Abstract

Second-phase Al3Sc particles play an important role in several aspects of material performance. These include increasing strength, stabilizing microstructure and increasing recrystallization temperature and thermal stability. The present work was conducted to investigate the stability of Al3Sc particles in a severely deformed Al-0.25 wt% Sc alloy at room temperature in comparison to that of Al2Cu precipitates in an Al-Cu alloy. Microstructural examination and hardness tests showed that the Al3Sc particles were coarsening resistant with substantially higher stability than Al2Cu and the hardness of the Al-0.25Sc alloy remained almost constant while an apparent hardness drop was observed for the Al-Cu alloy.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
1.
Zurück zum Zitat Rokhlin LL, Dobatkina T, Kharakterova ML (1997) Structure of the phase equilibrium diagrams of aluminum alloys with scandium. Powder Metal Met Ceram. 36: 128–132. Rokhlin LL, Dobatkina T, Kharakterova ML (1997) Structure of the phase equilibrium diagrams of aluminum alloys with scandium. Powder Metal Met Ceram. 36: 128–132.
2.
Zurück zum Zitat Davydov VG, Rostova TD, Zakharov VV, FilatovYA, Yelagin VI (2000) Scientific principles of making an alloying addition of scandium to aluminium alloys. Mater Sci Eng. A280:30–36. Davydov VG, Rostova TD, Zakharov VV, FilatovYA, Yelagin VI (2000) Scientific principles of making an alloying addition of scandium to aluminium alloys. Mater Sci Eng. A280:30–36.
3.
Zurück zum Zitat Yelagin VI, Zakharov VV, Rostova DT (1991) Features of Sc-bearing aluminium alloy recrystallization. In: Problems of Light Alloy Metallurgy. VILS, Moscow, p 114–129. Yelagin VI, Zakharov VV, Rostova DT (1991) Features of Sc-bearing aluminium alloy recrystallization. In: Problems of Light Alloy Metallurgy. VILS, Moscow, p 114–129.
4.
Zurück zum Zitat Huang Y, Robson JD, Prangnell PB (2010) The formation of nano grain structures and accelerated room temperature theta precipitation in a severely deformed Al-4 wt%Cu alloy. Acta Mater. 58:1643–1657. Huang Y, Robson JD, Prangnell PB (2010) The formation of nano grain structures and accelerated room temperature theta precipitation in a severely deformed Al-4 wt%Cu alloy. Acta Mater. 58:1643–1657.
5.
Zurück zum Zitat Zuo J, Hou L, Shi J, et al. (2017) Effect of deformation induced precipitation on dynamic aging process and improvement of mechanical/corrosion properties AA7055 aluminum alloy. J All Comp.708:1131–1140. Zuo J, Hou L, Shi J, et al. (2017) Effect of deformation induced precipitation on dynamic aging process and improvement of mechanical/corrosion properties AA7055 aluminum alloy. J All Comp.708:1131–1140.
6.
Zurück zum Zitat Huang Y, Prangnell PB (2008) Effect of cryogenic temperatures and change in deformation mode on the limiting grain size in a severely deformed dilute Al alloy. Acta Mater. 56:1619–1631. Huang Y, Prangnell PB (2008) Effect of cryogenic temperatures and change in deformation mode on the limiting grain size in a severely deformed dilute Al alloy. Acta Mater. 56:1619–1631.
7.
Zurück zum Zitat Apps PJ, Berta M, Prangnell PB (2005) The Effect of Dispersoids on the Grain Refinement Mechanisms During Deformation of Aluminium Alloys to Ultra-High Strains. Acta Mater. 53:499–511. Apps PJ, Berta M, Prangnell PB (2005) The Effect of Dispersoids on the Grain Refinement Mechanisms During Deformation of Aluminium Alloys to Ultra-High Strains. Acta Mater. 53:499–511.
Metadaten
Titel
Coarsening-Resistance of a Severely Deformed Al-0.2 wt% Sc Alloy
verfasst von
Yan Huang
Copyright-Jahr
2020
DOI
https://doi.org/10.1007/978-3-030-36408-3_39

    Marktübersichten

    Die im Laufe eines Jahres in der „adhäsion“ veröffentlichten Marktübersichten helfen Anwendern verschiedenster Branchen, sich einen gezielten Überblick über Lieferantenangebote zu verschaffen.