Comparative High-Temperature Corrosion Behavior of Ni-20Cr Coatings on T22 Boiler Steel Produced by HVOF, D-Gun, and Cold Spraying

verfasst von: Gagandeep Kaushal, Niraj Bala, Narinder Kaur, Harpreet Singh, Satya Prakash

Erschienen in: Metallurgical and Materials Transactions A | Ausgabe 1/2014

Einloggen

Aktivieren Sie unsere intelligente Suche, um passende Fachinhalte oder Patente zu finden.

search-config
loading …

Abstract

To protect materials from surface degradations such as wear, corrosion, and thermal flux, a wide variety of materials can be deposited on the materials by several spraying processes. This paper examines and compares the microstructure and high-temperature corrosion of Ni-20Cr coatings deposited on T22 boiler steel by high velocity oxy-fuel (HVOF), detonation gun spray, and cold spraying techniques. The coatings’ microstructural features were characterized by means of XRD and FE-SEM/EDS analyses. Based upon the results of mass gain, XRD, and FE-SEM/EDS analyses it may be concluded that the Ni-20Cr coating sprayed by all the three techniques was effective in reducing the corrosion rate of the steel. Among the three coatings, D-gun spray coating proved to be better than HVOF-spray and cold-spray coatings.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
1.
Zurück zum Zitat A.M. Beltran and D.A. Shores: in The Superalloys, C.T. Sims and W.C. Hagel, vol. 44 (24), Wiley, New York, 1972, pp. 4289–96. A.M. Beltran and D.A. Shores: in The Superalloys, C.T. Sims and W.C. Hagel, vol. 44 (24), Wiley, New York, 1972, pp. 4289–96.
2.
Zurück zum Zitat Eliaz, N., Shemesh, G. and Latanision, R.M. (2002), Eng. Fail. Anal., Vol. 9, pp. 31-43.CrossRef Eliaz, N., Shemesh, G. and Latanision, R.M. (2002), Eng. Fail. Anal., Vol. 9, pp. 31-43.CrossRef
3.
Zurück zum Zitat Gil, L. and Staia, M.H., (1999), Surf. Coat. Technol., Vol. 120-121, pp. 423-29.CrossRef Gil, L. and Staia, M.H., (1999), Surf. Coat. Technol., Vol. 120-121, pp. 423-29.CrossRef
4.
Zurück zum Zitat Gil, L. and Staia, M.H., (2002), Thin Solid Films, Vol. 420-421, pp. 446-54.CrossRef Gil, L. and Staia, M.H., (2002), Thin Solid Films, Vol. 420-421, pp. 446-54.CrossRef
5.
Zurück zum Zitat Lugscheider, E., Herbst, C. and Zhao, L., (1998), Surf. Coat. Technol., Vol. 108-109, pp. 16-23.CrossRef Lugscheider, E., Herbst, C. and Zhao, L., (1998), Surf. Coat. Technol., Vol. 108-109, pp. 16-23.CrossRef
6.
Zurück zum Zitat M.R. Ramesh, S. Prakash, S.K. Nath, P.K. Sapra, and B. Venkatraman: Wear, 2010, 269, 197–205.CrossRef M.R. Ramesh, S. Prakash, S.K. Nath, P.K. Sapra, and B. Venkatraman: Wear, 2010, 269, 197–205.CrossRef
7.
Zurück zum Zitat R.A. Mahesh, R. Jayaganthan, S. Prakash, Mater. Chem. Phys., 2010, 119, 3, 449-57.CrossRef R.A. Mahesh, R. Jayaganthan, S. Prakash, Mater. Chem. Phys., 2010, 119, 3, 449-57.CrossRef
8.
Zurück zum Zitat D. Ozimina, M. Madej, T. Kałdoński., Tribol Lett., 2011, 41, 103–111.CrossRef D. Ozimina, M. Madej, T. Kałdoński., Tribol Lett., 2011, 41, 103–111.CrossRef
9.
Zurück zum Zitat M. Benegra, M. Magnani, H. Goldenstein, O. Maranho, and G. Pintaude: Surf. Eng., 2010, vol. 26 (6), 463–68. M. Benegra, M. Magnani, H. Goldenstein, O. Maranho, and G. Pintaude: Surf. Eng., 2010, vol. 26 (6), 463–68.
10.
Zurück zum Zitat A.P. Alkimov, A.N. Papyrin, V.P. Dosarev, N.I. Nesterovich, and M.M. Shushpanov: US Patent 5,302,414, 12 April 1994. A.P. Alkimov, A.N. Papyrin, V.P. Dosarev, N.I. Nesterovich, and M.M. Shushpanov: US Patent 5,302,414, 12 April 1994.
12.
Zurück zum Zitat Kosarev, V.F., Klinkov, S.V., Alkhimov, A.P. and Papyrin, A.N., (2003), J. Therm. Spray Technol., Vol. 12, No. 2, pp. 265-81.CrossRef Kosarev, V.F., Klinkov, S.V., Alkhimov, A.P. and Papyrin, A.N., (2003), J. Therm. Spray Technol., Vol. 12, No. 2, pp. 265-81.CrossRef
14.
Zurück zum Zitat G. Kaushal, H. Singh, and S. Prakash: International Thermal Spray Conference and Exposition (ITSC 08), Maastricht, The Netherlands, 02–04 June 2008, pp. 1351–56. G. Kaushal, H. Singh, and S. Prakash: International Thermal Spray Conference and Exposition (ITSC 08), Maastricht, The Netherlands, 02–04 June 2008, pp. 1351–56.
15.
Zurück zum Zitat Kaushal, G., Singh, H. and Prakash, S. (2011) Oxid. Met., 76 (3-4), 169–91.CrossRef Kaushal, G., Singh, H. and Prakash, S. (2011) Oxid. Met., 76 (3-4), 169–91.CrossRef
16.
Zurück zum Zitat Singh, H., Puri, D., and Prakash, S. (2005) Surf. Coat. Technol. 192, 27–38.CrossRef Singh, H., Puri, D., and Prakash, S. (2005) Surf. Coat. Technol. 192, 27–38.CrossRef
17.
Zurück zum Zitat Metals Handbook: ASM Publication, vol. 10, Metals Park OH, 1975. Metals Handbook: ASM Publication, vol. 10, Metals Park OH, 1975.
18.
Zurück zum Zitat National Materials Advisory Board Report: Coatings for High-Temperature Structural Materials: Trends and Opportunities, National Academy Press, Washington, DC, 1996. National Materials Advisory Board Report: Coatings for High-Temperature Structural Materials: Trends and Opportunities, National Academy Press, Washington, DC, 1996.
19.
Zurück zum Zitat Bala, N., Singh, H. and Prakash, S., (2009) Appl. Surf. Sci., Vol. 255, No. 15, pp. 6862–69.CrossRef Bala, N., Singh, H. and Prakash, S., (2009) Appl. Surf. Sci., Vol. 255, No. 15, pp. 6862–69.CrossRef
20.
Zurück zum Zitat Zhao, W.M., Wang, Y., Han, T., Wu, K.Y. and Xue, J., (2004), Surf. Coat. Technol., Vol. 183, pp. 118-25.CrossRef Zhao, W.M., Wang, Y., Han, T., Wu, K.Y. and Xue, J., (2004), Surf. Coat. Technol., Vol. 183, pp. 118-25.CrossRef
21.
Zurück zum Zitat Zhao, W.M., Wang, Y., Dong, L.X., Wu, K.Y. and Xue, J., (2005), Surf. Coat. Technol., Vol. 190, pp. 293-98.CrossRef Zhao, W.M., Wang, Y., Dong, L.X., Wu, K.Y. and Xue, J., (2005), Surf. Coat. Technol., Vol. 190, pp. 293-98.CrossRef
22.
Zurück zum Zitat Miguel, J.M., Guilemany, J.M. and Vizcaino, S. (2003) Tribol. Int, Vol. 36, pp. 181-87.CrossRef Miguel, J.M., Guilemany, J.M. and Vizcaino, S. (2003) Tribol. Int, Vol. 36, pp. 181-87.CrossRef
23.
Zurück zum Zitat Sahraoui, T., Fenineche, N.E., Montavon, G. and Coddet, C. (2003) Mater. Des., 24, pp. 309-13.CrossRef Sahraoui, T., Fenineche, N.E., Montavon, G. and Coddet, C. (2003) Mater. Des., 24, pp. 309-13.CrossRef
24.
Zurück zum Zitat Lih, W.C. Yang, S.H. Su, C.Y. Huang, S.C. Hsu, I.C. and Leu, M.S., Surf. Coat. Technol. 133–134 (2000) 54–60.CrossRef Lih, W.C. Yang, S.H. Su, C.Y. Huang, S.C. Hsu, I.C. and Leu, M.S., Surf. Coat. Technol. 133–134 (2000) 54–60.CrossRef
25.
Zurück zum Zitat Rajasekaran, B., Raman, S.G.S., Joshi, S.V. and Sundararajan, S., (2006) Surf. Coat. Technol., Vol. 201, Issue 3–4, pp. 1548-58.CrossRef Rajasekaran, B., Raman, S.G.S., Joshi, S.V. and Sundararajan, S., (2006) Surf. Coat. Technol., Vol. 201, Issue 3–4, pp. 1548-58.CrossRef
27.
Zurück zum Zitat Sampath, S., Jiang, X.Y., Matejicek, J., Prchlik, L., Kulkarni, A. and Vaidya, A., (2004) Mater. Sci. Eng. A Struct., Vol. 364, pp. 216-31.CrossRef Sampath, S., Jiang, X.Y., Matejicek, J., Prchlik, L., Kulkarni, A. and Vaidya, A., (2004) Mater. Sci. Eng. A Struct., Vol. 364, pp. 216-31.CrossRef
28.
Zurück zum Zitat Ak, N.K., Tekmen, C., Ozdemir, I., Soykan, H.S. and Celik, E., (2003) Surf. Coat. Technol, Vol. 173-174, pp. 1070-73.CrossRef Ak, N.K., Tekmen, C., Ozdemir, I., Soykan, H.S. and Celik, E., (2003) Surf. Coat. Technol, Vol. 173-174, pp. 1070-73.CrossRef
29.
Zurück zum Zitat Singh, H., Puri, D. and Prakash, S. (2005b) Surf. Coat. Technol., 192(1), pp. 27-38.CrossRef Singh, H., Puri, D. and Prakash, S. (2005b) Surf. Coat. Technol., 192(1), pp. 27-38.CrossRef
30.
Zurück zum Zitat Singh, H., Puri, D., Prakash, S., Maiti, R. (2007) Mater. Sci. Eng. A 464 (1), pp. 110–16.CrossRef Singh, H., Puri, D., Prakash, S., Maiti, R. (2007) Mater. Sci. Eng. A 464 (1), pp. 110–16.CrossRef
31.
Zurück zum Zitat Lee, H.Y., Young, H.Y., Young, C.L., Young, P.H. and Kyung, H.K., (2005) J. Therm. Spray Technol., Vol. 14, No. 2, pp. 183-86.CrossRef Lee, H.Y., Young, H.Y., Young, C.L., Young, P.H. and Kyung, H.K., (2005) J. Therm. Spray Technol., Vol. 14, No. 2, pp. 183-86.CrossRef
32.
Zurück zum Zitat Kolta, G.A., Hewaidy, I.F. and Felix, N.S., (1972) Thermochim. Acta, Vol. 4, pp. 151-64. Kolta, G.A., Hewaidy, I.F. and Felix, N.S., (1972) Thermochim. Acta, Vol. 4, pp. 151-64.
33.
Zurück zum Zitat Das, D., Balasubramaniam, R. and Mungole, M.N., (2002) J. Mater. Sci., Vol. 37, No. 6, pp.1135-42.CrossRef Das, D., Balasubramaniam, R. and Mungole, M.N., (2002) J. Mater. Sci., Vol. 37, No. 6, pp.1135-42.CrossRef
34.
Zurück zum Zitat F.H. Stott and G.C. Wood: Mater. Sci. Technol., 1998, vol. 4, pp. 1072–78.CrossRef F.H. Stott and G.C. Wood: Mater. Sci. Technol., 1998, vol. 4, pp. 1072–78.CrossRef
35.
Zurück zum Zitat S.R.J. Saunders and J.R. Nicholls: Mater. Sci. Technol., 1998, vol. 5, pp. 780–98.CrossRef S.R.J. Saunders and J.R. Nicholls: Mater. Sci. Technol., 1998, vol. 5, pp. 780–98.CrossRef
36.
Zurück zum Zitat S. Kamal, R. Jayaganthan, S. Prakash, and S. Kumar: J. Alloys Compd., 2008, vol. 463 (1–2), pp. 358–72.CrossRef S. Kamal, R. Jayaganthan, S. Prakash, and S. Kumar: J. Alloys Compd., 2008, vol. 463 (1–2), pp. 358–72.CrossRef
37.
38.
Zurück zum Zitat U.K. Chatterjee, S.K. Bose, and S.K. Roy: Environmental Degradation of Metals, Marcel Dekker, New York, NY, 2001. U.K. Chatterjee, S.K. Bose, and S.K. Roy: Environmental Degradation of Metals, Marcel Dekker, New York, NY, 2001.
39.
40.
Zurück zum Zitat Sidhu, T.S. Agrawal, R.D. and Prakash, S. (2006) J. Mater. Eng. Perform., 15(1), 130–38.CrossRef Sidhu, T.S. Agrawal, R.D. and Prakash, S. (2006) J. Mater. Eng. Perform., 15(1), 130–38.CrossRef
41.
Zurück zum Zitat Sundararajan, T, Kuroda, S. Itagaki, T. and Abe, F. (2003) ISIJ Int., 43(1), 104–111.CrossRef Sundararajan, T, Kuroda, S. Itagaki, T. and Abe, F. (2003) ISIJ Int., 43(1), 104–111.CrossRef
42.
Zurück zum Zitat S.S. Chatha, H.S. Sidhu, B.S. Sidhu (2012) Surf. Coat. Technol., 206(19–20), 3839–50.CrossRef S.S. Chatha, H.S. Sidhu, B.S. Sidhu (2012) Surf. Coat. Technol., 206(19–20), 3839–50.CrossRef
43.
Zurück zum Zitat Zhu, Z., Cheng, X., Ye, W., Min, J. (2012). Int. J. Miner. Metall. Mater. 19(3), 266–70.CrossRef Zhu, Z., Cheng, X., Ye, W., Min, J. (2012). Int. J. Miner. Metall. Mater. 19(3), 266–70.CrossRef
Metadaten
Titel
Comparative High-Temperature Corrosion Behavior of Ni-20Cr Coatings on T22 Boiler Steel Produced by HVOF, D-Gun, and Cold Spraying
verfasst von
Gagandeep Kaushal
Niraj Bala
Narinder Kaur
Harpreet Singh
Satya Prakash
Publikationsdatum
01.01.2014
Verlag
Springer US
Erschienen in
Metallurgical and Materials Transactions A / Ausgabe 1/2014
Print ISSN: 1073-5623
Elektronische ISSN: 1543-1940
DOI
https://doi.org/10.1007/s11661-013-1984-4

Weitere Artikel der Ausgabe 1/2014

Metallurgical and Materials Transactions A 1/2014 Zur Ausgabe

Symposium: Deformation, Damage, and Fracture of Light Metals and Alloys

The Effect of Indium Additions on Mg-Li and Mg-Li-Al Alloys

    Marktübersichten

    Die im Laufe eines Jahres in der „adhäsion“ veröffentlichten Marktübersichten helfen Anwendern verschiedenster Branchen, sich einen gezielten Überblick über Lieferantenangebote zu verschaffen.