Fracture Toughness and Adhesion of Transparent Al:ZnO Films Deposited on Glass Substrates

verfasst von: Xiaolu Pang, Hongjian Ma, Kewei Gao, Huisheng Yang, Xiaolei Wu, Alex A. Volinsky

Erschienen in: Journal of Materials Engineering and Performance | Ausgabe 10/2013

Einloggen

Aktivieren Sie unsere intelligente Suche, um passende Fachinhalte oder Patente zu finden.

search-config
loading …

Abstract

Al-doped zinc oxide films (AZO) of different thicknesses were deposited by reactive magnetron sputtering on glass substrates. Fracture toughness and adhesion of transparent AZO films were measured by indentation in air and water. Fracture toughness of glass is about 0.63 MPa·m1/2. Under the same normal load, radial crack length shortened with the increase of AZO film thickness. When indented under deionized water, cracks in both glass and AZO films got longer, signifying corresponding decrease in the fracture toughness.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
1.
Zurück zum Zitat X. Jiang, F.L. Wong, M.K. Fung, and S.T. Lee, Aluminum-Doped Zinc Oxide Films as Transparent Conductive Electrode for Organic Light-Emitting Devices, Appl. Phys. Lett., 2003, 83, p 1875CrossRef X. Jiang, F.L. Wong, M.K. Fung, and S.T. Lee, Aluminum-Doped Zinc Oxide Films as Transparent Conductive Electrode for Organic Light-Emitting Devices, Appl. Phys. Lett., 2003, 83, p 1875CrossRef
2.
Zurück zum Zitat J. Yoo, J. Lee, S. Kim, K. Yoon, I.J. Park, S.K. Dhungel, B. Karunagaran, D. Mangalaraj, and J. Yi, The Properties of Surface Textured ZnO:Al Films for Thin Film Solar Cells, Thin Solid Films, 2005, 480, p 213CrossRef J. Yoo, J. Lee, S. Kim, K. Yoon, I.J. Park, S.K. Dhungel, B. Karunagaran, D. Mangalaraj, and J. Yi, The Properties of Surface Textured ZnO:Al Films for Thin Film Solar Cells, Thin Solid Films, 2005, 480, p 213CrossRef
3.
Zurück zum Zitat M. Bender, E. Gagaoudakis, E. Douloufakis, E. Natsakou, N. Katsarakis, V. Cimalla, G. Kiriakidis, E. Fortunato, P. Nunes, A. Marques, and R. Martins, Production and Characterization of Zinc Oxide Thin Films for Room Temperature Ozone Sensing, Thin Solid Films, 2002, 418, p 45CrossRef M. Bender, E. Gagaoudakis, E. Douloufakis, E. Natsakou, N. Katsarakis, V. Cimalla, G. Kiriakidis, E. Fortunato, P. Nunes, A. Marques, and R. Martins, Production and Characterization of Zinc Oxide Thin Films for Room Temperature Ozone Sensing, Thin Solid Films, 2002, 418, p 45CrossRef
4.
Zurück zum Zitat S. Kobayakawa, Y. Tanaka, and A. Ide-Ektessabi, Characteristics of Al Doped Zinc Oxide (ZAO) Thin Films Deposited by RF Magnetron Sputtering, Nucl. Instrum. Methods B, 2006, 249, p 536CrossRef S. Kobayakawa, Y. Tanaka, and A. Ide-Ektessabi, Characteristics of Al Doped Zinc Oxide (ZAO) Thin Films Deposited by RF Magnetron Sputtering, Nucl. Instrum. Methods B, 2006, 249, p 536CrossRef
5.
Zurück zum Zitat M. Suchea, S. Christoulakis, N. Katsarakis, T. Kitsopoulos, and G. Kiriakidis, Comparative Study of Zinc Oxide and Aluminum Doped Zinc Oxide Transparent Thin Films Grown by Direct Current Magnetron Sputtering, Thin Solid Films, 2007, 515, p 6562CrossRef M. Suchea, S. Christoulakis, N. Katsarakis, T. Kitsopoulos, and G. Kiriakidis, Comparative Study of Zinc Oxide and Aluminum Doped Zinc Oxide Transparent Thin Films Grown by Direct Current Magnetron Sputtering, Thin Solid Films, 2007, 515, p 6562CrossRef
6.
Zurück zum Zitat H. Zhou, D. Yi, Z. Yu, L. Xiao, and J. Li, Preparation of Aluminum Doped Zinc Oxide Films and the Study of Their Microstructure, Electrical and Optical Properties, Thin Solid Films, 2007, 515, p 6909CrossRef H. Zhou, D. Yi, Z. Yu, L. Xiao, and J. Li, Preparation of Aluminum Doped Zinc Oxide Films and the Study of Their Microstructure, Electrical and Optical Properties, Thin Solid Films, 2007, 515, p 6909CrossRef
7.
Zurück zum Zitat W. Lin, R. Ma, W. Shao, and B. Liu, Structural, Electrical and Optical Properties of Gd Doped and Undoped ZnO:Al (ZAO) Thin Films Prepared by RF Magnetron Sputtering, Appl. Surf. Sci., 2007, 253, p 5180 W. Lin, R. Ma, W. Shao, and B. Liu, Structural, Electrical and Optical Properties of Gd Doped and Undoped ZnO:Al (ZAO) Thin Films Prepared by RF Magnetron Sputtering, Appl. Surf. Sci., 2007, 253, p 5180
8.
Zurück zum Zitat X. Pang, K. Gao, F. Luo, Y. Emirov, A.A. Levin, and A.A. Volinsky, Investigation of Microstructure and Mechanical Properties of Multi-layer Cr/Cr2O3 Coatings, Thin Solid Films, 2009, 517, p 1923–1926 X. Pang, K. Gao, F. Luo, Y. Emirov, A.A. Levin, and A.A. Volinsky, Investigation of Microstructure and Mechanical Properties of Multi-layer Cr/Cr2O3 Coatings, Thin Solid Films, 2009, 517, p 1923–1926
9.
Zurück zum Zitat W.W. Gerberich, W. Yu, D. Kramer, A. Strojny, D. Bahr, E. Lilleodden, and J. Nelson, Elastic Loading and Elastoplastic Unloading from Nanometer Level Indentations for Modulus Determinations, J. Mater. Res., 1998, 13(2), p 421CrossRef W.W. Gerberich, W. Yu, D. Kramer, A. Strojny, D. Bahr, E. Lilleodden, and J. Nelson, Elastic Loading and Elastoplastic Unloading from Nanometer Level Indentations for Modulus Determinations, J. Mater. Res., 1998, 13(2), p 421CrossRef
10.
Zurück zum Zitat M. Doerner and W.D. Nix, A Method for Interpreting the Data from Depth-Sensing Indentation Instruments, J. Mater. Res., 1986, 1, p 601CrossRef M. Doerner and W.D. Nix, A Method for Interpreting the Data from Depth-Sensing Indentation Instruments, J. Mater. Res., 1986, 1, p 601CrossRef
11.
Zurück zum Zitat G.M. Pharr, W.C. Oliver, and F. Brotzen, On the Generality of the Relationship Among Contact Stiffness, Contact Area and Elastic Modulus During Indentation, J. Mater. Res., 1992, 7(3), p 613CrossRef G.M. Pharr, W.C. Oliver, and F. Brotzen, On the Generality of the Relationship Among Contact Stiffness, Contact Area and Elastic Modulus During Indentation, J. Mater. Res., 1992, 7(3), p 613CrossRef
12.
Zurück zum Zitat W.C. Oliver and G.M. Pharr, An Improved Technique for Determining Hardness and Elastic Modulus Using Load and Displacement Sensing Indentation Experiment, J. Mater. Res., 1992, 7, p 1564CrossRef W.C. Oliver and G.M. Pharr, An Improved Technique for Determining Hardness and Elastic Modulus Using Load and Displacement Sensing Indentation Experiment, J. Mater. Res., 1992, 7, p 1564CrossRef
13.
Zurück zum Zitat D.B. Marshall and A.G. Evans, Measurement of Adherence of Residually Stressed Thin Films by Indentation. I. Mechanics of Interface Delamination, J. Appl. Phys., 1984, 56, p 2632CrossRef D.B. Marshall and A.G. Evans, Measurement of Adherence of Residually Stressed Thin Films by Indentation. I. Mechanics of Interface Delamination, J. Appl. Phys., 1984, 56, p 2632CrossRef
14.
Zurück zum Zitat J.J. Vlassak, M.D. Drory, and W.D. Nix, Simple Technique for Measuring the Adhesion of Brittle Films to Ductile Substrates with Application to Diamond-Coated Titanium, J. Mater. Res., 1997, 12(7), p 1900CrossRef J.J. Vlassak, M.D. Drory, and W.D. Nix, Simple Technique for Measuring the Adhesion of Brittle Films to Ductile Substrates with Application to Diamond-Coated Titanium, J. Mater. Res., 1997, 12(7), p 1900CrossRef
15.
Zurück zum Zitat M.D. Kriese and W.W. Gerberich, Quantitative Adhesion Measures of Multilayer Films: Part I. Indentation Mechanics, J. Mater. Res., 1999, 14(7), p 3007CrossRef M.D. Kriese and W.W. Gerberich, Quantitative Adhesion Measures of Multilayer Films: Part I. Indentation Mechanics, J. Mater. Res., 1999, 14(7), p 3007CrossRef
16.
Zurück zum Zitat M.D. Kriese and W.W. Gerberich, Quantitative Adhesion Measures of Multilayer Films: Part II. Indentation of W/Cu, W/W, Cr/W, J. Mater. Res., 1999, 14(7), p 3019CrossRef M.D. Kriese and W.W. Gerberich, Quantitative Adhesion Measures of Multilayer Films: Part II. Indentation of W/Cu, W/W, Cr/W, J. Mater. Res., 1999, 14(7), p 3019CrossRef
17.
Zurück zum Zitat A.A. Volinsky, N.I. Tymiak, M.D. Kriese, W.W. Gerberich, and J.W. Hutchinson, Quantitative Modeling and Measurement of Copper Thin Film Adhesion, Mater. Res. Soc. Symp. Proc., 1999, 539, p 277CrossRef A.A. Volinsky, N.I. Tymiak, M.D. Kriese, W.W. Gerberich, and J.W. Hutchinson, Quantitative Modeling and Measurement of Copper Thin Film Adhesion, Mater. Res. Soc. Symp. Proc., 1999, 539, p 277CrossRef
18.
Zurück zum Zitat A.A.Volinsky, N.R. Moody, W.W. Gerberich, Interfacial toughness measurements for thin films on substrates, Acta Mater. 50/3 (2002) 441 A.A.Volinsky, N.R. Moody, W.W. Gerberich, Interfacial toughness measurements for thin films on substrates, Acta Mater. 50/3 (2002) 441
19.
Zurück zum Zitat D.S. Harding, W.C. Oliver, and G.M. Pharr, Cracking During Nanoindentation and Its Use in the Measurement of Fracture Toughness, Mater. Res. Soc. Symp. Proc., 1995, 356, p 663CrossRef D.S. Harding, W.C. Oliver, and G.M. Pharr, Cracking During Nanoindentation and Its Use in the Measurement of Fracture Toughness, Mater. Res. Soc. Symp. Proc., 1995, 356, p 663CrossRef
20.
Zurück zum Zitat K.E. Lee, M. Wang, E.J. Kim, and S.H. Hahn, Structural, Electrical and Optical Properties of Sol-Gel AZO Thin Films, Curr. Appl. Phys., 2009, 9, p 685 K.E. Lee, M. Wang, E.J. Kim, and S.H. Hahn, Structural, Electrical and Optical Properties of Sol-Gel AZO Thin Films, Curr. Appl. Phys., 2009, 9, p 685
21.
Zurück zum Zitat B. Bhushan, Handbook of Micro/Nanotribology, 2nd ed., CRC Press, Boca Raton, 1999 B. Bhushan, Handbook of Micro/Nanotribology, 2nd ed., CRC Press, Boca Raton, 1999
22.
Zurück zum Zitat G.M. Pharr, Measurement of Mechanical Properties by Ultra-low Load Indentation, Mater. Sci. Eng., A, 1998, 253, p 151–159CrossRef G.M. Pharr, Measurement of Mechanical Properties by Ultra-low Load Indentation, Mater. Sci. Eng., A, 1998, 253, p 151–159CrossRef
23.
Zurück zum Zitat D.F. Bahr, D.E. Kramer, and W.W. Gerberich, Non-linear Deformation Mechanisms During Nanoindentation, Acta Mater., 1998, 46, p 3605CrossRef D.F. Bahr, D.E. Kramer, and W.W. Gerberich, Non-linear Deformation Mechanisms During Nanoindentation, Acta Mater., 1998, 46, p 3605CrossRef
24.
Zurück zum Zitat J. Malzbender, G. de With, and J.M.J. den Toonder, Elastic Modulus, Hardness and Fracture Toughness of Hybrid Coatings on Glass, Thin Solid Films, 2000, 366, p 149CrossRef J. Malzbender, G. de With, and J.M.J. den Toonder, Elastic Modulus, Hardness and Fracture Toughness of Hybrid Coatings on Glass, Thin Solid Films, 2000, 366, p 149CrossRef
25.
Zurück zum Zitat A.A. Volinsky, J.B. Vella, and W.W. Gerberich, Fracture Toughness, Adhesion and Mechanical Properties of Low-K Dielectric Thin Films Measured by Nanoindentation, Thin Solid Films, 2003, 429, p 202CrossRef A.A. Volinsky, J.B. Vella, and W.W. Gerberich, Fracture Toughness, Adhesion and Mechanical Properties of Low-K Dielectric Thin Films Measured by Nanoindentation, Thin Solid Films, 2003, 429, p 202CrossRef
26.
Zurück zum Zitat X. Pang, K. Gao, H. Yang, L. Qiao, and A.A. Volinsky, Annealing Effects on Microstructure and Mechanical Properties of Chromium Oxide Coatings, Thin Solid Films, 2008, 516, p 4685CrossRef X. Pang, K. Gao, H. Yang, L. Qiao, and A.A. Volinsky, Annealing Effects on Microstructure and Mechanical Properties of Chromium Oxide Coatings, Thin Solid Films, 2008, 516, p 4685CrossRef
27.
Zurück zum Zitat B.R. Lawn and A.G. Evans, Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack System, J. Am. Ceram. Soc., 1980, 63, p 574CrossRef B.R. Lawn and A.G. Evans, Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack System, J. Am. Ceram. Soc., 1980, 63, p 574CrossRef
28.
Zurück zum Zitat G.R. Anstis, P. Chantikul, B.R. Lawn, and D.B. Marshall, A critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I. Direct Crack Measurements, J. Am. Ceram. Soc., 1981, 64, p 536CrossRef G.R. Anstis, P. Chantikul, B.R. Lawn, and D.B. Marshall, A critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I. Direct Crack Measurements, J. Am. Ceram. Soc., 1981, 64, p 536CrossRef
29.
Zurück zum Zitat J. Chen and S.J. Bull, Indentation Fracture and Toughness Assessment for Thin Optical Coatings on Glass, J. Phys. D: Appl. Phys., 2007, 40, p 5403 J. Chen and S.J. Bull, Indentation Fracture and Toughness Assessment for Thin Optical Coatings on Glass, J. Phys. D: Appl. Phys., 2007, 40, p 5403
30.
Zurück zum Zitat B. Bhushan and X.D. Li, Nanomechanical Characterization of Solid Surfaces and Thin Films, Int. Mater. Rev., 2003, 48, p 125CrossRef B. Bhushan and X.D. Li, Nanomechanical Characterization of Solid Surfaces and Thin Films, Int. Mater. Rev., 2003, 48, p 125CrossRef
31.
Zurück zum Zitat X.D. Li, D.F. Diao, and B. Bhushan, Fracture Mechanisms of Thin Amorphous Carbon Films in Nanoindentation, Acta Mater., 1997, 45, p 4453CrossRef X.D. Li, D.F. Diao, and B. Bhushan, Fracture Mechanisms of Thin Amorphous Carbon Films in Nanoindentation, Acta Mater., 1997, 45, p 4453CrossRef
32.
33.
Zurück zum Zitat M.T. Laugier, New Formula for Indentation Toughness in Ceramics, J. Mater. Sci. Lett., 1987, 6, p 898 M.T. Laugier, New Formula for Indentation Toughness in Ceramics, J. Mater. Sci. Lett., 1987, 6, p 898
34.
Zurück zum Zitat K. Nihara, R. Morena, and D.P.H. Hasselman, Evaluation of K Ic of Brittle Solids by the Indentation Method with Low Crack-to-Indent Ratios, J. Mater. Sci. Lett., 1982, 1, p 13CrossRef K. Nihara, R. Morena, and D.P.H. Hasselman, Evaluation of K Ic of Brittle Solids by the Indentation Method with Low Crack-to-Indent Ratios, J. Mater. Sci. Lett., 1982, 1, p 13CrossRef
35.
Zurück zum Zitat M.M. Lim, C. Godoy, P.J. Modenesi, J.C. Avelar-Batista, A. Davison, and A. Matthews, Coating Fracture Toughness Determined by Vickers Indentation: An Important Parameter in Cavitation Erosion Resistance of WC-Co Thermally Sprayed Coatings, Surf. Coat. Technol., 2004, 177–178, p 492 M.M. Lim, C. Godoy, P.J. Modenesi, J.C. Avelar-Batista, A. Davison, and A. Matthews, Coating Fracture Toughness Determined by Vickers Indentation: An Important Parameter in Cavitation Erosion Resistance of WC-Co Thermally Sprayed Coatings, Surf. Coat. Technol., 2004, 177–178, p 492
36.
Zurück zum Zitat J. Jang, S. Wen, M.J. Lance, I.M. Anderson, and G.M. Pharr, Cracking and Phase Transformation in Silicon During Nanoindentation, Mater. Res. Soc. Symp. Proc., 2004, 795, p 313 J. Jang, S. Wen, M.J. Lance, I.M. Anderson, and G.M. Pharr, Cracking and Phase Transformation in Silicon During Nanoindentation, Mater. Res. Soc. Symp. Proc., 2004, 795, p 313
37.
Zurück zum Zitat T. Scholz, G.A. Schneider, J. Munoz-Saldana, and M.V. Swain, Fracture Toughness from Submicron Derived Indentation Cracks, Appl. Phys. Lett., 2004, 84, p 3056CrossRef T. Scholz, G.A. Schneider, J. Munoz-Saldana, and M.V. Swain, Fracture Toughness from Submicron Derived Indentation Cracks, Appl. Phys. Lett., 2004, 84, p 3056CrossRef
38.
Zurück zum Zitat J. Deva Reddy, A.A. Volinsky, C.L. Frewin, C. Locke, and S.E. Saddow, Mechanical Properties of Single and Polycrystalline SiC Thin Films, Mater. Res. Soc. Symp. Proc. Vol 1049, 2008 J. Deva Reddy, A.A. Volinsky, C.L. Frewin, C. Locke, and S.E. Saddow, Mechanical Properties of Single and Polycrystalline SiC Thin Films, Mater. Res. Soc. Symp. Proc. Vol 1049, 2008
39.
Zurück zum Zitat J. Chen and S.J. Bull, Indentation Fracture and Toughness Assessment for Thin Optical Coatings on Glass, J. Phys. D: Appl. Phys., 2007, 40, p 5405 J. Chen and S.J. Bull, Indentation Fracture and Toughness Assessment for Thin Optical Coatings on Glass, J. Phys. D: Appl. Phys., 2007, 40, p 5405
40.
Zurück zum Zitat J. Malzbender, G. de With, and J.M.J. den Toonder, Elastic Modulus, Indentation Pressure and Fracture Toughness of Hybrid Coatings on Glass, Thin Solid Films, 2000, 366, p 145CrossRef J. Malzbender, G. de With, and J.M.J. den Toonder, Elastic Modulus, Indentation Pressure and Fracture Toughness of Hybrid Coatings on Glass, Thin Solid Films, 2000, 366, p 145CrossRef
41.
Zurück zum Zitat P.D. Warren, Determining the Fracture Toughness of Brittle Materials by Hertzian Indentation, J. Eur. Ceram. Soc., 1995, 15, p 201CrossRef P.D. Warren, Determining the Fracture Toughness of Brittle Materials by Hertzian Indentation, J. Eur. Ceram. Soc., 1995, 15, p 201CrossRef
42.
Zurück zum Zitat J.J. Vlassak, Y. Lin, and T.Y. Tsui, Fracture of Organosilicate Glass Thin Films: Environmental Effects, Mater. Sci. Eng. A, 2005, 391, p 172 J.J. Vlassak, Y. Lin, and T.Y. Tsui, Fracture of Organosilicate Glass Thin Films: Environmental Effects, Mater. Sci. Eng. A, 2005, 391, p 172
43.
Zurück zum Zitat Y. Lin, T.Y. Tsui, and J.J. Vlassak, PECVD Low-Permittivity Organosilicate Glass Coatings: Adhesion, Fracture and Mechanical Properties, Acta Mater., 2007, 55, p 2463 Y. Lin, T.Y. Tsui, and J.J. Vlassak, PECVD Low-Permittivity Organosilicate Glass Coatings: Adhesion, Fracture and Mechanical Properties, Acta Mater., 2007, 55, p 2463
Metadaten
Titel
Fracture Toughness and Adhesion of Transparent Al:ZnO Films Deposited on Glass Substrates
verfasst von
Xiaolu Pang
Hongjian Ma
Kewei Gao
Huisheng Yang
Xiaolei Wu
Alex A. Volinsky
Publikationsdatum
01.10.2013
Verlag
Springer US
Erschienen in
Journal of Materials Engineering and Performance / Ausgabe 10/2013
Print ISSN: 1059-9495
Elektronische ISSN: 1544-1024
DOI
https://doi.org/10.1007/s11665-013-0603-2

Weitere Artikel der Ausgabe 10/2013

Journal of Materials Engineering and Performance 10/2013 Zur Ausgabe

    Marktübersichten

    Die im Laufe eines Jahres in der „adhäsion“ veröffentlichten Marktübersichten helfen Anwendern verschiedenster Branchen, sich einen gezielten Überblick über Lieferantenangebote zu verschaffen.