Skip to main content
Erschienen in: Metallurgical and Materials Transactions A 13/2007

01.09.2007 | Symposium: Deformation & Fracture from Nano to Macro: Honoring W.W. Gerberich's 70th Birthday

Dislocation Nucleation and Source Activation during Nanoindentation Yield Points

verfasst von: A.A. Zbib, D.F. Bahr

Erschienen in: Metallurgical and Materials Transactions A | Ausgabe 13/2007

Einloggen

Aktivieren Sie unsere intelligente Suche, um passende Fachinhalte oder Patente zu finden.

search-config
loading …

Abstract

The onset of plasticity during nanoindentation of a tungsten single crystal was examined as a function of pre-existing dislocation density. Vickers indentations were used to generate a spatially varying dislocation density, and nanoindentation was then carried out at regions of high and low dislocation densities. Even with dislocation densities as high as 1.8 × 1013 m−2, a sharp elastic-plastic transition was observed during some indentations. At lower dislocation densities, 3.5 × 109 m−2, the shear stress at the elastic plastic transition increased and approached the theoretical shear stress of the crystal. A first-order model that predicts the load required for the onset of plasticity during nanoindentation from the activation of a dislocation source within a critical volume of material, rather than homogeneous dislocation nucleation, is developed. The model correlates well with experimentally measured loads at the onset of plasticity for dislocation densities of 1012 m−2 and higher for these nanoindentation conditions.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
1.
2.
3.
Zurück zum Zitat A.B. Mann, J.B. Pethica: Appl. Phys. Lett., 1996, vol. 69, pp. 907–09CrossRef A.B. Mann, J.B. Pethica: Appl. Phys. Lett., 1996, vol. 69, pp. 907–09CrossRef
4.
Zurück zum Zitat W.W. Gerberich, J.C. Nelson, E.E. Lilleodden, P. Anderson, J.T. Wyrobek: Acta Mater., 1996, vol. 44, pp. 3585–98CrossRef W.W. Gerberich, J.C. Nelson, E.E. Lilleodden, P. Anderson, J.T. Wyrobek: Acta Mater., 1996, vol. 44, pp. 3585–98CrossRef
5.
Zurück zum Zitat S.A. Syed-Asif, J.B. Pethica: Phil. Mag. A, 1997, vol. 76, pp. 1105–18CrossRef S.A. Syed-Asif, J.B. Pethica: Phil. Mag. A, 1997, vol. 76, pp. 1105–18CrossRef
6.
Zurück zum Zitat D.F. Bahr, D.E. Kramer, W.W. Gerberich: Acta Mater., 1998, vol. 46, pp. 3605–17CrossRef D.F. Bahr, D.E. Kramer, W.W. Gerberich: Acta Mater., 1998, vol. 46, pp. 3605–17CrossRef
8.
Zurück zum Zitat J. Bradby, J. William, M. Swain: J. Mater. Res., 2003, vol. 19, pp. 380–86CrossRef J. Bradby, J. William, M. Swain: J. Mater. Res., 2003, vol. 19, pp. 380–86CrossRef
10.
Zurück zum Zitat C.L. Kelchner, S.J. Plimpton, J.C. Hamilton: Phys. Rev. B, 1998, vol. 58, pp. 11085–11088CrossRef C.L. Kelchner, S.J. Plimpton, J.C. Hamilton: Phys. Rev. B, 1998, vol. 58, pp. 11085–11088CrossRef
11.
Zurück zum Zitat D. Rodriquez-Marek, M. Pang, D.F. Bahr: Metall. Mater. Trans. A, 2003, vol. 34A, 1291–96CrossRef D. Rodriquez-Marek, M. Pang, D.F. Bahr: Metall. Mater. Trans. A, 2003, vol. 34A, 1291–96CrossRef
12.
Zurück zum Zitat M. Pang, D.F. Bahr: J. Mater. Res., 2001, vol. 16, pp. 2634–43 M. Pang, D.F. Bahr: J. Mater. Res., 2001, vol. 16, pp. 2634–43
13.
Zurück zum Zitat E. Weppelmann, M.V. Swain: Thin Solid Films, 1996, vol. 286, pp. 111–21CrossRef E. Weppelmann, M.V. Swain: Thin Solid Films, 1996, vol. 286, pp. 111–21CrossRef
14.
Zurück zum Zitat S.V. Hainsworth, M.R. McGurk, T.F. Page: Surf. Coat. Technol., 1998, vol. 102, pp. 97–107CrossRef S.V. Hainsworth, M.R. McGurk, T.F. Page: Surf. Coat. Technol., 1998, vol. 102, pp. 97–107CrossRef
15.
Zurück zum Zitat D.E. Kramer, K.B. Yoder, W.W. Gerberich: Phil. Mag. A, 2001, vol. 81, pp. 2033–58CrossRef D.E. Kramer, K.B. Yoder, W.W. Gerberich: Phil. Mag. A, 2001, vol. 81, pp. 2033–58CrossRef
16.
Zurück zum Zitat G.F. Vander Voort: Metallography Principles and Practice, McGraw-Hill, New York, NY, 1984, pp. 599 and 697 G.F. Vander Voort: Metallography Principles and Practice, McGraw-Hill, New York, NY, 1984, pp. 599 and 697
17.
19.
Zurück zum Zitat K.L. Johnson: Contact Mechanics, Cambridge University Press, New York, NY, 1985, pp. 90–104 K.L. Johnson: Contact Mechanics, Cambridge University Press, New York, NY, 1985, pp. 90–104
20.
Zurück zum Zitat N. Stelmashenko, M.G. Walls, L.M. Brown, and Yu.V. Milman: Acta Metall. Mater., 1993, vol. 46, pp. 2855–65 N. Stelmashenko, M.G. Walls, L.M. Brown, and Yu.V. Milman: Acta Metall. Mater., 1993, vol. 46, pp. 2855–65
21.
Zurück zum Zitat T. Michalske and J.E. Houston: Acta Mater., 1998, vol. 46, pp. 391–96CrossRef T. Michalske and J.E. Houston: Acta Mater., 1998, vol. 46, pp. 391–96CrossRef
22.
Zurück zum Zitat D.F. Bahr, D.E. Wilson, D.A. Crowson: J. Mater. Res., 1999, vol. 14, pp. 2269–75 D.F. Bahr, D.E. Wilson, D.A. Crowson: J. Mater. Res., 1999, vol. 14, pp. 2269–75
23.
Zurück zum Zitat J.G. Swadener, B. Taljit, G.M. Pharr: J. Mater. Res., 2001, vol. 16, pp. 2091–2102CrossRef J.G. Swadener, B. Taljit, G.M. Pharr: J. Mater. Res., 2001, vol. 16, pp. 2091–2102CrossRef
Metadaten
Titel
Dislocation Nucleation and Source Activation during Nanoindentation Yield Points
verfasst von
A.A. Zbib
D.F. Bahr
Publikationsdatum
01.09.2007
Verlag
Springer US
Erschienen in
Metallurgical and Materials Transactions A / Ausgabe 13/2007
Print ISSN: 1073-5623
Elektronische ISSN: 1543-1940
DOI
https://doi.org/10.1007/s11661-007-9284-5

Weitere Artikel der Ausgabe 13/2007

Metallurgical and Materials Transactions A 13/2007 Zur Ausgabe

SYMPOSIUM: Deformation & Fracture from Nano to Macro: Honoring W.W. Gerberich’s 70th Birthday

Crack-Tip Deformation Mechanisms in α-Fe and Binary Fe Alloys: An Atomistic Study on Single Crystals

Symposium: Deformation and Fracture from Nano to Macro: Honoring W.W. Gerberich's 70th Birthday

Deformation and Fracture from Nano to Macro: Honoring W.W. Gerberich’s 70th Birthday

SYMPOSIUM: Deformation & Fracture from Nano to Macro: Honoring W.W. Gerberich’s 70th Birthday

Microbridge Tests on Bilayer Thin Films

    Marktübersichten

    Die im Laufe eines Jahres in der „adhäsion“ veröffentlichten Marktübersichten helfen Anwendern verschiedenster Branchen, sich einen gezielten Überblick über Lieferantenangebote zu verschaffen.