Abstract

To measure nanomechanical properties of surface layers of bulk materials and thin films, depth-sensing nanoindentation measurement techniques are used commonly. The nanoindentation apparatus continuously monitors the load and the position of the indenter relative to the surface of the specimen (depth of an indent or displacement) during the indentation process. Indentation experiments can be performed at a penetration depth of as low as about 5 nm. This paper presents an overview of various nanoindentation techniques, various measurement options, and data analysis. Data on elastic–plastic deformation behavior, hardness, elastic modulus, scratch resistance, film-substrate adhesion, residual stresses, time-dependent creep and relaxation properties, fracture toughness, and fatigue are presented.

Sie haben noch keine Lizenz? Dann Informieren Sie sich jetzt über unsere Produkte:

Springer Professional "Wirtschaft+Technik"

Online-Abonnement

Mit Springer Professional "Wirtschaft+Technik" erhalten Sie Zugriff auf:

  • über 102.000 Bücher
  • über 537 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Finance + Banking
  • Management + Führung
  • Marketing + Vertrieb
  • Maschinenbau + Werkstoffe
  • Versicherung + Risiko

Jetzt Wissensvorsprung sichern!

Springer Professional "Technik"

Online-Abonnement

Mit Springer Professional "Technik" erhalten Sie Zugriff auf:

  • über 67.000 Bücher
  • über 390 Zeitschriften

aus folgenden Fachgebieten:

  • Automobil + Motoren
  • Bauwesen + Immobilien
  • Business IT + Informatik
  • Elektrotechnik + Elektronik
  • Energie + Nachhaltigkeit
  • Maschinenbau + Werkstoffe




 

Jetzt Wissensvorsprung sichern!

Literatur
Zurück zum Zitat Ahn J, Mittal KL, Macqueen RH (1978) Adhesion measurement of thin films, thick films, and bulk coatings: hardness and adhesion of filmed structures as determined by the scratch technique STP 640. ASTM, Philadelphia, pp 134–157CrossRef Ahn J, Mittal KL, Macqueen RH (1978) Adhesion measurement of thin films, thick films, and bulk coatings: hardness and adhesion of filmed structures as determined by the scratch technique STP 640. ASTM, Philadelphia, pp 134–157CrossRef
Zurück zum Zitat Alba S, Loubet JL, Vovelle L (1993) Evaluation of mechanical properties and adhesion of polymer coatings by continous hardness measurements. J Adhes Sci Technol 7:131–140CrossRef Alba S, Loubet JL, Vovelle L (1993) Evaluation of mechanical properties and adhesion of polymer coatings by continous hardness measurements. J Adhes Sci Technol 7:131–140CrossRef
Zurück zum Zitat Alekhin VP, Berlin GS, Isaev AV, Kalei GN, Merkulov VA, Skvortsov VN, Ternovskii AP, Krushchov MM, Shnyrev GD, Shorshorov MKh (1972) Micromechanical testing by micromechanical testing of materials by microcompression. Zavod Lab 38:619–621 Alekhin VP, Berlin GS, Isaev AV, Kalei GN, Merkulov VA, Skvortsov VN, Ternovskii AP, Krushchov MM, Shnyrev GD, Shorshorov MKh (1972) Micromechanical testing by micromechanical testing of materials by microcompression. Zavod Lab 38:619–621
Zurück zum Zitat Anonymous (1979) Standard Test Method for Microhardness of Materials ASME Designation: E384-73, ASTM, Philadelphia, pp 359–379 Anonymous (1979) Standard Test Method for Microhardness of Materials ASME Designation: E384-73, ASTM, Philadelphia, pp 359–379
Zurück zum Zitat Anonymous (1988) Properties of Silicon EMIS Data Reviews Series No. 4, INSPEC, The Institution of Electrical Engineers, London Anonymous (1988) Properties of Silicon EMIS Data Reviews Series No. 4, INSPEC, The Institution of Electrical Engineers, London
Zurück zum Zitat Anonymous (2014) Keysight Nano Indenter G200 Data Sheet,” Keysight Technologies, Santa Rosa, CA Anonymous (2014) Keysight Nano Indenter G200 Data Sheet,” Keysight Technologies, Santa Rosa, CA
Zurück zum Zitat Antis GR, Chantikul P, Lawn BR, Marshall DB (1981) A critical evaluation of indentation techniques for measuring fracture toughness: I direct crack measurements. J Am Ceram Soc 64:533–538CrossRef Antis GR, Chantikul P, Lawn BR, Marshall DB (1981) A critical evaluation of indentation techniques for measuring fracture toughness: I direct crack measurements. J Am Ceram Soc 64:533–538CrossRef
Zurück zum Zitat Atkins AG, Silverio A, Tabor D (1966) Indentation hardness and the creep of solids. J Inst Metals 94:369–378 Atkins AG, Silverio A, Tabor D (1966) Indentation hardness and the creep of solids. J Inst Metals 94:369–378
Zurück zum Zitat Bell TJ, Field JS, Swain MV (1992) Elastic-plastic characterization of thin films with spherical indentation. Thin Solid Films 220:289–294CrossRef Bell TJ, Field JS, Swain MV (1992) Elastic-plastic characterization of thin films with spherical indentation. Thin Solid Films 220:289–294CrossRef
Zurück zum Zitat Benjamin P, Weaver C (1960) Measurement of adhesion of thin films. Proc R Soc Lond A 254:163–176CrossRef Benjamin P, Weaver C (1960) Measurement of adhesion of thin films. Proc R Soc Lond A 254:163–176CrossRef
Zurück zum Zitat Berkovich ES (1951) Three-faceted diamond pyramid for micro-hardness testing. Indus Diam Rev 11:129–132 Berkovich ES (1951) Three-faceted diamond pyramid for micro-hardness testing. Indus Diam Rev 11:129–132
Zurück zum Zitat Bhattacharya AK, Nix WE (1988a) Finite element simulation of indentation experiments. Int J Solids Struct 24:881–891CrossRef Bhattacharya AK, Nix WE (1988a) Finite element simulation of indentation experiments. Int J Solids Struct 24:881–891CrossRef
Zurück zum Zitat Bhattacharya AK, Nix WD (1988b) Analysis of elastic and plastic deformation associated with indentation testing of the thin films on substrates. Int J Solids Struct 24:1287–1298CrossRef Bhattacharya AK, Nix WD (1988b) Analysis of elastic and plastic deformation associated with indentation testing of the thin films on substrates. Int J Solids Struct 24:1287–1298CrossRef
Zurück zum Zitat Bhushan B (1987) Overview of Coating Materials, Surface Treatments, and Screening Techniques for Tribological Applications—Part 2: Screening Techniques. In: Harding WB, DiBari GA (eds) Testing of Metallic and Inorganic Coatings STP 947. ASTM, Philadelphia, pp 310–319CrossRef Bhushan B (1987) Overview of Coating Materials, Surface Treatments, and Screening Techniques for Tribological Applications—Part 2: Screening Techniques. In: Harding WB, DiBari GA (eds) Testing of Metallic and Inorganic Coatings STP 947. ASTM, Philadelphia, pp 310–319CrossRef
Zurück zum Zitat Bhushan B (1996) Tribology and mechanics of magnetic storage devices, 2nd edn. Springer, New YorkCrossRef Bhushan B (1996) Tribology and mechanics of magnetic storage devices, 2nd edn. Springer, New YorkCrossRef
Zurück zum Zitat Bhushan B (1999a) Nanomechanical properties of solid surfaces and thin films, in Handbook of micro/nanotribology, 2nd edn. CRC Press, Boca Raton, pp 443–524 Bhushan B (1999a) Nanomechanical properties of solid surfaces and thin films, in Handbook of micro/nanotribology, 2nd edn. CRC Press, Boca Raton, pp 443–524
Zurück zum Zitat Bhushan B (1999b) Wear and mechanical characterisation on micro- to picoscales using AFM. Int Mater Rev 44:105–117CrossRef Bhushan B (1999b) Wear and mechanical characterisation on micro- to picoscales using AFM. Int Mater Rev 44:105–117CrossRef
Zurück zum Zitat Bhushan B (1999c) Chemical, mechanical, and tribological characterization of ultra-thin and hard amorphous carbon coatings as thin as 3.5 nm: recent developments. Diam Relat Mater 8:1985–2015CrossRef Bhushan B (1999c) Chemical, mechanical, and tribological characterization of ultra-thin and hard amorphous carbon coatings as thin as 3.5 nm: recent developments. Diam Relat Mater 8:1985–2015CrossRef
Zurück zum Zitat Bhushan B (2001) Modern tribology handbook, Vol. 1 and 2. CRC Press, Boca Raton Bhushan B (2001) Modern tribology handbook, Vol. 1 and 2. CRC Press, Boca Raton
Zurück zum Zitat Bhushan B (2011) Nanotribology and nanomechanics I & II. Springer, HeidelbergCrossRef Bhushan B (2011) Nanotribology and nanomechanics I & II. Springer, HeidelbergCrossRef
Zurück zum Zitat Bhushan B (2013a) Principles and applications of tribology, 2nd edn. Wiley, New YorkCrossRef Bhushan B (2013a) Principles and applications of tribology, 2nd edn. Wiley, New YorkCrossRef
Zurück zum Zitat Bhushan B (2013b) Introduction to tribology, 2nd edn. Wiley, New YorkCrossRef Bhushan B (2013b) Introduction to tribology, 2nd edn. Wiley, New YorkCrossRef
Zurück zum Zitat Bhushan B (2017) Springer handbook of nanotechnology, 4th edn. Springer International, Switzerland Bhushan B (2017) Springer handbook of nanotechnology, 4th edn. Springer International, Switzerland
Zurück zum Zitat Bhushan B, Gupta BK (1995) Micromechanical Characterization of Ni-P Coated Aluminum-Magnesium, Glass, and Glass Ceramic Substrates and Finished Magnetic Thin-Film Rigid Disks. Adv Info Storage Syst 6:193–208CrossRef Bhushan B, Gupta BK (1995) Micromechanical Characterization of Ni-P Coated Aluminum-Magnesium, Glass, and Glass Ceramic Substrates and Finished Magnetic Thin-Film Rigid Disks. Adv Info Storage Syst 6:193–208CrossRef
Zurück zum Zitat Bhushan B, Gupta BK (1997) Handbook of Tribology: Materials, Coatings and Surface Treatments, McGraw Hill, New York (1991); Reprint edition (1997). Krieger Publishing Co., Malabar Bhushan B, Gupta BK (1997) Handbook of Tribology: Materials, Coatings and Surface Treatments, McGraw Hill, New York (1991); Reprint edition (1997). Krieger Publishing Co., Malabar
Zurück zum Zitat Bhushan B, Koinkar VN (1994) Nanoindentation hardness measurements using atomic force microscopy. Appl Phys Lett 64:1653–1655CrossRef Bhushan B, Koinkar VN (1994) Nanoindentation hardness measurements using atomic force microscopy. Appl Phys Lett 64:1653–1655CrossRef
Zurück zum Zitat Bhushan B, Li X (1997) Micromechanical and tribological characterization of doped single-crystal silicon and polysilicon films for microelectromechanical system devices. J Mater Res 12:54–63CrossRef Bhushan B, Li X (1997) Micromechanical and tribological characterization of doped single-crystal silicon and polysilicon films for microelectromechanical system devices. J Mater Res 12:54–63CrossRef
Zurück zum Zitat Bhushan B, Li X (2003) Nanomechanical characterisation of solid surfaces and thin films. Int Mater Rev 48:125–164CrossRef Bhushan B, Li X (2003) Nanomechanical characterisation of solid surfaces and thin films. Int Mater Rev 48:125–164CrossRef
Zurück zum Zitat Bhushan B, Patton ST (1996) Pole tip recession studies of hard carbon-coated thin-film tape heads. J Appl Phys 79:5916–5918CrossRef Bhushan B, Patton ST (1996) Pole tip recession studies of hard carbon-coated thin-film tape heads. J Appl Phys 79:5916–5918CrossRef
Zurück zum Zitat Bhushan B, Venkatesan S (2005) Effective mechanical properties of layered rough surfaces. Thin Solid Films 473:278–295CrossRef Bhushan B, Venkatesan S (2005) Effective mechanical properties of layered rough surfaces. Thin Solid Films 473:278–295CrossRef
Zurück zum Zitat Bhushan B, Landesman AL, Shack RV, Vukobratovich D, Walters VS (1985) Instrument for Testing Thin Films Such as Magnetic Tapes. IBM Tech Discl Bull 28:2975–2976 Bhushan B, Landesman AL, Shack RV, Vukobratovich D, Walters VS (1985) Instrument for Testing Thin Films Such as Magnetic Tapes. IBM Tech Discl Bull 28:2975–2976
Zurück zum Zitat Bhushan B, Williams VS, Shack RV (1988) In-situ nanoindentation hardness apparatus for mechanical characterization of extremely thin films. ASME J Tribol 110:563–571CrossRef Bhushan B, Williams VS, Shack RV (1988) In-situ nanoindentation hardness apparatus for mechanical characterization of extremely thin films. ASME J Tribol 110:563–571CrossRef
Zurück zum Zitat Bhushan B, Gupta BK, Azarian MH (1995) Nanoindentation, microscratch, friciton and wear studies of coatings for contact recording applications. Wear 181–183:743–758CrossRef Bhushan B, Gupta BK, Azarian MH (1995) Nanoindentation, microscratch, friciton and wear studies of coatings for contact recording applications. Wear 181–183:743–758CrossRef
Zurück zum Zitat Bhushan B, Kulkarni AV, Bonin W, Wyrobek JT (1996a) Nanoindentation and picoindentation measurements using a capacitive transducer system in atomic force microscopy. Philos Mag 74:1117–1128CrossRef Bhushan B, Kulkarni AV, Bonin W, Wyrobek JT (1996a) Nanoindentation and picoindentation measurements using a capacitive transducer system in atomic force microscopy. Philos Mag 74:1117–1128CrossRef
Zurück zum Zitat Bhushan B, Chyung K, Miller RA (1996b) Micromechanical property measurements of glass and glass-ceramic substrates for magnetic thin-film rigid disks for gigabit recording. Adv Info Storage Syst 7:3–16 Bhushan B, Chyung K, Miller RA (1996b) Micromechanical property measurements of glass and glass-ceramic substrates for magnetic thin-film rigid disks for gigabit recording. Adv Info Storage Syst 7:3–16
Zurück zum Zitat Bhushan B, Theunissen GSAM, Li X (1997) Tribological studies of chromium oxide films for magnetic recording applications. Thin Solid Films 311:67–80CrossRef Bhushan B, Theunissen GSAM, Li X (1997) Tribological studies of chromium oxide films for magnetic recording applications. Thin Solid Films 311:67–80CrossRef
Zurück zum Zitat Bhushan B, Luo D, Schricker SR, Sigmund W, Zauscher S (2014) Handbook of nanomaterials properties, Vol. 1-2. Springer, HeidelbergCrossRef Bhushan B, Luo D, Schricker SR, Sigmund W, Zauscher S (2014) Handbook of nanomaterials properties, Vol. 1-2. Springer, HeidelbergCrossRef
Zurück zum Zitat Blau PJ, Lawn BR (1986) Microindentation techniques in materials science and engineering, STP 889. ASTM, Philadelphia Blau PJ, Lawn BR (1986) Microindentation techniques in materials science and engineering, STP 889. ASTM, Philadelphia
Zurück zum Zitat Blau PJ, Oliver WC, Snead L (1997) The scanning micro-sclerometer: a new method for scratch hardness mapping. Tribol Int 30:483–490CrossRef Blau PJ, Oliver WC, Snead L (1997) The scanning micro-sclerometer: a new method for scratch hardness mapping. Tribol Int 30:483–490CrossRef
Zurück zum Zitat Bolshakov A, Oliver WC, Pharr GM (1996) Influences of stress on the measurement of mechanical properties using nanoindentation. II. Finite element simulations. J Mater Res 11:760–768CrossRef Bolshakov A, Oliver WC, Pharr GM (1996) Influences of stress on the measurement of mechanical properties using nanoindentation. II. Finite element simulations. J Mater Res 11:760–768CrossRef
Zurück zum Zitat Buckle H (1973) Use of the hardness test to determine other material properties. In: Westbrook JW, Conrad H (eds) The science of hardness testing and its research applications. American Society for Metals, Metals Park, Ohio, pp 453–491 Buckle H (1973) Use of the hardness test to determine other material properties. In: Westbrook JW, Conrad H (eds) The science of hardness testing and its research applications. American Society for Metals, Metals Park, Ohio, pp 453–491
Zurück zum Zitat Bull SJ, Rickerby DS (1990) New developments in the modelling of the hardness and scratch adhesion of thin films. Surf Coat Technol 42:149–164CrossRef Bull SJ, Rickerby DS (1990) New developments in the modelling of the hardness and scratch adhesion of thin films. Surf Coat Technol 42:149–164CrossRef
Zurück zum Zitat Bulychev SI, Alekhin VP, Shorshorov MKh, Ternovskii AP, Shnyrev GD (1975) Determining Young’s modulus from the indenter penetration diagram. Zavod Lab 41:11137–11140 Bulychev SI, Alekhin VP, Shorshorov MKh, Ternovskii AP, Shnyrev GD (1975) Determining Young’s modulus from the indenter penetration diagram. Zavod Lab 41:11137–11140
Zurück zum Zitat Bulychev SI, Alekhin VP, Shorshorov MKh (1979) Studies of physico-mechanical properties in surface layers and microvolumes of materials by the method of continuous application of an indenter. Fizika Khim. Obrab. Materialov, No, p 5 Bulychev SI, Alekhin VP, Shorshorov MKh (1979) Studies of physico-mechanical properties in surface layers and microvolumes of materials by the method of continuous application of an indenter. Fizika Khim. Obrab. Materialov, No, p 5
Zurück zum Zitat Burnett PJ, Rickerby DS (1987a) The relationship between hardness and scratch adhesion. Thin Solid Films 154:403–416CrossRef Burnett PJ, Rickerby DS (1987a) The relationship between hardness and scratch adhesion. Thin Solid Films 154:403–416CrossRef
Zurück zum Zitat Burnett PJ, Rickerby DS (1987b) The mechanical properties of wear resistant coatings I: modelling of hardness behavior. Thin Solid Films 148:41–50CrossRef Burnett PJ, Rickerby DS (1987b) The mechanical properties of wear resistant coatings I: modelling of hardness behavior. Thin Solid Films 148:41–50CrossRef
Zurück zum Zitat Callahan DL, Morris JC (1992) The extent of phase transformation in silicon hardness indentations. J Mater Res 7:1614–1617CrossRef Callahan DL, Morris JC (1992) The extent of phase transformation in silicon hardness indentations. J Mater Res 7:1614–1617CrossRef
Zurück zum Zitat Campbell DS (1970) Mechanical properties of thin films. In: Maissel LI, Glang R (eds) Handbook of thin film technology, Chap. 12. McGraw-Hill, New York Campbell DS (1970) Mechanical properties of thin films. In: Maissel LI, Glang R (eds) Handbook of thin film technology, Chap. 12. McGraw-Hill, New York
Zurück zum Zitat Chantikul P, Anstis GR, Lawn BR, Marshall DB (1981) A critical evaluation of indentation techniques for measuring fracture toughness: II, strength method. J Am Ceram Soc 64:539–543CrossRef Chantikul P, Anstis GR, Lawn BR, Marshall DB (1981) A critical evaluation of indentation techniques for measuring fracture toughness: II, strength method. J Am Ceram Soc 64:539–543CrossRef
Zurück zum Zitat Chiang SS, Marshall DB, Evans AG (1981) Simple method for adhesion measurement. In: Pask J, Evans AG (eds) Surfaces and interfaces in ceramics and ceramic-metal systems. Plenum, New York, pp 603–612CrossRef Chiang SS, Marshall DB, Evans AG (1981) Simple method for adhesion measurement. In: Pask J, Evans AG (eds) Surfaces and interfaces in ceramics and ceramic-metal systems. Plenum, New York, pp 603–612CrossRef
Zurück zum Zitat Chiang SS, Marshall DB, Evans AG (1982) The response of solids to elastic/plastic indentation: I. Stresses and residual stresses. J Appl Phys 53:298–311CrossRef Chiang SS, Marshall DB, Evans AG (1982) The response of solids to elastic/plastic indentation: I. Stresses and residual stresses. J Appl Phys 53:298–311CrossRef
Zurück zum Zitat Cho D, Bhushan B (2016) Nanofriction and nanowear of polypropylene, polyethylene terephthalate, and high-density polyethylene during sliding. Wear 352–353:18–23CrossRef Cho D, Bhushan B (2016) Nanofriction and nanowear of polypropylene, polyethylene terephthalate, and high-density polyethylene during sliding. Wear 352–353:18–23CrossRef
Zurück zum Zitat Chu SNG, Li JCM (1977) Impression creep: a new creep test. J Mater Sci 12:2200–2208CrossRef Chu SNG, Li JCM (1977) Impression creep: a new creep test. J Mater Sci 12:2200–2208CrossRef
Zurück zum Zitat Chu SNG, Li JCM (1980) Localized stress relaxation by impression testing. Mater Sci Eng 45:167–171CrossRef Chu SNG, Li JCM (1980) Localized stress relaxation by impression testing. Mater Sci Eng 45:167–171CrossRef
Zurück zum Zitat Cook RF, Pharr GM (1990) Direct observation and analysis of indentation cracking in glasses and ceramics. J Am Ceram Soc 73:787–817CrossRef Cook RF, Pharr GM (1990) Direct observation and analysis of indentation cracking in glasses and ceramics. J Am Ceram Soc 73:787–817CrossRef
Zurück zum Zitat Doerner MF, Nix WD (1986) A method for interpreting the data from depth-sensing indentation instruments. J Mater Res 1:601–609CrossRef Doerner MF, Nix WD (1986) A method for interpreting the data from depth-sensing indentation instruments. J Mater Res 1:601–609CrossRef
Zurück zum Zitat Doerner MF, Gardner DS, Nix WD (1986) Plastic properties of thin films on substrates as measured by submicron indentation hardness and substrate curvature techniques. J Mater Res 1:845–851CrossRef Doerner MF, Gardner DS, Nix WD (1986) Plastic properties of thin films on substrates as measured by submicron indentation hardness and substrate curvature techniques. J Mater Res 1:845–851CrossRef
Zurück zum Zitat Evans AG, Hutchinson JW (1984) On the mechanics of delamination and spalling in compressed films. Int J Solids Struct 20:455–466CrossRef Evans AG, Hutchinson JW (1984) On the mechanics of delamination and spalling in compressed films. Int J Solids Struct 20:455–466CrossRef
Zurück zum Zitat Fabes BD, Oliver WC, McKee RA, Walker FJ (1992) The determination of film hardness from the composite response of film and substrate to nanometer scale indentation. J Mater Res 7:3056–3064CrossRef Fabes BD, Oliver WC, McKee RA, Walker FJ (1992) The determination of film hardness from the composite response of film and substrate to nanometer scale indentation. J Mater Res 7:3056–3064CrossRef
Zurück zum Zitat Fleck NA, Muller GM, Ashby MF, Hutchinson JW (1994) Strain gradient plasticity: theory and experiments. Acta Metall et Mater 42:475–487CrossRef Fleck NA, Muller GM, Ashby MF, Hutchinson JW (1994) Strain gradient plasticity: theory and experiments. Acta Metall et Mater 42:475–487CrossRef
Zurück zum Zitat Gane N, Cox JM (1970) The micro-hardness of metals at very low loads. Philos Mag 22:881–891CrossRef Gane N, Cox JM (1970) The micro-hardness of metals at very low loads. Philos Mag 22:881–891CrossRef
Zurück zum Zitat Goken M, Kempf M (2001) Pop-ins in nanoindentation-the initial yield point. Zeitschrift Metallikd 92:1061–1067 Goken M, Kempf M (2001) Pop-ins in nanoindentation-the initial yield point. Zeitschrift Metallikd 92:1061–1067
Zurück zum Zitat Greene JE, Woodhouse J, Pestes M (1974) A technique for detecting critical loads in the scratch test for thin-film adhesion. Rev Sci Instrum 45:747–749CrossRef Greene JE, Woodhouse J, Pestes M (1974) A technique for detecting critical loads in the scratch test for thin-film adhesion. Rev Sci Instrum 45:747–749CrossRef
Zurück zum Zitat Gupta BK, Bhushan B (1994) The nanoindentation studies of ion implanted silicon. Surf Coat Technol 68(69):564–570CrossRef Gupta BK, Bhushan B (1994) The nanoindentation studies of ion implanted silicon. Surf Coat Technol 68(69):564–570CrossRef
Zurück zum Zitat Gupta BK, Bhushan B (1995a) Micromechanical properties of amorphous carbon coatings deposited by different deposition techniques. Thin Solid Films 270:391–398CrossRef Gupta BK, Bhushan B (1995a) Micromechanical properties of amorphous carbon coatings deposited by different deposition techniques. Thin Solid Films 270:391–398CrossRef
Zurück zum Zitat Gupta BK, Bhushan B (1995b) Mechanical and tribological properties of hard carbon coatings for magnetic recording heads. Wear 190:110–122CrossRef Gupta BK, Bhushan B (1995b) Mechanical and tribological properties of hard carbon coatings for magnetic recording heads. Wear 190:110–122CrossRef
Zurück zum Zitat Gupta BK, Chevallier J, Bhushan B (1993) Tribology of ion bombarded silicon for micromechanical applications. ASME J Tribol 115:392–399CrossRef Gupta BK, Chevallier J, Bhushan B (1993) Tribology of ion bombarded silicon for micromechanical applications. ASME J Tribol 115:392–399CrossRef
Zurück zum Zitat Gupta BK, Bhushan B, Chevallier J (1994) Modification of tribological properties of silicon by boron ion implantation. Tribol Trans 37:601–607CrossRef Gupta BK, Bhushan B, Chevallier J (1994) Modification of tribological properties of silicon by boron ion implantation. Tribol Trans 37:601–607CrossRef
Zurück zum Zitat Hainsworth SV, Chandler HW, Page TF (1996) Analysis of nanoindentation load-displacement loading curves. J Mater Res 14:2283–2295 Hainsworth SV, Chandler HW, Page TF (1996) Analysis of nanoindentation load-displacement loading curves. J Mater Res 14:2283–2295
Zurück zum Zitat Hainsworth SV, McGurk MR, Page TF (1998) The effect of coating cracking on the indentation response of thin hard-coated systems. Surf Coat Technol 102:97–107CrossRef Hainsworth SV, McGurk MR, Page TF (1998) The effect of coating cracking on the indentation response of thin hard-coated systems. Surf Coat Technol 102:97–107CrossRef
Zurück zum Zitat Hannula SP, Wanagel J, Li CY (1986) A Miniaturized Mechanical Testing System for Small Scale Specimen Testing. In: Corwin WR, Lucas GE (eds) The Use of Small-Scale Specimens for Testing Irradiated Material STP 888. ASTM, Philadelphia, pp 233–251CrossRef Hannula SP, Wanagel J, Li CY (1986) A Miniaturized Mechanical Testing System for Small Scale Specimen Testing. In: Corwin WR, Lucas GE (eds) The Use of Small-Scale Specimens for Testing Irradiated Material STP 888. ASTM, Philadelphia, pp 233–251CrossRef
Zurück zum Zitat Hay JC, Bolshakov A, Pharr GM (1999) A critical examination of the fundamental relations used in the analysis of nanoindentation data. J Mater Res 14:2296–2305CrossRef Hay JC, Bolshakov A, Pharr GM (1999) A critical examination of the fundamental relations used in the analysis of nanoindentation data. J Mater Res 14:2296–2305CrossRef
Zurück zum Zitat Heavens OS (1950) Some factors influencing the adhesion of films produced by vacuum evaporation. J Phys Rad 11:355–360CrossRef Heavens OS (1950) Some factors influencing the adhesion of films produced by vacuum evaporation. J Phys Rad 11:355–360CrossRef
Zurück zum Zitat Henshall JL, Brookes CA (1985) The measurement of KIc in single crystal SiC using the indentation method. J Mater Sci Lett 4:783–786CrossRef Henshall JL, Brookes CA (1985) The measurement of KIc in single crystal SiC using the indentation method. J Mater Sci Lett 4:783–786CrossRef
Zurück zum Zitat Hong S, Weihs TP, Bravman JC, Nix WD (1990) Measuring stiffnesses and residual stresses of silicon nitride in thin films. J Electron Mater 19:903CrossRef Hong S, Weihs TP, Bravman JC, Nix WD (1990) Measuring stiffnesses and residual stresses of silicon nitride in thin films. J Electron Mater 19:903CrossRef
Zurück zum Zitat Jacobson S, Jonsson B, Sundquist B (1983) The use of fast heavy ions to improve thin film adhesion. Thin Solid Films 107:89–98CrossRef Jacobson S, Jonsson B, Sundquist B (1983) The use of fast heavy ions to improve thin film adhesion. Thin Solid Films 107:89–98CrossRef
Zurück zum Zitat Joslin DL, Oliver WC (1990) A new method for analyzing data from continuous depth-sensing microindentation tests. J Mater Res 5:123–126CrossRef Joslin DL, Oliver WC (1990) A new method for analyzing data from continuous depth-sensing microindentation tests. J Mater Res 5:123–126CrossRef
Zurück zum Zitat King RB (1987) Elastic analysis of some punch problems for layered medium. Int J Solids Struct 23:1657–1664MATHCrossRef King RB (1987) Elastic analysis of some punch problems for layered medium. Int J Solids Struct 23:1657–1664MATHCrossRef
Zurück zum Zitat Korsunsky AM, McGurk MR, Bull SJ, Page TF (1998) On the hardness of coated systems. Surf Coat Technol 99:171–183CrossRef Korsunsky AM, McGurk MR, Bull SJ, Page TF (1998) On the hardness of coated systems. Surf Coat Technol 99:171–183CrossRef
Zurück zum Zitat Kulkarni AV, Bhushan B (1996a) Nanoscale mechanical property measurements using modified atomic force microscopy. Thin Solid Films 290–291:206–210CrossRef Kulkarni AV, Bhushan B (1996a) Nanoscale mechanical property measurements using modified atomic force microscopy. Thin Solid Films 290–291:206–210CrossRef
Zurück zum Zitat Kulkarni AV, Bhushan B (1996b) Nano/picoindentation measurements on single-crystal aluminum using modified atomic force microscopy. Mater Lett 29:221–227CrossRef Kulkarni AV, Bhushan B (1996b) Nano/picoindentation measurements on single-crystal aluminum using modified atomic force microscopy. Mater Lett 29:221–227CrossRef
Zurück zum Zitat Kulkarni AV, Bhushan B (1997) Nanoindentation measurements of amorphous carbon coatings. J Mater Res 12:2707–2714CrossRef Kulkarni AV, Bhushan B (1997) Nanoindentation measurements of amorphous carbon coatings. J Mater Res 12:2707–2714CrossRef
Zurück zum Zitat Kumar A, Bhushan B (2015) Nanomechanical, nanotribological, and macrotribological characterization of hard coatings and surface treatment of H-13 steel. Tribol Int 81:149–158CrossRef Kumar A, Bhushan B (2015) Nanomechanical, nanotribological, and macrotribological characterization of hard coatings and surface treatment of H-13 steel. Tribol Int 81:149–158CrossRef
Zurück zum Zitat LaFontaine WR, Yost B, Black RD, Li CY (1990) Indentation load relaxation experiments with indentation depth in the submicron range. J Mater Res 5:2100–2116CrossRef LaFontaine WR, Yost B, Black RD, Li CY (1990) Indentation load relaxation experiments with indentation depth in the submicron range. J Mater Res 5:2100–2116CrossRef
Zurück zum Zitat LaFontaine WR, Paszkiet CA, Korhonen MA, Li CY (1991) Residual stress measurements of thin aluminum metallizations by continuous indentation and X-ray stress measurement techniques. J Mater Res 6:2084–2090CrossRef LaFontaine WR, Paszkiet CA, Korhonen MA, Li CY (1991) Residual stress measurements of thin aluminum metallizations by continuous indentation and X-ray stress measurement techniques. J Mater Res 6:2084–2090CrossRef
Zurück zum Zitat Lankford J (1981) Threshold-microfracture during elastic/plastic indentation of ceramics. J Mater Sci 16:1177–1182CrossRef Lankford J (1981) Threshold-microfracture during elastic/plastic indentation of ceramics. J Mater Sci 16:1177–1182CrossRef
Zurück zum Zitat Laugier M (1981) The development of scratch test technique for the determination of the adhesion of coating. Thin Solid Films 76:289–294CrossRef Laugier M (1981) The development of scratch test technique for the determination of the adhesion of coating. Thin Solid Films 76:289–294CrossRef
Zurück zum Zitat Laursen TA, Simo JC (1992) A study of the mechanics of microindentation using finite elements. J Mater Res 7:618–626CrossRef Laursen TA, Simo JC (1992) A study of the mechanics of microindentation using finite elements. J Mater Res 7:618–626CrossRef
Zurück zum Zitat Lawn B (1993) Fracture of brittle solids, 2nd edn. Cambridge University Press, CambridgeCrossRef Lawn B (1993) Fracture of brittle solids, 2nd edn. Cambridge University Press, CambridgeCrossRef
Zurück zum Zitat Lawn B, Wilshaw R (1975) Review indentation fracture: principles and applications. J Mater Sci 10:1049–1081CrossRef Lawn B, Wilshaw R (1975) Review indentation fracture: principles and applications. J Mater Sci 10:1049–1081CrossRef
Zurück zum Zitat Lawn BR, Evans AG, Marshall DB (1980) Elastic/plastic indentation damage in ceramics: the median/radial crack system. J Am Ceram Soc 63:574–581CrossRef Lawn BR, Evans AG, Marshall DB (1980) Elastic/plastic indentation damage in ceramics: the median/radial crack system. J Am Ceram Soc 63:574–581CrossRef
Zurück zum Zitat Li X, Bhushan B (1998a) Measurement of fracture toughness of ultra-thin amorphous carbon films. Thin Solid Films 315:214–221CrossRef Li X, Bhushan B (1998a) Measurement of fracture toughness of ultra-thin amorphous carbon films. Thin Solid Films 315:214–221CrossRef
Zurück zum Zitat Li X, Bhushan B (1998b) Micromechanical and tribological characterization of hard amorphous carbon coatings as thin as 5 nm for magnetic recording heads. Wear 220:51–58CrossRef Li X, Bhushan B (1998b) Micromechanical and tribological characterization of hard amorphous carbon coatings as thin as 5 nm for magnetic recording heads. Wear 220:51–58CrossRef
Zurück zum Zitat Li X, Bhushan B (1999a) Micro/nanomechanical and tribological characterization of ultra-thin amorphous carbon coatings. J Mater Res 14:2328–2337CrossRef Li X, Bhushan B (1999a) Micro/nanomechanical and tribological characterization of ultra-thin amorphous carbon coatings. J Mater Res 14:2328–2337CrossRef
Zurück zum Zitat Li X, Bhushan B (1999b) Mechanical and tribological studies of ultra-thin hard carbon overcoats for magnetic recording heads. Z Metallkd 90:820–830 Li X, Bhushan B (1999b) Mechanical and tribological studies of ultra-thin hard carbon overcoats for magnetic recording heads. Z Metallkd 90:820–830
Zurück zum Zitat Li X, Bhushan B (1999c) Micro/nanomechanical characterization of ceramic films for microdevices. Thin Solid Films 340:210–217CrossRef Li X, Bhushan B (1999c) Micro/nanomechanical characterization of ceramic films for microdevices. Thin Solid Films 340:210–217CrossRef
Zurück zum Zitat Li X, Bhushan B (1999d) Evaluation of fracture toughness of ultrathin and hard amorphous carbon coatings deposited by different deposition techniques. Thin Solid Films 355–356:330–336CrossRef Li X, Bhushan B (1999d) Evaluation of fracture toughness of ultrathin and hard amorphous carbon coatings deposited by different deposition techniques. Thin Solid Films 355–356:330–336CrossRef
Zurück zum Zitat Li X, Bhushan B (2000a) Development of continuous stiffness measurement technique for composite magnetic tapes. Scripta Mater 42:929–935CrossRef Li X, Bhushan B (2000a) Development of continuous stiffness measurement technique for composite magnetic tapes. Scripta Mater 42:929–935CrossRef
Zurück zum Zitat Li X, Bhushan B (2000b) Continuous stiffness measurement and creep behavior of composite magnetic tapes. Thin Solid Films 377–378:401–406CrossRef Li X, Bhushan B (2000b) Continuous stiffness measurement and creep behavior of composite magnetic tapes. Thin Solid Films 377–378:401–406CrossRef
Zurück zum Zitat Li X, Bhushan B (2001a) Continuous stiffness measurements of layered materials used in magnetic storage devices. J Info Storage Proc Syst 3:131–142MATH Li X, Bhushan B (2001a) Continuous stiffness measurements of layered materials used in magnetic storage devices. J Info Storage Proc Syst 3:131–142MATH
Zurück zum Zitat Li X, Bhushan B (2001b) Dynamic mechanical characterization of magnetic tapes using nanoindentation techniques. IEEE Trans Magn 37:1616–1619CrossRef Li X, Bhushan B (2001b) Dynamic mechanical characterization of magnetic tapes using nanoindentation techniques. IEEE Trans Magn 37:1616–1619CrossRef
Zurück zum Zitat Li X, Bhushan B (2002a) A review of nanoindentation continuous stiffness measurement and its applications. Mater Charact 48:11–36CrossRef Li X, Bhushan B (2002a) A review of nanoindentation continuous stiffness measurement and its applications. Mater Charact 48:11–36CrossRef
Zurück zum Zitat Li X, Bhushan B (2002b) Development of a nanoscale fatigue measurement technique and its application to ultrathin amorphous carbon coatings. Scripta Mater 47:473–479CrossRef Li X, Bhushan B (2002b) Development of a nanoscale fatigue measurement technique and its application to ultrathin amorphous carbon coatings. Scripta Mater 47:473–479CrossRef
Zurück zum Zitat Li X, Bhushan B (2002c) Nanofatigue studies of ultrathin hard carbon overcoats used in magnetic storage devices. J Appl Phys 91:8334–8336CrossRef Li X, Bhushan B (2002c) Nanofatigue studies of ultrathin hard carbon overcoats used in magnetic storage devices. J Appl Phys 91:8334–8336CrossRef
Zurück zum Zitat Li X, Bhushan B (2003) Fatigue studies of nanoscale structures for MEMS/NEMS applications using nanoindentation techniques. Surf Coat Technol 163–164:521–526CrossRef Li X, Bhushan B (2003) Fatigue studies of nanoscale structures for MEMS/NEMS applications using nanoindentation techniques. Surf Coat Technol 163–164:521–526CrossRef
Zurück zum Zitat Li WB, Henshall JL, Hooper RM, Easterling KE (1991) The mechanism of indentation creep. Acta Metall Mater 39:3099–3110CrossRef Li WB, Henshall JL, Hooper RM, Easterling KE (1991) The mechanism of indentation creep. Acta Metall Mater 39:3099–3110CrossRef
Zurück zum Zitat Li X, Diao D, Bhushan B (1997) Fracture mechanisms of thin amorphous carbon films in nanoindentation. Acta Mater 45:4453–4461CrossRef Li X, Diao D, Bhushan B (1997) Fracture mechanisms of thin amorphous carbon films in nanoindentation. Acta Mater 45:4453–4461CrossRef
Zurück zum Zitat Li X, Bhushan B, Inoue M (2001) Time-dependent mechanical properties and tribological behavior of magnetic tapes. Wear 251:1150–1158CrossRef Li X, Bhushan B, Inoue M (2001) Time-dependent mechanical properties and tribological behavior of magnetic tapes. Wear 251:1150–1158CrossRef
Zurück zum Zitat Li X, Bhushan B, Takashima K, Baek CS, Kim YK (2003) Mechanical characterization of micro/nanoscale structures for MEMS/NEMS applications using nanoindentation techniques. Ultramicroscopy 97:481–494CrossRef Li X, Bhushan B, Takashima K, Baek CS, Kim YK (2003) Mechanical characterization of micro/nanoscale structures for MEMS/NEMS applications using nanoindentation techniques. Ultramicroscopy 97:481–494CrossRef
Zurück zum Zitat Lin MR, Ritter JE, Rosenfeld L, Lardner TJ (1990) Measuring the interfacial shear strength of thin polymer coatings on glass. J Mater Res 5:1110–1117CrossRef Lin MR, Ritter JE, Rosenfeld L, Lardner TJ (1990) Measuring the interfacial shear strength of thin polymer coatings on glass. J Mater Res 5:1110–1117CrossRef
Zurück zum Zitat Loubet JL, Georges JM, Marchesini O, Meille G (1984) Vickers indentation curves of magnesium oxide (MgO). ASME J Tribol 106:43–48CrossRef Loubet JL, Georges JM, Marchesini O, Meille G (1984) Vickers indentation curves of magnesium oxide (MgO). ASME J Tribol 106:43–48CrossRef
Zurück zum Zitat Loubet JL, Bauer M, Tonck A, Bec S, Gauthier-Manuel B (1993) Nanoindentation with a surface force apparatus. In: Nastasi M, Parkin DM, Gleiter H (eds) Mechanical properties and deformation behavior of materials having ultra-fine microstructures. Kluwer Academic Pub, Dordrecht, pp 429–447CrossRef Loubet JL, Bauer M, Tonck A, Bec S, Gauthier-Manuel B (1993) Nanoindentation with a surface force apparatus. In: Nastasi M, Parkin DM, Gleiter H (eds) Mechanical properties and deformation behavior of materials having ultra-fine microstructures. Kluwer Academic Pub, Dordrecht, pp 429–447CrossRef
Zurück zum Zitat Lysaght VE (1949) Indentation hardness testing. Reinhold, New York Lysaght VE (1949) Indentation hardness testing. Reinhold, New York
Zurück zum Zitat Maharaj D, Bhushan B (2015) Friction, wear, and mechanical behavior of nano-objects on the nanoscale. Mater Sci Eng R 95:1–43CrossRef Maharaj D, Bhushan B (2015) Friction, wear, and mechanical behavior of nano-objects on the nanoscale. Mater Sci Eng R 95:1–43CrossRef
Zurück zum Zitat Marshall DB, Evans AG (1984) Measurement of adherence of residual stresses in thin films by indentation. I. Mechanics of interface delamination. J Appl Phys 15:2632–2638CrossRef Marshall DB, Evans AG (1984) Measurement of adherence of residual stresses in thin films by indentation. I. Mechanics of interface delamination. J Appl Phys 15:2632–2638CrossRef
Zurück zum Zitat Marshall DB, Lawn BR (1979) Residual stress effects in sharp contact cracking Part 1 indentation fracture mechanics. J Mater Sci 14:2001–2012CrossRef Marshall DB, Lawn BR (1979) Residual stress effects in sharp contact cracking Part 1 indentation fracture mechanics. J Mater Sci 14:2001–2012CrossRef
Zurück zum Zitat Marshall DB, Oliver WC (1987) Measurement of Interfacial Mechanical Properties in Fiber-Reinforced Ceramic Composites. J Am Ceram Soc 70:542–548CrossRef Marshall DB, Oliver WC (1987) Measurement of Interfacial Mechanical Properties in Fiber-Reinforced Ceramic Composites. J Am Ceram Soc 70:542–548CrossRef
Zurück zum Zitat Mayo MJ, Nix WD (1988) A micro-indentation study of superplasticity in Pb, Sn, and Sn-38 wt% Pb. Acta Metall 36:2183–2192CrossRef Mayo MJ, Nix WD (1988) A micro-indentation study of superplasticity in Pb, Sn, and Sn-38 wt% Pb. Acta Metall 36:2183–2192CrossRef
Zurück zum Zitat McGurk MR, Page TF (1999) Using the P-δ2 analysis to deconvolute the nanoindentation response of hard-coated systems. J Mater Res 14:2283–2295CrossRef McGurk MR, Page TF (1999) Using the P-δ2 analysis to deconvolute the nanoindentation response of hard-coated systems. J Mater Res 14:2283–2295CrossRef
Zurück zum Zitat Mehrotra PK, Qunito DT (1985) Techniques for evaluating mechanical properties of hard coatings. J Vac Sci Technol A 3:2401–2405CrossRef Mehrotra PK, Qunito DT (1985) Techniques for evaluating mechanical properties of hard coatings. J Vac Sci Technol A 3:2401–2405CrossRef
Zurück zum Zitat Mittal KL (ed) (1978) Adhesion measurements on thin coatings, thick coatings, and bulk coatings, STP640. ASTM, Philadelphia Mittal KL (ed) (1978) Adhesion measurements on thin coatings, thick coatings, and bulk coatings, STP640. ASTM, Philadelphia
Zurück zum Zitat Mott BW (1957) Microindentation hardness testing. Butterworths, London Mott BW (1957) Microindentation hardness testing. Butterworths, London
Zurück zum Zitat Mulhearn TO, Tabor D (1960) Creep and hardness of metals: a physical study. J Inst Metals 87:7–12 Mulhearn TO, Tabor D (1960) Creep and hardness of metals: a physical study. J Inst Metals 87:7–12
Zurück zum Zitat Nastasi M, Parkin DM, Gleiter H (eds) (1993) Mechanical properties and deformation behavior of materials having ultra-fine microstructures. Kluwer Academic Pub, Dordrecht Nastasi M, Parkin DM, Gleiter H (eds) (1993) Mechanical properties and deformation behavior of materials having ultra-fine microstructures. Kluwer Academic Pub, Dordrecht
Zurück zum Zitat Newey D, Wilkins MA, Pollock HM (1982) An ultra-low-load penetration hardness tester. J Phys E Sci Instrum 15:119–122CrossRef Newey D, Wilkins MA, Pollock HM (1982) An ultra-low-load penetration hardness tester. J Phys E Sci Instrum 15:119–122CrossRef
Zurück zum Zitat Nix WD (1989) Mechanical properties of thin films. Metall Trans A 20:2217–2245CrossRef Nix WD (1989) Mechanical properties of thin films. Metall Trans A 20:2217–2245CrossRef
Zurück zum Zitat Oliver WC (2001) Alternative technique for analyzing instrumented indentation data. J Mater Res 16:3202–3206CrossRef Oliver WC (2001) Alternative technique for analyzing instrumented indentation data. J Mater Res 16:3202–3206CrossRef
Zurück zum Zitat Oliver WC, Pharr GM (1992) An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J Mater Res 7:1564–1583CrossRef Oliver WC, Pharr GM (1992) An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J Mater Res 7:1564–1583CrossRef
Zurück zum Zitat Oliver WC, Hutchings R, Pethica JB (1986) Measurement of hardness at indentation depths as small as 20 nm. In: Blau PJ, Lawn BR (eds) Microindentation techniques in materials science and engineering STP 889. ASTM, Philadelphia, pp 90–108 Oliver WC, Hutchings R, Pethica JB (1986) Measurement of hardness at indentation depths as small as 20 nm. In: Blau PJ, Lawn BR (eds) Microindentation techniques in materials science and engineering STP 889. ASTM, Philadelphia, pp 90–108
Zurück zum Zitat O’Neill H (1967) Hardness measurement of metals and alloys. Chapman and Hall, London O’Neill H (1967) Hardness measurement of metals and alloys. Chapman and Hall, London
Zurück zum Zitat Page TF, Oliver WC, McHargue CJ (1992) the deformation behavior of ceramic crystals subjected to very low load (Nano) indentations. J Mater Res 7:450–473CrossRef Page TF, Oliver WC, McHargue CJ (1992) the deformation behavior of ceramic crystals subjected to very low load (Nano) indentations. J Mater Res 7:450–473CrossRef
Zurück zum Zitat Palacio M, Bhushan B (2010) Nanomechanical characterization of adaptive optics components in microprojectors. J Micromech Microeng 20:064002CrossRef Palacio M, Bhushan B (2010) Nanomechanical characterization of adaptive optics components in microprojectors. J Micromech Microeng 20:064002CrossRef
Zurück zum Zitat Palacio MLB, Bhushan B (2013) Depth-sensing indentation of nanomaterials and nanostructures. Mater Charact 78:1–20CrossRef Palacio MLB, Bhushan B (2013) Depth-sensing indentation of nanomaterials and nanostructures. Mater Charact 78:1–20CrossRef
Zurück zum Zitat Palacio M, Bhushan B, Ferrell N, Hansford D (2007a) Nanomechanical characterization of polymer beam structures for BioMEMS applications. Sens Actuators A 135:637–650CrossRef Palacio M, Bhushan B, Ferrell N, Hansford D (2007a) Nanomechanical characterization of polymer beam structures for BioMEMS applications. Sens Actuators A 135:637–650CrossRef
Zurück zum Zitat Palacio M, Bhushan B, Ferrell N, Hansford D (2007b) Adhesion properties of polymer/silicon interfaces for biological micro-/nanoelectromechanical systems applications. J Vac Sci Technol A 25:1275–1284CrossRef Palacio M, Bhushan B, Ferrell N, Hansford D (2007b) Adhesion properties of polymer/silicon interfaces for biological micro-/nanoelectromechanical systems applications. J Vac Sci Technol A 25:1275–1284CrossRef
Zurück zum Zitat Palmquist S (1957) Method of determining the toughness of brittle materials, particularly sintered carbides. Jernkontorets Ann 141:300–307 Palmquist S (1957) Method of determining the toughness of brittle materials, particularly sintered carbides. Jernkontorets Ann 141:300–307
Zurück zum Zitat Patton ST, Bhushan B (1996) Micromechanical and tribological characterization of alternate pole tip materials for magnetic recording heads. Wear 202:99–109CrossRef Patton ST, Bhushan B (1996) Micromechanical and tribological characterization of alternate pole tip materials for magnetic recording heads. Wear 202:99–109CrossRef
Zurück zum Zitat Perry AJ (1981) The adhesion of chemically vapour-deposited hard coatings on steel—the scratch test. Thin Solid Films 78:77–93CrossRef Perry AJ (1981) The adhesion of chemically vapour-deposited hard coatings on steel—the scratch test. Thin Solid Films 78:77–93CrossRef
Zurück zum Zitat Perry AJ (1983) Scratch adhesion testing of hard coatings. Thin Solid Films 197:167–180CrossRef Perry AJ (1983) Scratch adhesion testing of hard coatings. Thin Solid Films 197:167–180CrossRef
Zurück zum Zitat Pethica JB, Oliver WC (1989) Mechanical properties of nanometer volumes of material: use of the elastic response of small area indentations. In: Bravman JC, Nix WD, Barnett DM, Smith DA (eds) Thin films: stresses and mechanical properties, vol 130. Mat. Res. Soc., Pittsburgh, pp 13–23 Pethica JB, Oliver WC (1989) Mechanical properties of nanometer volumes of material: use of the elastic response of small area indentations. In: Bravman JC, Nix WD, Barnett DM, Smith DA (eds) Thin films: stresses and mechanical properties, vol 130. Mat. Res. Soc., Pittsburgh, pp 13–23
Zurück zum Zitat Pethica JB, Hutchings R, Oliver WC (1983) Hardness measurements at penetration depths as small as 20 nm. Philos Mag A 48:593–606CrossRef Pethica JB, Hutchings R, Oliver WC (1983) Hardness measurements at penetration depths as small as 20 nm. Philos Mag A 48:593–606CrossRef
Zurück zum Zitat Pharr GM (1992) The anomalous behavior of silicon during nanoindentation. In: Nix WD, Bravman JC, Arzt E, Freund LB (eds) Thin film: stresses and mechanical properties III, vol 239. Mater Res Soc, Pittsburgh, pp 301–312 Pharr GM (1992) The anomalous behavior of silicon during nanoindentation. In: Nix WD, Bravman JC, Arzt E, Freund LB (eds) Thin film: stresses and mechanical properties III, vol 239. Mater Res Soc, Pittsburgh, pp 301–312
Zurück zum Zitat Pharr GM (1998) Measurement of mechanical properties by ultra-low load indentation. Mater Sci Eng A 253:151–159CrossRef Pharr GM (1998) Measurement of mechanical properties by ultra-low load indentation. Mater Sci Eng A 253:151–159CrossRef
Zurück zum Zitat Pharr GM, Oliver WC, Clarke DR (1989) Hysteresis and discontinuity in the indentation load-displacement behavior of silicon. Scr Metall 23:1949–1952CrossRef Pharr GM, Oliver WC, Clarke DR (1989) Hysteresis and discontinuity in the indentation load-displacement behavior of silicon. Scr Metall 23:1949–1952CrossRef
Zurück zum Zitat Pharr GM, Oliver WC, Clarke DR (1990) The mechanical behavior of silicon during small-scale indentation. J. Electron Mater 19:881–887CrossRef Pharr GM, Oliver WC, Clarke DR (1990) The mechanical behavior of silicon during small-scale indentation. J. Electron Mater 19:881–887CrossRef
Zurück zum Zitat Pharr GM, Oliver WC, Brotzen FR (1992) On the generality of the relationship among contact stiffness, contact area, and elastic modulus during indentation. J Mater Res 7:613–617CrossRef Pharr GM, Oliver WC, Brotzen FR (1992) On the generality of the relationship among contact stiffness, contact area, and elastic modulus during indentation. J Mater Res 7:613–617CrossRef
Zurück zum Zitat Pharr GM, Harding DS, Oliver WC (1993) Measurement of fracture toughness in thin films and small volumes using nanoindentation methods. In: Nastasi M, Parkin DM, Gleiter H (eds) Mechanical properties and deformation behavior of materials having ultra-fine microsctructures. Kluwer Academic, Dordrecht, pp 449–461CrossRef Pharr GM, Harding DS, Oliver WC (1993) Measurement of fracture toughness in thin films and small volumes using nanoindentation methods. In: Nastasi M, Parkin DM, Gleiter H (eds) Mechanical properties and deformation behavior of materials having ultra-fine microsctructures. Kluwer Academic, Dordrecht, pp 449–461CrossRef
Zurück zum Zitat Raman V, Berriche R (1992) An investigation of the creep processes in tin and aluminum using a depth-sensing indentation technique. J Mater Res 7:627–638CrossRef Raman V, Berriche R (1992) An investigation of the creep processes in tin and aluminum using a depth-sensing indentation technique. J Mater Res 7:627–638CrossRef
Zurück zum Zitat Randall NX, Cristoph R, Droz S, Julia-Schmutz C (1996) Localised micro-hardness measurements with a combined scanning force microscope/nanoindentation system. Thin Solid Films 290–291:348–354CrossRef Randall NX, Cristoph R, Droz S, Julia-Schmutz C (1996) Localised micro-hardness measurements with a combined scanning force microscope/nanoindentation system. Thin Solid Films 290–291:348–354CrossRef
Zurück zum Zitat San Juan J, No ML, Schuh CA (2009) Nanoscale shape-memory alloys for ultrahigh mechanical damping. Nat Nanotechnol 4:415–419CrossRef San Juan J, No ML, Schuh CA (2009) Nanoscale shape-memory alloys for ultrahigh mechanical damping. Nat Nanotechnol 4:415–419CrossRef
Zurück zum Zitat Sargent PM (1986) Use of the indentation size effect on microhardness of materials characterization. In: Blau PJ, Lawn BR (eds) Microindentation techniques in materials science and engineering, STP vol 889. ASTM, Philadelphia, pp 160–174 Sargent PM (1986) Use of the indentation size effect on microhardness of materials characterization. In: Blau PJ, Lawn BR (eds) Microindentation techniques in materials science and engineering, STP vol 889. ASTM, Philadelphia, pp 160–174
Zurück zum Zitat Scruby CB (1987) An introduction to acoustic emission. J Phys E Sci Instrum 20:946–953CrossRef Scruby CB (1987) An introduction to acoustic emission. J Phys E Sci Instrum 20:946–953CrossRef
Zurück zum Zitat Sekler J, Steinmann PA, Hintermann HE (1988) The scratch test: different critical load determination techniques. Surf Coat Technol 36:519–529CrossRef Sekler J, Steinmann PA, Hintermann HE (1988) The scratch test: different critical load determination techniques. Surf Coat Technol 36:519–529CrossRef
Zurück zum Zitat Shih CW, Yang M, Li JCM (1991) Effect of tip radius on nanoindentation. J Mater Res 6:2623–2628CrossRef Shih CW, Yang M, Li JCM (1991) Effect of tip radius on nanoindentation. J Mater Res 6:2623–2628CrossRef
Zurück zum Zitat Sneddon IN (1965) The relation between load and penetration in the axisymmetric Boussinesq problem for a punch of arbitrary profile. Int J Eng Sci 3:47–57MathSciNetMATHCrossRef Sneddon IN (1965) The relation between load and penetration in the axisymmetric Boussinesq problem for a punch of arbitrary profile. Int J Eng Sci 3:47–57MathSciNetMATHCrossRef
Zurück zum Zitat Stone D, LaFontaine WR, Alexopoulos PS, Wu TW, Li CY (1988) An investigation of hardness and adhesion of sputter-depostied aluminum on silicon by utilizing a continuous indentation test. J Mater Res 3:141–147CrossRef Stone D, LaFontaine WR, Alexopoulos PS, Wu TW, Li CY (1988) An investigation of hardness and adhesion of sputter-depostied aluminum on silicon by utilizing a continuous indentation test. J Mater Res 3:141–147CrossRef
Zurück zum Zitat Sundararajan S, Bhushan B (2001) Development of a continuous microscratch technique in an atomic force microscope and its application to study scratch resistance of ultra-thin hard amorphous carbon coatings. J Mater Res 16:437–445CrossRef Sundararajan S, Bhushan B (2001) Development of a continuous microscratch technique in an atomic force microscope and its application to study scratch resistance of ultra-thin hard amorphous carbon coatings. J Mater Res 16:437–445CrossRef
Zurück zum Zitat Sundararajan S, Bhushan B, Namazu T, Isono Y (2002) Mechanical property measurements of nanoscale structures using an atomic force microscope. Ultramicroscopy 91:111–118CrossRef Sundararajan S, Bhushan B, Namazu T, Isono Y (2002) Mechanical property measurements of nanoscale structures using an atomic force microscope. Ultramicroscopy 91:111–118CrossRef
Zurück zum Zitat Suresh S (1991) Fatige of materials. Cambridge University Press, Cambridge Suresh S (1991) Fatige of materials. Cambridge University Press, Cambridge
Zurück zum Zitat Swadener JG, George EP, Pharr GM (2002) The correlation of the indentation size effect measured with indenters of various shapes. J Mech Phys Solids 50:681–694MATHCrossRef Swadener JG, George EP, Pharr GM (2002) The correlation of the indentation size effect measured with indenters of various shapes. J Mech Phys Solids 50:681–694MATHCrossRef
Zurück zum Zitat Swain MV, Hagan JT, Field JE (1977) Determination of the surface residual stresses in tempered glasses by indentation fracture mechanics. J Mater Sci 12:1914–1917CrossRef Swain MV, Hagan JT, Field JE (1977) Determination of the surface residual stresses in tempered glasses by indentation fracture mechanics. J Mater Sci 12:1914–1917CrossRef
Zurück zum Zitat Syed Asif SA, Pethica JB (1997) Nano scale creep and the role of defects. In: Gerberich WW, Gao H, Sundgren JE, Baker SP (eds) Thin films: stresses and mechanical properties IV MRS Symp Proc, vol 436. Mat. Res. Soc., Pittsburgh, pp 201–206 Syed Asif SA, Pethica JB (1997) Nano scale creep and the role of defects. In: Gerberich WW, Gao H, Sundgren JE, Baker SP (eds) Thin films: stresses and mechanical properties IV MRS Symp Proc, vol 436. Mat. Res. Soc., Pittsburgh, pp 201–206
Zurück zum Zitat Tabor D (1951) The hardness of metals. Clarendon Press, Oxford Tabor D (1951) The hardness of metals. Clarendon Press, Oxford
Zurück zum Zitat Tangena AG, Hurkx GAM (1986) The determination of stress-strain curves of thin layers using indentation tests, ASME. J Eng Mater Technol 108:230–232CrossRef Tangena AG, Hurkx GAM (1986) The determination of stress-strain curves of thin layers using indentation tests, ASME. J Eng Mater Technol 108:230–232CrossRef
Zurück zum Zitat Ternovskii AP, Alekhin VP, Shorshorov MKh, Khrushchov MM, Skvortsov VN (1973) Micromechanical testing of materials by depression. Zavod Lab 39:1620–1624 Ternovskii AP, Alekhin VP, Shorshorov MKh, Khrushchov MM, Skvortsov VN (1973) Micromechanical testing of materials by depression. Zavod Lab 39:1620–1624
Zurück zum Zitat Tsui TY, Pharr GM (1999) Substrate effects on nanoindentation mechanical property measurement of soft films on hard substrates. J Mater Res 14:292–301CrossRef Tsui TY, Pharr GM (1999) Substrate effects on nanoindentation mechanical property measurement of soft films on hard substrates. J Mater Res 14:292–301CrossRef
Zurück zum Zitat Tsui TY, Oliver WC, Pharr GM (1996) Influences of stress on the measurement of mechanical properties using nanoindentation. I. Experimental studies in an aluminum alloy. J Mater Res 11:752–759CrossRef Tsui TY, Oliver WC, Pharr GM (1996) Influences of stress on the measurement of mechanical properties using nanoindentation. I. Experimental studies in an aluminum alloy. J Mater Res 11:752–759CrossRef
Zurück zum Zitat Tsukamoto Y, Yamaguchi H, Yanagisawa M (1987) Mechanical properties of thin films: measurements of ultramicroindentation hardness, Young’s modulus and internal stresses. Thin Solid Films 154:171–181CrossRef Tsukamoto Y, Yamaguchi H, Yanagisawa M (1987) Mechanical properties of thin films: measurements of ultramicroindentation hardness, Young’s modulus and internal stresses. Thin Solid Films 154:171–181CrossRef
Zurück zum Zitat Valli J (1986) A review of adhesion test method for thin hard coatings. J Vac Sci Technol A4:3007–3014CrossRef Valli J (1986) A review of adhesion test method for thin hard coatings. J Vac Sci Technol A4:3007–3014CrossRef
Zurück zum Zitat VanLandingham MR, Villarrubia JS, Guthrie WF, Meyers GF (2001) Nanoindentation of polymers: an overview. Macromol Symp 167:15–43CrossRef VanLandingham MR, Villarrubia JS, Guthrie WF, Meyers GF (2001) Nanoindentation of polymers: an overview. Macromol Symp 167:15–43CrossRef
Zurück zum Zitat Venkataraman S, Kohlstedt DL, Gerberich WW (1992) Microscratch analysis of the work of adhesion for Pt thin films on NiO. J Mater Res 1:1126–1132CrossRef Venkataraman S, Kohlstedt DL, Gerberich WW (1992) Microscratch analysis of the work of adhesion for Pt thin films on NiO. J Mater Res 1:1126–1132CrossRef
Zurück zum Zitat Vinci RP, Vlassak JJ (1996) Mechanical Behavior of thin films. Annu Rev Mater Sci 26:431–462CrossRef Vinci RP, Vlassak JJ (1996) Mechanical Behavior of thin films. Annu Rev Mater Sci 26:431–462CrossRef
Zurück zum Zitat Vitovec FH (1986) Stress and load dependence of microindentation hardness. In: Blau PJ, Lawn BR (eds) Microindentation techniques in materials science and engineering, STP, vol 889. ASTM, Philadelphia, pp 175–185 Vitovec FH (1986) Stress and load dependence of microindentation hardness. In: Blau PJ, Lawn BR (eds) Microindentation techniques in materials science and engineering, STP, vol 889. ASTM, Philadelphia, pp 175–185
Zurück zum Zitat Walker WW (1973) Indentation creep at low homologous temperatures. In: Westbrook JH, Conrad H (eds) The science of hardness testing and its research applications. American Society for Metals, Metals Park, Ohio, pp 258–273 Walker WW (1973) Indentation creep at low homologous temperatures. In: Westbrook JH, Conrad H (eds) The science of hardness testing and its research applications. American Society for Metals, Metals Park, Ohio, pp 258–273
Zurück zum Zitat Wei G, Bhushan B, Ferrell N, Hansford D (2005) Microfabrication and nanomechanical characterization of polymer MEMS for biological applications. J Vac Sci Technol A 23:811–819CrossRef Wei G, Bhushan B, Ferrell N, Hansford D (2005) Microfabrication and nanomechanical characterization of polymer MEMS for biological applications. J Vac Sci Technol A 23:811–819CrossRef
Zurück zum Zitat Weihs TP, Lawrence CW, Derby CB, Pethica JB (1992) Acoustic emissions during indentation tests. MRS Proc 239:361–370CrossRef Weihs TP, Lawrence CW, Derby CB, Pethica JB (1992) Acoustic emissions during indentation tests. MRS Proc 239:361–370CrossRef
Zurück zum Zitat Westbrook JH (1957) Microhardness testing at high temperatures. Proc Am Soc Test Mater 57:873–895 Westbrook JH (1957) Microhardness testing at high temperatures. Proc Am Soc Test Mater 57:873–895
Zurück zum Zitat Westbrook JH, Conrad H (eds) (1973) The science of hardness and its research applications. American Soc. Metals, Metals Park Westbrook JH, Conrad H (eds) (1973) The science of hardness and its research applications. American Soc. Metals, Metals Park
Zurück zum Zitat Whitehead AJ, Page TF (1992) Nanoindentation studies of thin film coated systems. Thin Solid Films 220:277–283CrossRef Whitehead AJ, Page TF (1992) Nanoindentation studies of thin film coated systems. Thin Solid Films 220:277–283CrossRef
Zurück zum Zitat Wierenga PE, Franken AJJ (1984) Ultramicroindentation apparatus for the mechanical characterization of thin films. J Appl Phys 55:4244–4247CrossRef Wierenga PE, Franken AJJ (1984) Ultramicroindentation apparatus for the mechanical characterization of thin films. J Appl Phys 55:4244–4247CrossRef
Zurück zum Zitat Wierenga PE, van der Linden JHM (1986) Quasistatic and Dynamic Indentation Measurements on Magnetic Tapes. In: Bhushan B, Eiss NS (eds) Tribology and Mechanics of Magnetic Storage Systems, vol. 3. ASLE, Park Ridge, pp 31–37 Wierenga PE, van der Linden JHM (1986) Quasistatic and Dynamic Indentation Measurements on Magnetic Tapes. In: Bhushan B, Eiss NS (eds) Tribology and Mechanics of Magnetic Storage Systems, vol. 3. ASLE, Park Ridge, pp 31–37
Zurück zum Zitat Williams VS, Landesman AL, Shack RV, Vukobratovich D, Bhushan B (1988) In situ microviscoelastic measurements by polarization-interferometric monitoring of indentation depth. Appl Opt 27:541–546CrossRef Williams VS, Landesman AL, Shack RV, Vukobratovich D, Bhushan B (1988) In situ microviscoelastic measurements by polarization-interferometric monitoring of indentation depth. Appl Opt 27:541–546CrossRef
Zurück zum Zitat Wu TW (1991) Microscratch and load relaxation tests for ultra-thin films. J Mater Res 6:407–426CrossRef Wu TW (1991) Microscratch and load relaxation tests for ultra-thin films. J Mater Res 6:407–426CrossRef
Zurück zum Zitat Wu TW, Hwang C, Lo J, Alexopoulos P (1988) Microhardness and microstructure of ion-beam-sputtered, nitrogen doped NiFe films. Thin Solid Films 166:299–308CrossRef Wu TW, Hwang C, Lo J, Alexopoulos P (1988) Microhardness and microstructure of ion-beam-sputtered, nitrogen doped NiFe films. Thin Solid Films 166:299–308CrossRef
Zurück zum Zitat Wu TW, Shull AL, Berriche R (1991) Microindentation fatigue tests on submicron carbon films. Surf Coat Technol 47:696–709CrossRef Wu TW, Shull AL, Berriche R (1991) Microindentation fatigue tests on submicron carbon films. Surf Coat Technol 47:696–709CrossRef
Zurück zum Zitat Yanagisawa M, Motomura Y (1987) An ultramicro indentation hardness tester and its application to thin films. Lub Eng 43:52–56 Yanagisawa M, Motomura Y (1987) An ultramicro indentation hardness tester and its application to thin films. Lub Eng 43:52–56
Zurück zum Zitat Young WC, Budynas RG, Sadegh AM (2012) Roark’s formulas for stress and strain, 8th edn. McGraw-Hill, New York Young WC, Budynas RG, Sadegh AM (2012) Roark’s formulas for stress and strain, 8th edn. McGraw-Hill, New York
Metadaten
Titel
Depth-sensing nanoindentation measurement techniques and applications
verfasst von
Bharat Bhushan
Publikationsdatum
28.03.2017
Verlag
Springer Berlin Heidelberg
Erschienen in
Microsystem Technologies / Ausgabe 5/2017
Print ISSN: 0946-7076
Elektronische ISSN: 1432-1858
DOI
https://doi.org/10.1007/s00542-017-3372-2

Weitere Artikel der Ausgabe 5/2017

Microsystem Technologies 5/2017 Zur Ausgabe