the art on high-temperature corrosion-resistant coatings. Materials Science and Engineering: A, 120, 13–24.CrossRef Mevrel, R. (1989). State of the art on high-temperature corrosion-resistant coatings. Materials Science and Engineering: A, 120, 13–24.CrossRef
go back to reference Misra, A. K. (1986). Mechanism of Na2SO4-induced corrosion of molybdenum containing nickel-base superalloys at high temperatures. Journal of the Electrochemical Society, 133(5), 1029–1037.CrossRef Misra, A. K. (1986). Mechanism of Na2SO4-induced corrosion of molybdenum containing nickel-base superalloys at high temperatures. Journal of the Electrochemical Society, 133(5), 1029–1037.CrossRef
go back to reference Moujahid, S. E. (1987). High temperature corrosion of cast iron chains by Coal Ash. In Proceedings of the 10th ICMC (Vol. I, pp. 857–860). Madras, India. Moujahid, S. E. (1987). High temperature corrosion of cast iron chains by Coal Ash. In Proceedings of the 10th ICMC (Vol. I, pp. 857–860). Madras, India.
go back to reference Murthy, J. K. N., & Venkataraman, B. (2006). Abrasive wear behaviour of WC–CoCr and Cr3C2–20(NiCr) deposited by HVOF and detonation spray processes. Surface and Coatings Technology, 200, 2642–2652.CrossRef Murthy, J. K. N., & Venkataraman, B. (2006). Abrasive wear behaviour of WC–CoCr and Cr3C2–20(NiCr) deposited by HVOF and detonation spray processes. Surface and Coatings Technology, 200, 2642–2652.CrossRef
go back to reference Natesan, K. (1985). High-temperature corrosion in coal gasification systems. Corrosion, 41(11), 646–655.CrossRef Natesan, K. (1985). High-temperature corrosion in coal gasification systems. Corrosion, 41(11), 646–655.CrossRef
go back to reference Nelson, H. W., Krause, H. H., Ungar, E. W., Putnam, A. A., Slunder, C. J., Miller, P. D., et al. (1959). A review of available information on, corrosion and deposits in coal- and oil-fired boilers and gas turbines. Report of ASME research committee on corrosion and deposits from combustion gases. New York: Pergamon Press, ASME. Nelson, H. W., Krause, H. H., Ungar, E. W., Putnam, A. A., Slunder, C. J., Miller, P. D., et al. (1959). A review of available information on, corrosion and deposits in coal- and oil-fired boilers and gas turbines. Report of ASME research committee on corrosion and deposits from combustion gases. New York: Pergamon Press, ASME.
go back to reference Nerz, J. E., Kushner B. A., Jr., & Rotolico, A. J. (1992). Microstructural evaluation of tungsten carbide-cobalt coatings. ASM International (USA) (pp. 115–120). Nerz, J. E., Kushner B. A., Jr., & Rotolico, A. J. (1992). Microstructural evaluation of tungsten carbide-cobalt coatings. ASM International (USA) (pp. 115–120).
go back to reference Nicholls, J. R. (2000). Designing oxidation-resistant coatings. JOM, 52, 28–35. Nicholls, J. R. (2000). Designing oxidation-resistant coatings. JOM, 52, 28–35.
go back to reference Nicholls, J. R., Simms, N. J., Chan, W. Y., & Evans, H. E. (2002). Smart overlay coatings—concept and practice. Surface and Coatings Technology, 149, 236–244.CrossRef Nicholls, J. R., Simms, N. J., Chan, W. Y., & Evans, H. E. (2002). Smart overlay coatings—concept and practice. Surface and Coatings Technology, 149, 236–244.CrossRef
go back to reference Nickel, H., Quadakkers, W. J., & Singheiser, L. (2002). Analysis of corrosion layers on protective coatings and high temperature materials in simulated service environments of modern power plants using SNMS, SIMS, SEM, TEM, RBS and X-ray diffraction strudies. Analytical and Bioanalytical Chemistry, 374, 581–587.CrossRef Nickel, H., Quadakkers, W. J., & Singheiser, L. (2002). Analysis of corrosion layers on protective coatings and high temperature materials in simulated service environments of modern power plants using SNMS, SIMS, SEM, TEM, RBS and X-ray diffraction strudies. Analytical and Bioanalytical Chemistry, 374, 581–587.CrossRef
go back to reference Nicoll, A. R. (1984). The production and performance evaluation of high temperature coatings. In K. N. Strafford, P. K. Datta, & C. G. Googan (Eds.), Coatings and surface treatment for corrosion and wear resistance. Chichester: Institution of Corros. Sci. and Techol., Birmingham, Pub. Ellis Horwood Ltd. (Chapter 13). Nicoll, A. R. (1984). The production and performance evaluation of high temperature coatings. In K. N. Strafford, P. K. Datta, & C. G. Googan (Eds.), Coatings and surface treatment for corrosion and wear resistance. Chichester: Institution of Corros. Sci. and Techol., Birmingham, Pub. Ellis Horwood Ltd. (Chapter 13).
go back to reference Otero, E., Merino, M. C., Pardo, A., Biezma, M. V., & Buitrago, G. (1987). Study on corrosion products of IN657 alloy in molten salts. In Proceedings of 10th ICMC (Vol. IV, pp. 3583–3591). Madras, India. Otero, E., Merino, M. C., Pardo, A., Biezma, M. V., & Buitrago, G. (1987). Study on corrosion products of IN657 alloy in molten salts. In Proceedings of 10th ICMC (Vol. IV, pp. 3583–3591). Madras, India.
go back to reference Otero, E., Pardo, A., Hernaez, J., & Perez, F. J. (1990). The hot corrosion of IN-657 superalloy in Na2SO4–V2O5 melt eutectic. Corrosion Science, 30, 677–683. Otero, E., Pardo, A., Hernaez, J., & Perez, F. J. (1990). The hot corrosion of IN-657 superalloy in Na2SO4–V2O5 melt eutectic. Corrosion Science, 30, 677–683.
go back to reference Otsuka, N., & Rapp, R. A. (1990). Effects of chromate and vanadate anions on the hot corrosion of pre oxidized Ni by a thin fused Na2SO4 film at 900 °C. Journal of the Electrochemical Society, 137(1), 53–60.CrossRef Otsuka, N., & Rapp, R. A. (1990). Effects of chromate and vanadate anions on the hot corrosion of pre oxidized Ni by a thin fused Na2SO4 film at 900 °C. Journal of the Electrochemical Society, 137(1), 53–60.CrossRef
go back to reference Pettit, F. (2011). Hot corrosion of metals and alloys. Oxidation of Metals, 76, 1–21.CrossRef Pettit, F. (2011). Hot corrosion of metals and alloys. Oxidation of Metals, 76, 1–21.CrossRef
go back to reference Pettit, F. S., & Giggins, C. S. (1987). Hot corrosion. In C. T. Sims, N. S. Stollof, & W. C. Hagel (Eds.), Superalloys II. N Y: Pub. Wiley Pub. (Chapter 12). Pettit, F. S., & Giggins, C. S. (1987). Hot corrosion. In C. T. Sims, N. S. Stollof, & W. C. Hagel (Eds.), Superalloys II. N Y: Pub. Wiley Pub. (Chapter 12).
go back to reference Pettit, F. S., & Meier, G. H. (1985). Oxidation and hot corrosion of superalloys. In M. Gell, C. S. Kartovich, R. H. Bricknel, W. B. Kent & J. F. Radovich (Eds.), Superalloys 85 (pp. 651–687). Warrendale, Pennsylvania: Met. Soc. of AIME. Pettit, F. S., & Meier, G. H. (1985). Oxidation and hot corrosion of superalloys. In M. Gell, C. S. Kartovich, R. H. Bricknel, W. B. Kent & J. F. Radovich (Eds.), Superalloys 85 (pp. 651–687). Warrendale, Pennsylvania: Met. Soc. of AIME.
go back to reference Porcayo-Calderon, J., Gonzalez-Rodriguez, J. G., & Martinez, L. (1998). Protection of carbon steel against hot corrosion using thermal spray Si- and Cr-base coatings. Journal of Materials Engineering and Performance, 7, 79–87.CrossRef Porcayo-Calderon, J., Gonzalez-Rodriguez, J. G., & Martinez, L. (1998). Protection of carbon steel against hot corrosion using thermal spray Si- and Cr-base coatings. Journal of Materials Engineering and Performance, 7, 79–87.CrossRef
go back to reference Gitanjaly, & Prakash, S. (1999). Review on effect of additives on the hot corrosion. In 5th NACE Proceedings (pp. 174-182). New Delhi, India, November 22–24. Gitanjaly, & Prakash, S. (1999). Review on effect of additives on the hot corrosion. In 5th NACE Proceedings (pp. 174-182). New Delhi, India, November 22–24.
go back to reference Prakash, S., Puri, D., & Singh, H. (2005). Hot corrosion behaviour of plasma sprayed coating on Ni-based superalloys in Na2SO4–60 %V2O5 environment. ISIJ International, 45(6), 886–895.CrossRef Prakash, S., Puri, D., & Singh, H. (2005). Hot corrosion behaviour of plasma sprayed coating on Ni-based superalloys in Na2SO4–60 %V2O5 environment. ISIJ International, 45(6), 886–895.CrossRef
go back to reference Prakash, S., Singh, S., Sidhu, B. S., & Madeshia, A. (2001). Tube failures in coal fired boilers. In Proceedings of the National Seminar on Advances in Material and Processing (pp. 245–253) IITR, Roorkee, India, November 9–10. Prakash, S., Singh, S., Sidhu, B. S., & Madeshia, A. (2001). Tube failures in coal fired boilers. In Proceedings of the National Seminar on Advances in Material and Processing (pp. 245–253) IITR, Roorkee, India, November 9–10.
go back to reference Priyantha, N., Jayaweera, P., Sanjurjo, A., Lau, K., Lu, F., & Krist, K. (2003). Corrosion-resistant metallic coatings for applications in highly aggressive environments. Surface and Coatings Technology, 163–64, 31–36.CrossRef Priyantha, N., Jayaweera, P., Sanjurjo, A., Lau, K., Lu, F., & Krist, K. (2003). Corrosion-resistant metallic coatings for applications in highly aggressive environments. Surface and Coatings Technology, 163–64, 31–36.CrossRef
go back to reference Rapp, R. A. (2002). Hot corrosion of materials: A fluxing mechanism. Corrosion Science, 44(2), 209–221.CrossRef Rapp, R. A. (2002). Hot corrosion of materials: A fluxing mechanism. Corrosion Science, 44(2), 209–221.CrossRef
go back to reference Rapp, R. A., & Goto, K. S. (1981). The hot corrosion of metals by Molten Salts. In J. Braunstein & J. R. Selman (Eds.), Sympos. fused salts (pp. 159). Pennington, NJ: The Electrochemical Society. Rapp, R. A., & Goto, K. S. (1981). The hot corrosion of metals by Molten Salts. In J. Braunstein & J. R. Selman (Eds.), Sympos. fused salts (pp. 159). Pennington, NJ: The Electrochemical Society.
go back to reference Rapp, R. A., & Mehl, Robert. F. (2000). Some generalities in the analyses of equilibria in lonic solutions. Metallurgical and Materials Transactions A, 31(9), 2105–2118.CrossRef Rapp, R. A., & Mehl, Robert. F. (2000). Some generalities in the analyses of equilibria in lonic solutions. Metallurgical and Materials Transactions A, 31(9), 2105–2118.CrossRef
go back to reference Ravindra, T., Raghavan, S., & Kamaraj, M. (2007). Hot corrosion and oxidation behaviour of a directionally solidified nickel base superalloy. Transactions of the Indian Institute of Metals, 60, 385–392. Ravindra, T., Raghavan, S., & Kamaraj, M. (2007). Hot corrosion and oxidation behaviour of a directionally solidified nickel base superalloy. Transactions of the Indian Institute of Metals, 60, 385–392.
go back to reference Ren, X., & Wang, F. (2006). High-temperature oxidation and hot-corrosion behavior of a sputtered NiCrAlY coating with and without aluminizing. Surface and Coatings Technology, 201, 30–37.CrossRef Ren, X., & Wang, F. (2006). High-temperature oxidation and hot-corrosion behavior of a sputtered NiCrAlY coating with and without aluminizing. Surface and Coatings Technology, 201, 30–37.CrossRef
go back to reference Salmenoja, K., Makela, K., Hupa, M., & Backman, R. (1996). Superheater corrosion in environments containing potassium and chlorine. Journal of the Institute of Energy, 69, 155–162. Salmenoja, K., Makela, K., Hupa, M., & Backman, R. (1996). Superheater corrosion in environments containing potassium and chlorine. Journal of the Institute of Energy, 69, 155–162.
go back to reference Saravanan, P., Selvarajan, V., Rao, D. S., Joshi, S. V., & Sundararajan, G. (2000). Influence of process variables on the quality of detonation gun sprayed alumina coatings. Surface and Coatings Technology, 123, 44–54.CrossRef Saravanan, P., Selvarajan, V., Rao, D. S., Joshi, S. V., & Sundararajan, G. (2000). Influence of process variables on the quality of detonation gun sprayed alumina coatings. Surface and Coatings Technology, 123, 44–54.CrossRef
go back to reference Seiersten, M., & Kofstad, P. (1987). The effect of SO3 on vanadate-induced hot corrosion. High Temperature Technology, 5(3), 115–122.CrossRef Seiersten, M., & Kofstad, P. (1987). The effect of SO3 on vanadate-induced hot corrosion. High Temperature Technology, 5(3), 115–122.CrossRef
go back to reference Seybolt, A. U. (1968). Hot corrosion mechanism. Transactions of the Metallurgical Society of AIME, 242, 1955–1961. Seybolt, A. U. (1968). Hot corrosion mechanism. Transactions of the Metallurgical Society of AIME, 242, 1955–1961.
go back to reference Sharma, R. N. (1996). Hot corrosion behaviour of iron- and nickel-base superalloys in salt environments at elevated temperatures (Ph.D. thesis). Met. Mat. Engg. Deptt., University of Roorkee, Roorkee, India. Sharma, R. N. (1996). Hot corrosion behaviour of iron- and nickel-base superalloys in salt environments at elevated temperatures (Ph.D. thesis). Met. Mat. Engg. Deptt., University of Roorkee, Roorkee, India.
go back to reference Shaw, L. L., Goberman, D., Ren, R., Gell, M., Jiang, S., Wang, Y., et al. (2000). The dependency of microstructure and properties of nanostructured coatings on plasma spray conditions. Surface and Coatings Technology, 130, 1–8.CrossRef Shaw, L. L., Goberman, D., Ren, R., Gell, M., Jiang, S., Wang, Y., et al. (2000). The dependency of microstructure and properties of nanostructured coatings on plasma spray conditions. Surface and Coatings Technology, 130, 1–8.CrossRef
go back to reference Shi, L., Zhang, Y., & Shih, S. (1992). The effect of K2SO4 additive in Na2SO4 deposits on low temperature hot corrosion of iron-aluminum alloys. Oxidation of Metals, 38, 385–405.CrossRef Shi, L., Zhang, Y., & Shih, S. (1992). The effect of K2SO4 additive in Na2SO4 deposits on low temperature hot corrosion of iron-aluminum alloys. Oxidation of Metals, 38, 385–405.CrossRef
go back to reference Shih, S., Zhang, Y., & Li, X. (1989). Sub-melting point hot corrosion of alloys and coatings. Materials Science and Engineering A, 120, 277–282.CrossRef Shih, S., Zhang, Y., & Li, X. (1989). Sub-melting point hot corrosion of alloys and coatings. Materials Science and Engineering A, 120, 277–282.CrossRef
go back to reference Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006a). Performance of high velocity oxy fuel—sprayed coating on an Fe-based superalloy in Na2SO4–60 % V2O5 environment at 900 °C part II: Hot corrosion behaviour of coating. Journal of Materials Engineering and Performance, 15, 130–138.CrossRef Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006a). Performance of high velocity oxy fuel—sprayed coating on an Fe-based superalloy in Na2SO4–60 % V2O5 environment at 900 °C part II: Hot corrosion behaviour of coating. Journal of Materials Engineering and Performance, 15, 130–138.CrossRef
go back to reference Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006b). Hot corrosion studies of HVOF sprayed Cr3C2–NiCr and Ni–20Cr coatings on nickel-based superalloy at 900 °C. Surface and Coatings Technology, 201(3-4), 792–800.CrossRef Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006b). Hot corrosion studies of HVOF sprayed Cr3C2–NiCr and Ni–20Cr coatings on nickel-based superalloy at 900 °C. Surface and Coatings Technology, 201(3-4), 792–800.CrossRef
go back to reference Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006c). Hot corrosion studies of HVOF NiCrBSi and stellite-6 coatings on a Ni-based superalloy in an actual industrial environment of a coal fired boiler. Surface and Coatings Technology, 201(3/4), 1602–1612.CrossRef Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006c). Hot corrosion studies of HVOF NiCrBSi and stellite-6 coatings on a Ni-based superalloy in an actual industrial environment of a coal fired boiler. Surface and Coatings Technology, 201(3/4), 1602–1612.CrossRef
go back to reference Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006d). Characterisation of NiCr wire coatings on Ni- and Fe-based superalloys by the HVOF process. Surface and Coatings Technology, 200, 5542–5549.CrossRef Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006d). Characterisation of NiCr wire coatings on Ni- and Fe-based superalloys by the HVOF process. Surface and Coatings Technology, 200, 5542–5549.CrossRef
go back to reference Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006e). Studies of the metallurgical and mechanical properties of high velocity oxy-fuel sprayed stellite-6 coatings on Ni- and Fe-based superalloys. Surface and Coatings Technology, 201(1/2), 273–281.CrossRef Sidhu, T. S., Prakash, S., & Agrawal, R. D. (2006e). Studies of the metallurgical and mechanical properties of high velocity oxy-fuel sprayed stellite-6 coatings on Ni- and Fe-based superalloys. Surface and Coatings Technology, 201(1/2), 273–281.CrossRef
go back to reference Sidhu, H. S., Sidhu, B. S., & Prakash, S. (2006f). The role of HVOF coatings in improving hot corrosion resistance of ASTM-SA210 GrA1 steel in the presence of Na2SO4–V2O5 salt deposits. Surface and Coatings Technology, 200, 5386–5394.CrossRef Sidhu, H. S., Sidhu, B. S., & Prakash, S. (2006f). The role of HVOF coatings in improving hot corrosion resistance of ASTM-SA210 GrA1 steel in the presence of Na2SO4–V2O5 salt deposits. Surface and Coatings Technology, 200, 5386–5394.CrossRef
go back to reference Sidky, P. S., & Hocking, M. G. (1999). Review of inorganic coatings and coating processes for reducing wear and corrosion. British Corrosion Journal, 34(3), 171–183.CrossRef Sidky, P. S., & Hocking, M. G. (1999). Review of inorganic coatings and coating processes for reducing wear and corrosion. British Corrosion Journal, 34(3), 171–183.CrossRef
go back to reference Simons, E. L., Browning, G. V., & Liebhatsky, H. A. (1955). Corrosion, 11, 505.CrossRef Simons, E. L., Browning, G. V., & Liebhatsky, H. A. (1955). Corrosion, 11, 505.CrossRef
go back to reference Singh, H., Puri, D., & Prakash, S. (2005a). Some studies on hot corrosion performance of plasma sprayed coatings on a Fe-based superalloy. Surface and Coatings Technology, 192(1), 27–38.CrossRef Singh, H., Puri, D., & Prakash, S. (2005a). Some studies on hot corrosion performance of plasma sprayed coatings on a Fe-based superalloy. Surface and Coatings Technology, 192(1), 27–38.CrossRef
go back to reference Singh, H., Puri, D., & Prakash, S. (2005b). Corrosion behaviour of plasma sprayed coating on Ni-based superalloys in Na2SO4–60%V2O5 environment at 900 °C. ISIJ International, 45(6), 886–895.CrossRef Singh, H., Puri, D., & Prakash, S. (2005b). Corrosion behaviour of plasma sprayed coating on Ni-based superalloys in Na2SO4–60%V2O5 environment at 900 °C. ISIJ International, 45(6), 886–895.CrossRef
go back to reference Sobolev, V.V., Guilemany, J.M., & Nutting, J. (2004). HVOF spraying. B0655, Maney, IOM3 (pp. 5). Sobolev, V.V., Guilemany, J.M., & Nutting, J. (2004). HVOF spraying. B0655, Maney, IOM3 (pp. 5).
go back to reference Soltani, R., Coyle, T. W., & Mostaghimi, J. (2003). Wear resistance of nanostructured thermal barrier coatings. In C. Moreau & B. Marple (Eds.), Thermal spray 2003: Advancing the science & applying the technology (pp. 1535–1540). Materials Park, Ohio, USA: ASM International. Soltani, R., Coyle, T. W., & Mostaghimi, J. (2003). Wear resistance of nanostructured thermal barrier coatings. In C. Moreau & B. Marple (Eds.), Thermal spray 2003: Advancing the science & applying the technology (pp. 1535–1540). Materials Park, Ohio, USA: ASM International.
go back to reference Stokes, J., & Looney, L. (2001). HVOF system definition to maximise the thickness of formed components. Surface and Coatings Technology, 148, 18–24.CrossRef Stokes, J., & Looney, L. (2001). HVOF system definition to maximise the thickness of formed components. Surface and Coatings Technology, 148, 18–24.CrossRef
go back to reference Stott, F. H., De Wet, D. J., & Taylor, R. (1994). The degradation resistance of thermal barrier coatings to molten deposits at very high temperatures. Transactions of the Materials Research Society of Japan, 14A, 135–140. Stott, F. H., De Wet, D. J., & Taylor, R. (1994). The degradation resistance of thermal barrier coatings to molten deposits at very high temperatures. Transactions of the Materials Research Society of Japan, 14A, 135–140.
go back to reference Stringer, J. (1977). Hot corrosion of high temperature alloys. Annual Review of Materials Research, 7, 477–509. Stringer, J. (1977). Hot corrosion of high temperature alloys. Annual Review of Materials Research, 7, 477–509.
go back to reference Stringer, J. (1987). High temperature corrosion of superalloys. Materials Science and Technology, 3(7), 482–493.CrossRef Stringer, J. (1987). High temperature corrosion of superalloys. Materials Science and Technology, 3(7), 482–493.CrossRef
go back to reference Stringer, J. (1998). Coatings in the electricity supply industry: past, present, and opportunities for the future. Surface and Coatings Technology, 108–109, 1–9.CrossRef Stringer, J. (1998). Coatings in the electricity supply industry: past, present, and opportunities for the future. Surface and Coatings Technology, 108–109, 1–9.CrossRef
go back to reference Stroosnijder, M. F., Mevrel, R., & Bennet, M. J. (1994). The interaction of surface engineering and high temperature corrosion protection. Materials at High Temperatures, 12(1), 53–66.CrossRef Stroosnijder, M. F., Mevrel, R., & Bennet, M. J. (1994). The interaction of surface engineering and high temperature corrosion protection. Materials at High Temperatures, 12(1), 53–66.CrossRef
go back to reference Suito, H., & Gaskell, D. R. (1971). The thermodynamics of melts in the system VO2–V2O5. Metallurgical and Materials Transactions B, 2, 3299–3303.CrossRef Suito, H., & Gaskell, D. R. (1971). The thermodynamics of melts in the system VO2–V2O5. Metallurgical and Materials Transactions B, 2, 3299–3303.CrossRef
go back to reference Taylor, M. P., & Evans, H. E. (2001). The influence of bond coat surface roughness and structure on the oxidation of a thermal barrier coating system. Materials Science Forum, 369–372, 711–717.CrossRef Taylor, M. P., & Evans, H. E. (2001). The influence of bond coat surface roughness and structure on the oxidation of a thermal barrier coating system. Materials Science Forum, 369–372, 711–717.CrossRef
go back to reference Tiwari, S. N. (1997). Investigations on hot corrosion of some Fe-, Ni- and Co-base superalloy in Na2SO4–V2O5 environment under cyclic conditions (Ph.D. thesis). Met. Mat. Engg. Deptt., University of Roorkee, Roorkee, India. Tiwari, S. N. (1997). Investigations on hot corrosion of some Fe-, Ni- and Co-base superalloy in Na2SO4–V2O5 environment under cyclic conditions (Ph.D. thesis). Met. Mat. Engg. Deptt., University of Roorkee, Roorkee, India.
go back to reference Tiwari, S. N., & Prakash, S. (1996). Hot corrosion behaviour of an iron-base superalloy in salt environment at elevated temperatures. In Proceedings of the Symposium Metals and Materials Research, Indian Institute of Technology Madras (pp. 107–117) Madras, July 4–5. Tiwari, S. N., & Prakash, S. (1996). Hot corrosion behaviour of an iron-base superalloy in salt environment at elevated temperatures. In Proceedings of the Symposium Metals and Materials Research, Indian Institute of Technology Madras (pp. 107–117) Madras, July 4–5.
go back to reference Tiwari, S. N., & Prakash, S. (1997). Studies on the hot corrosion behaviour of some superalloys in Na2SO4–V2O5. In Proceedings of the SOLCEC, Kalpakkam, India, January 22–24, Paper C33. Tiwari, S. N., & Prakash, S. (1997). Studies on the hot corrosion behaviour of some superalloys in Na2SO4–V2O5. In Proceedings of the SOLCEC, Kalpakkam, India, January 22–24, Paper C33.
go back to reference Tiwari, S. N., & Prakash, S. (1998). Literature review-magnesium oxide as inhibitor of hot oil ash corrosion. Materials Science and Technology, 14, 467–472.CrossRef Tiwari, S. N., & Prakash, S. (1998). Literature review-magnesium oxide as inhibitor of hot oil ash corrosion. Materials Science and Technology, 14, 467–472.CrossRef
go back to reference Tzvetkoff, T., & Gencheva, P. (2003). Mechanism of formation of corrosion layers on nickel and nickel-based alloys in melts containing Ox anions—A review. Materials Chemistry and Physics, 82(3), 897–904.CrossRef Tzvetkoff, T., & Gencheva, P. (2003). Mechanism of formation of corrosion layers on nickel and nickel-based alloys in melts containing Ox anions—A review. Materials Chemistry and Physics, 82(3), 897–904.CrossRef
go back to reference Uusitalo, M. A., Vuoristo, P. M. J., & Mantyla, T. A. (2004). High temperature corrosion of coatings and boiler steels below chlorine-containing salt deposits. Corrosion Science, 46(6), 1311–1331.CrossRef Uusitalo, M. A., Vuoristo, P. M. J., & Mantyla, T. A. (2004). High temperature corrosion of coatings and boiler steels below chlorine-containing salt deposits. Corrosion Science, 46(6), 1311–1331.CrossRef
go back to reference Valdes, C. J., Dooley, R. B., & Wilson, J. R. (1973). The corrosion of A.I.S.I 446 stainless steel in Molten Vanadates in the temperature range 700–900 °C (Grant No. 7535-14). Report Defense Research Board Canada. Valdes, C. J., Dooley, R. B., & Wilson, J. R. (1973). The corrosion of A.I.S.I 446 stainless steel in Molten Vanadates in the temperature range 700–900 °C (Grant No. 7535-14). Report Defense Research Board Canada.
go back to reference Wagner, N., Gnadic, K., Kreye, H., & Kronewetter, H. (1984). Particle velocity in hypersonic flame spraying of WC-Co. Surface and Coatings Technology, 22, 61–71.CrossRef Wagner, N., Gnadic, K., Kreye, H., & Kronewetter, H. (1984). Particle velocity in hypersonic flame spraying of WC-Co. Surface and Coatings Technology, 22, 61–71.CrossRef
go back to reference Wang, Q. M., Wu, Y. N., Ke, P. L., Cao, H. T., Gong, J., Sun, C., et al. (2004). Hot corrosion behavior of AIP NiCoCrAlY(SiB) coatings on nickel base superalloys. Surface and Coatings Technology, 86, 389–397.CrossRef Wang, Q. M., Wu, Y. N., Ke, P. L., Cao, H. T., Gong, J., Sun, C., et al. (2004). Hot corrosion behavior of AIP NiCoCrAlY(SiB) coatings on nickel base superalloys. Surface and Coatings Technology, 86, 389–397.CrossRef
go back to reference Yoshiba, M. (1993). Effect of hot corrosion on the mechanical performances of superalloys and coating systems. Corrosion Science, 35(5–8), 1115–1124.CrossRef Yoshiba, M. (1993). Effect of hot corrosion on the mechanical performances of superalloys and coating systems. Corrosion Science, 35(5–8), 1115–1124.CrossRef
go back to reference Zhang, Y. S., & Rapp, R. A. (1987). Solubilities of CeO2, HfO2 and Y2O3 in fused Na2SO4–30 mol% NaVO3 and CeO2 in pure Na2SO4 at 900 °C. Corrosion, 43(6), 348–352.CrossRef Zhang, Y. S., & Rapp, R. A. (1987). Solubilities of CeO2, HfO2 and Y2O3 in fused Na2SO4–30 mol% NaVO3 and CeO2 in pure Na2SO4 at 900 °C. Corrosion, 43(6), 348–352.CrossRef
go back to reference Zheng, D., Zhu, S., & Wang, F. (2006). Oxidation and hot corrosion behavior of a novel enamel-Al2O3 composite coating on K38G superalloy. Surface and Coatings Technology, 200, 5931–5936.CrossRef Zheng, D., Zhu, S., & Wang, F. (2006). Oxidation and hot corrosion behavior of a novel enamel-Al2O3 composite coating on K38G superalloy. Surface and Coatings Technology, 200, 5931–5936.CrossRef
Metadata
Title
Thermal Spray Coatings for Hot Corrosion Resistance
Authors
Subhash Kamal
K. V. Sharma
P. Srinivasa Rao
Othman Mamat
Copyright Year
2017
DOI
https://doi.org/10.1007/978-3-319-29761-3_10