27. Orientation Imaging Microscopy in Research on High Temperature Oxidation

verfasst von : Bae-Kyun Kim, Jerzy A. Szpunar

Erschienen in: Electron Backscatter Diffraction in Materials Science

Verlag: Springer US

Aktivieren Sie unsere intelligente Suche, um passende Fachinhalte oder Patente zu finden.

search-config
loading …

High temperature oxidation of steel has been studied for reducing steel losses and for understanding descaling of oxides (Kuiry et al. 1994; Tomellini and Mazzarano 1988; Sachs and Tuck 1968). Surface defects, such as scale pits and residues, are frequently observed on steel surfaces after hot rolling. The occurrence of surface defects is related to the formation of oxide scale. These defects are undesirable for the surface quality control of slab in the hot rolling process. The quality control of steel products is highly dependent on the removal of scale on slab during the hot rolling process. This is directly related to the scale structure formed in high temperature oxidation.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
Zurück zum Zitat Abuluwefa H, Root JH, Guthrie RIL, Ajersch F (1996) Real-time observations of the oxidation of mild steel at high temperature by neutron diffraction. Metall Mater Trans B 27: 993–997CrossRef Abuluwefa H, Root JH, Guthrie RIL, Ajersch F (1996) Real-time observations of the oxidation of mild steel at high temperature by neutron diffraction. Metall Mater Trans B 27: 993–997CrossRef
Zurück zum Zitat Baba-Kishi KZ, Dingley DJ (1989) Backscatter Kikuchi diffraction in the SEM for identification of crystallographic point groups. Scanning 11:305–312 Baba-Kishi KZ, Dingley DJ (1989) Backscatter Kikuchi diffraction in the SEM for identification of crystallographic point groups. Scanning 11:305–312
Zurück zum Zitat Béranger G (1996) Oxidation. In: Béranger G, Henry G, Sanz G (eds) The book of steel (trans Davidson J.H). Intercept LTD, Andover, U.K. Béranger G (1996) Oxidation. In: Béranger G, Henry G, Sanz G (eds) The book of steel (trans Davidson J.H). Intercept LTD, Andover, U.K.
Zurück zum Zitat Birks N, Meier GH (1983) Introduction to high temperature oxidation of metals. Edward Arnold, London Birks N, Meier GH (1983) Introduction to high temperature oxidation of metals. Edward Arnold, London
Zurück zum Zitat Birosca S, Dingley D, Higginson RL (2004) Microstructural and microtextural characterization of oxide scale on steel using electron backscatter diffraction. J Microsc 213:235–240CrossRefPubMedMathSciNet Birosca S, Dingley D, Higginson RL (2004) Microstructural and microtextural characterization of oxide scale on steel using electron backscatter diffraction. J Microsc 213:235–240CrossRefPubMedMathSciNet
Zurück zum Zitat Bredesen R, Kofstad P (1990) On the oxidation of iron in CO2 + CO gas mixtures: I. Scale morphology and reaction kinetics. Oxid Met 34:361–379CrossRef Bredesen R, Kofstad P (1990) On the oxidation of iron in CO2 + CO gas mixtures: I. Scale morphology and reaction kinetics. Oxid Met 34:361–379CrossRef
Zurück zum Zitat Bruckman K, Simkovich G (1972) Concerning the mechanism of scale growth due to cation diffusion in Fe2O3 and CuS. Corros Sci 12:595–601CrossRef Bruckman K, Simkovich G (1972) Concerning the mechanism of scale growth due to cation diffusion in Fe2O3 and CuS. Corros Sci 12:595–601CrossRef
Zurück zum Zitat Buscail H, Larpin JP (1996) The influence of cerium surface addition on low-pressure oxidation of pure iron at high temperatures. Solid State Ionics 92:243–251CrossRef Buscail H, Larpin JP (1996) The influence of cerium surface addition on low-pressure oxidation of pure iron at high temperatures. Solid State Ionics 92:243–251CrossRef
Zurück zum Zitat Caplan D, Cohen M (1966) Effect of cold work on the oxidation of iron from 400 to 650°C. Corros Sci 6:321–335CrossRef Caplan D, Cohen M (1966) Effect of cold work on the oxidation of iron from 400 to 650°C. Corros Sci 6:321–335CrossRef
Zurück zum Zitat Caplan D, Graham MJ, Cohen M (1970a) Effect of oxygen pressure and experimental method on the high temperature oxidation of pure Fe. Corros Sci 10:1–8CrossRef Caplan D, Graham MJ, Cohen M (1970a) Effect of oxygen pressure and experimental method on the high temperature oxidation of pure Fe. Corros Sci 10:1–8CrossRef
Zurück zum Zitat Caplan D, Sproule GI, Hussey RJ (1970b) Comparison of the kinetics of high-temperature oxidation of Fe as influenced by metal purity and cold work. Corros Sci 10:9–17CrossRef Caplan D, Sproule GI, Hussey RJ (1970b) Comparison of the kinetics of high-temperature oxidation of Fe as influenced by metal purity and cold work. Corros Sci 10:9–17CrossRef
Zurück zum Zitat Carpenter DL, Ray AC (1973) The effect of metallurgical pretreatment on the kinetics of oxidation of iron at 700°C in pure gaseous oxygen. Corros Sci 13:493–502CrossRef Carpenter DL, Ray AC (1973) The effect of metallurgical pretreatment on the kinetics of oxidation of iron at 700°C in pure gaseous oxygen. Corros Sci 13:493–502CrossRef
Zurück zum Zitat Caudron E, Buscail H, Riffard F (1999) Initial oxidation stage of yttrium implanted pure iron at 700°C by in situ high temperature X-ray diffraction. Eur Phys J-Appl Phys 8:233–240CrossRefADS Caudron E, Buscail H, Riffard F (1999) Initial oxidation stage of yttrium implanted pure iron at 700°C by in situ high temperature X-ray diffraction. Eur Phys J-Appl Phys 8:233–240CrossRefADS
Zurück zum Zitat Chen RY, Yuen WYD (2000) A study of the scale structure of hot rolled steel strip by simulated coiling and cooling. Oxid Met 53(5/6):539–560CrossRef Chen RY, Yuen WYD (2000) A study of the scale structure of hot rolled steel strip by simulated coiling and cooling. Oxid Met 53(5/6):539–560CrossRef
Zurück zum Zitat Condon NG, Murray PW, Leibsle FM, Thornton G, Lennie AR, Vaughan DJ (1994) Fe3O4 (111) termination of α- Fe2O3 (0001). Surf Sci 310:L609–L613CrossRef Condon NG, Murray PW, Leibsle FM, Thornton G, Lennie AR, Vaughan DJ (1994) Fe3O4 (111) termination of α- Fe2O3 (0001). Surf Sci 310:L609–L613CrossRef
Zurück zum Zitat Cornell RM, Schwertmann U (1996) The iron oxides. VCH, Weinheim, Germany, 458 Cornell RM, Schwertmann U (1996) The iron oxides. VCH, Weinheim, Germany, 458
Zurück zum Zitat Davies MH, Simnad MT, Birchenall CE (1951) Mechanism and kinetics of the scaling of iron. J Met-T AIME 3:889–896 Davies MH, Simnad MT, Birchenall CE (1951) Mechanism and kinetics of the scaling of iron. J Met-T AIME 3:889–896
Zurück zum Zitat Davies MJ, Parker SC (1989) Unpublished works (Bath University) cited in: Robertson J, Manning, MI (1990) Mater Sci Techn 6:81–91 Davies MJ, Parker SC (1989) Unpublished works (Bath University) cited in: Robertson J, Manning, MI (1990) Mater Sci Techn 6:81–91
Zurück zum Zitat Dingley DJ, Randle V (1992) Microtexture determination by electron back-scatter diffraction. J Mater Sci 27:4545–4566CrossRefADS Dingley DJ, Randle V (1992) Microtexture determination by electron back-scatter diffraction. J Mater Sci 27:4545–4566CrossRefADS
Zurück zum Zitat Dubinin GN (2000) On the columnar structure of a diffusion layer. Met Sci Heat Treat 42:89–93CrossRef Dubinin GN (2000) On the columnar structure of a diffusion layer. Met Sci Heat Treat 42:89–93CrossRef
Zurück zum Zitat Eades A (2000) EBSD: Buying a system. In: Schwartz AJ, Kumar M, Adams BL (eds) Electron backscatter diffraction in materials science. Kluwer Academic/Plenum, New York Eades A (2000) EBSD: Buying a system. In: Schwartz AJ, Kumar M, Adams BL (eds) Electron backscatter diffraction in materials science. Kluwer Academic/Plenum, New York
Zurück zum Zitat Goehner RP, Michael JR (1996) Phase identification in a scanning electron microscope using backscattered electron Kikuchi patterns. J Res Natl Inst Stand Tech 101: 301–308 Goehner RP, Michael JR (1996) Phase identification in a scanning electron microscope using backscattered electron Kikuchi patterns. J Res Natl Inst Stand Tech 101: 301–308
Zurück zum Zitat Graat PCJ, Brongers MPH, Zandbergen HW, Somers MAJ, Mittemeijer EJ (1997) HREM investigation of the constitution and the crystallography of thin thermal oxide layers on iron. In: Newcomb SB, Little JA (eds) Microscopy of oxidation, vol. 3. Institute of Materials, London, pp 503–514 Graat PCJ, Brongers MPH, Zandbergen HW, Somers MAJ, Mittemeijer EJ (1997) HREM investigation of the constitution and the crystallography of thin thermal oxide layers on iron. In: Newcomb SB, Little JA (eds) Microscopy of oxidation, vol. 3. Institute of Materials, London, pp 503–514
Zurück zum Zitat Gulbransen EA, Ruka R (1952) Role of crystal orientation in the oxidation of iron. J Electrochem Soc 99:360–368CrossRef Gulbransen EA, Ruka R (1952) Role of crystal orientation in the oxidation of iron. J Electrochem Soc 99:360–368CrossRef
Zurück zum Zitat Hauffe (1965) Oxidation of metals. Plenum, New York Hauffe (1965) Oxidation of metals. Plenum, New York
Zurück zum Zitat Higginson RL, Roebuckb B, Palmiere EJ (2002) Texture development in oxide scales on steel substrates. Scripta Mater 47:337–342CrossRef Higginson RL, Roebuckb B, Palmiere EJ (2002) Texture development in oxide scales on steel substrates. Scripta Mater 47:337–342CrossRef
Zurück zum Zitat Iordanova I, Surtchev M, Forcey KS, Krastev V (2000) High-temperature surface oxidation of low-carbon rimming steel. Surf Interface Anal 30:158–160CrossRef Iordanova I, Surtchev M, Forcey KS, Krastev V (2000) High-temperature surface oxidation of low-carbon rimming steel. Surf Interface Anal 30:158–160CrossRef
Zurück zum Zitat Katrakova D, Maas C, Hohnerlein D, Mucklich F (1998) Experiences on contrasting microstructure using orientation imaging microscopy. Prakt Metall 35:4–20 Katrakova D, Maas C, Hohnerlein D, Mucklich F (1998) Experiences on contrasting microstructure using orientation imaging microscopy. Prakt Metall 35:4–20
Zurück zum Zitat Kim BK, Szpunar JA (2001a) Orientation imaging microscopy for the study of high temperature oxidation. Scripta Mater 44:2605–2610CrossRef Kim BK, Szpunar JA (2001a) Orientation imaging microscopy for the study of high temperature oxidation. Scripta Mater 44:2605–2610CrossRef
Zurück zum Zitat Kim BK, Szpunar JA (2001b) Grain growth of iron oxides during high temperature oxidation. In: Gottstein G, Molodov DA (eds) Proceedings of the first joint international conference on recrystallization and grain growth, Aug. 27–31. Aachen, Germany Kim BK, Szpunar JA (2001b) Grain growth of iron oxides during high temperature oxidation. In: Gottstein G, Molodov DA (eds) Proceedings of the first joint international conference on recrystallization and grain growth, Aug. 27–31. Aachen, Germany
Zurück zum Zitat Kofstad P (1988) High temperature oxidation. Elsevier Applied Science, London Kofstad P (1988) High temperature oxidation. Elsevier Applied Science, London
Zurück zum Zitat Kuiry SC, Roy SK, Bose SK (1994) A superficial coating to improve high-temperature-oxidation resistance of a plain-carbon steel under nonisothermal conditions. Oxid Met 41:65–79CrossRef Kuiry SC, Roy SK, Bose SK (1994) A superficial coating to improve high-temperature-oxidation resistance of a plain-carbon steel under nonisothermal conditions. Oxid Met 41:65–79CrossRef
Zurück zum Zitat Lagoeiro LE (1998) Transformation of magnetite to hematite and its influence on the dissolution of iron oxide minerals. J Metamorph Geol 16:415–423CrossRef Lagoeiro LE (1998) Transformation of magnetite to hematite and its influence on the dissolution of iron oxide minerals. J Metamorph Geol 16:415–423CrossRef
Zurück zum Zitat Matthies S, Vinel GW (1993) On some methodical developments concerning calculations performed directly in the orientation space. Mater Sci Forum 157–162:1641–1646 Matthies S, Vinel GW (1993) On some methodical developments concerning calculations performed directly in the orientation space. Mater Sci Forum 157–162:1641–1646
Zurück zum Zitat Mehl RF, Candless EL, Rhines FN (1934) Orientation of oxide films on metals. Nature 134:1009CrossRefADS Mehl RF, Candless EL, Rhines FN (1934) Orientation of oxide films on metals. Nature 134:1009CrossRefADS
Zurück zum Zitat Michael JR, Eades JA (2000) Use of reciprocal lattice layer spacing in electron backscatter diffraction pattern analysis. Ultramicroscopy 81:67–81CrossRefPubMed Michael JR, Eades JA (2000) Use of reciprocal lattice layer spacing in electron backscatter diffraction pattern analysis. Ultramicroscopy 81:67–81CrossRefPubMed
Zurück zum Zitat Michael JR, Goehner RP (1993) Crystallographic phase identification in the scanning electron microscope: Backscattered electron Kikuchi patterns imaged with a CCD-based detector. MSA Bulletin 23:168–175 Michael JR, Goehner RP (1993) Crystallographic phase identification in the scanning electron microscope: Backscattered electron Kikuchi patterns imaged with a CCD-based detector. MSA Bulletin 23:168–175
Zurück zum Zitat Newcomb SB, Stobbs WM (1985) Proceedings of Electron Microscopy and Analysis Group (EMAG) Conference. The Institute of Physics, Newcastle upon Tyne, 2–5 Sept., UK., 451 Newcomb SB, Stobbs WM (1985) Proceedings of Electron Microscopy and Analysis Group (EMAG) Conference. The Institute of Physics, Newcastle upon Tyne, 2–5 Sept., UK., 451
Zurück zum Zitat Pawlik K, Pospiech J, Lücke K (1991) The ODF approximation from pole figures with the aid of the ADC method. Texture Microstructure 14–18, 25–30CrossRef Pawlik K, Pospiech J, Lücke K (1991) The ODF approximation from pole figures with the aid of the ADC method. Texture Microstructure 14–18, 25–30CrossRef
Zurück zum Zitat Pinder LW (1995) The oxidation resistance of low-alloy steels. In: Shreir LL, Jarman RA, Burstein GT (eds) Corrosion, vol. 1. Butterworth Heinemann, London Pinder LW (1995) The oxidation resistance of low-alloy steels. In: Shreir LL, Jarman RA, Burstein GT (eds) Corrosion, vol. 1. Butterworth Heinemann, London
Zurück zum Zitat Randle V, Engler O (2000) Introduction to texture analysis: macrotexture, microtexture and orientation mapping. Gordon & Breach Science, Amsterdam, The Netherlands Randle V, Engler O (2000) Introduction to texture analysis: macrotexture, microtexture and orientation mapping. Gordon & Breach Science, Amsterdam, The Netherlands
Zurück zum Zitat Sachs K, Tuck CW (1968) Surface oxidation of steel in industrial furnaces. Proceedings of the conference reheating for hot working. Iron and Steel Institute, Publication No. 111, London, pp 1–17 Sachs K, Tuck CW (1968) Surface oxidation of steel in industrial furnaces. Proceedings of the conference reheating for hot working. Iron and Steel Institute, Publication No. 111, London, pp 1–17
Zurück zum Zitat Scully JC (1990) The Fundamentals of corrosion. Pergamon Press, Oxford Scully JC (1990) The Fundamentals of corrosion. Pergamon Press, Oxford
Zurück zum Zitat Swell PB, Cohen M (1964) The oxidation of iron single crystals around 200°C. J Electrochem Soc 111(5):501–508CrossRef Swell PB, Cohen M (1964) The oxidation of iron single crystals around 200°C. J Electrochem Soc 111(5):501–508CrossRef
Zurück zum Zitat Tomellini M, Mazzarano A (1988) High-temperature oxidation under time-dependent gas pressure: An application to steel oxidation. Oxid Met 29(3/4):179–191CrossRef Tomellini M, Mazzarano A (1988) High-temperature oxidation under time-dependent gas pressure: An application to steel oxidation. Oxid Met 29(3/4):179–191CrossRef
Zurück zum Zitat Tominaga J, Wakimoto K, Mori T, Murakami M, Yoshimura T (1982) Manufacture of wire rods with good descaling property. Trans ISIJ 22:646–656 Tominaga J, Wakimoto K, Mori T, Murakami M, Yoshimura T (1982) Manufacture of wire rods with good descaling property. Trans ISIJ 22:646–656
Zurück zum Zitat TSL (2000) OIM analysis user manual (ver. 3.07) TSL (2000) OIM analysis user manual (ver. 3.07)
Zurück zum Zitat Wagner JB, Lawless KR Jr, Gwathmey AT (1961) T Metall Soc AIME 221:257–261 Wagner JB, Lawless KR Jr, Gwathmey AT (1961) T Metall Soc AIME 221:257–261
Zurück zum Zitat Watanabe Y, Ishii K (1995) Geometrical consideration of the crystallography of the transformation from α-Fe2O3 to Fe3O4. Phys Status Solidi A 150:673–686CrossRefADS Watanabe Y, Ishii K (1995) Geometrical consideration of the crystallography of the transformation from α-Fe2O3 to Fe3O4. Phys Status Solidi A 150:673–686CrossRefADS
Zurück zum Zitat Wright SI, Nowell MM (2002) Chemistry assisted phase differentiation in automated electron backscatter diffraction. Microsc Microanal 8(Suppl 2):682–683 Wright SI, Nowell MM (2002) Chemistry assisted phase differentiation in automated electron backscatter diffraction. Microsc Microanal 8(Suppl 2):682–683
Metadaten
Titel
Orientation Imaging Microscopy in Research on High Temperature Oxidation
verfasst von
Bae-Kyun Kim
Jerzy A. Szpunar
Copyright-Jahr
2009
Verlag
Springer US
DOI
https://doi.org/10.1007/978-0-387-88136-2_27

    Marktübersichten

    Die im Laufe eines Jahres in der „adhäsion“ veröffentlichten Marktübersichten helfen Anwendern verschiedenster Branchen, sich einen gezielten Überblick über Lieferantenangebote zu verschaffen.